Soo koobid degdeg ah:

Epoxy-ka-jiidashada-yar ayaa guud ahaan ka wanaagsan marka farsamaynta dhagaxu u baahan tahay dhexgalka qoto dheer ee daldaloolada iyo dildilaaca yar-yar, halka epoxy-ga jirka sare uu siinayo xakameyn badan oo nusqaamaha ballaaran, hagaajinta toosan, iyo codsiyada halka qulqulka xad-dhaafka ah uu yahay dhibaato. Si kastaba ha ahaatee, viscosity kaligiis ma aha in uu go'aamiyo alaabta. Nooca dhagaxa, ballaca cilladda, heerkulka, nolosha dheriga, muuqaalka daawaynta, balaadhinta, qoynta, iyo shuruudaha dhalaalka kama dambaysta ah dhammaan arrimaha. Dooro epoxy-ka hab-dhaqankiisa socodka uu la mid yahay habka dhabta ah halkii aad si fudud u iibsan lahayd CPS ugu hooseeya ama ugu sarreeya.

Iftiimin yar-yar ayaa u dhawaqaya si ka wanaagsan.

Wuu sii galaa, si fudud ayuu u fidaa, wuu qoysaa dildilaaca fiican, wuxuuna si fiican ugu shaqeeyaa hababka faakuumku caawiyay. Warshadaha dhagaxa ah ee isku dayaya in ay xoojiyaan xargaha ka hor inta aan la nadiifin, faa'iidooyinkaasi waxay noqon karaan kuwo soo jiidasho leh.

Laakin markaas waxaa soo ifbaxaya dhibaato wax soo saar ka duwan.

Resinku wuxuu ka soo qulqulaa cilad ballaadhan. Dayactir toosan ayaa bilaabmaya inuu hoos u dhaco. Tollayntu waxay nuugtaa walxo ka badan intii la filayay. Dhagax dalool ah ayaa cuna xabagta xabagta oo aad u badan. daawaynta ka dib, dib u hagaajintu waxa ay ahaanaysaa dib u dhac sababtoo ah inta badan epoxy-ga ayaa ka hoos maray dusha sare.

Halkaa marka ay marayso, walxo qulqulaya oo dhumuc weyn ama ka badan oo la xakameeyey ayaa bilaabaya inay si fiican u muuqdaan.

Tani waa sababta su'aasha faa'iido leh aysan ahayn:

"Epoxy-jiifka-hooseeya miyuu ka fiican yahay epoxy-ka-muuqaalka sare?"

Su'aasha wanaagsani waa:

"Intee in le'eg ayaa dhaq-dhaqaaqa epoxy-ga u baahan yahay ka hor inta aan la daaweynin, iyo halkee ayaan u baahanahay in uu sii jiro?"

Habaynta dhagaxa waxa ka mid ah hawlo aad u kala duwan: impregnation-ka yar-jeexjeexa, hagaajinta dusha marmarka, xoojinta granite, faleebo faaruq ah, mesh support, buuxinta tollaynta, isku xidhka toosan, buuxinta daloolka, iyo heerka ugu dambeeya ee dusha sare. Codsi kastaa wuxuu u baahan yahay dheellitir kala duwan oo u dhexeeya dhexgalka iyo sii-haynta.

Veropoxy hadda dhagax epoxy kala duwan waxay ka tarjumaysaa habkan codsiga ku salaysan, oo leh habab u go'ay oo loogu talagalay granite madow, marmar, dhagax cad, mesh support, faleebo faaruq ah, dhagax qaali ah, iyo hababka kale ee gaarka ah.

Viscosity-hooseeya iyo resin epoxy-viscosity-sare marka loo eego codsiyada habaynta dhagxaanta ee kala duwan

Waa maxay resin-ka-foox-hooseeya

Epoxy-muji-hoosaadku waa nadaamka qallafsan ee xabagta oo aan la daawayn kaas oo bixiya iska caabin aad u hooseeya oo ku socda socodka xaaladaha cabbirka ee qeexan.

Habka dhagxaanta ee wax ku oolka ah, taasi waxay la macno tahay epoxy-ga isku dhafan guud ahaan si fudud ayuu u fidi karaa, wuxuu geli karaa dildilaacyo yaryar, dalool qoyan, u dhex mara dhismayaal xoojin ah, oo u sii socdaal fog ka hor inta uusan viscosity ka kicin inta lagu jiro daaweynta.

Waa maxay sababta ay warshadaha dhagaxu u isticmaalaan epoxy-ga yar ee viscosity

Sababta ugu weyni waa dhexgalka.

Cilado badan oo qaab dhismeedka dhagaxa dabiiciga ah ayaa aad uga yar marka loo eego dusha sare. Dildilaac muuqda ayaa si aad ah u cidhiidhi kara wejiga salaxda. Granite cufan waxa ku jiri kara jeexjeexyo yaryar oo xabagta qaro weyni aanay si fudud u geli karin.

Nidaamka viscosity hoose wuxuu yareeyaa caabbinta qulqulka wuxuuna siinayaa resin fursad wanaagsan oo uu ku gaaro waddooyinka gudaha ah.

Tani waxay si gaar ah faa'iido u leedahay:

  • dildilaaca timaha;
  • yaryar-fissures;
  • granite cufan;
  • dildilaaca marmar;
  • vacuum impregnation;
  • xoojinta dhagaxa daloolka leh;
  • mesh qoynta; iyo
  • daawaynta dusha weyn ka hor inta aan la nadiifin.

Veropoxy's 2-Tallaabo-mugdi-hooseeya AB Xabagta loogu talagalay Granite Madow, tusaale ahaan, waxay isticmaashaa viscosity hoose, nidaam sal-gal sare ah si ay u dhex gasho daloolada granite cufan iyo kuwa yaryar ka hor inta aan la gaarin heerka dhamaadka.

Waa maxay muuqalka sare ama dheecaanka jidhka sare?

Viscosity-sare epoxy-ga ayaa si xoog leh u caabbiya qulqulka.

Halkii ay si degdeg ah ugu fidi lahaayeen dusha sare ama ay ku lumin lahaayeen daloolo yaryar, maaddadu waxay u egtahay inay ku sii dhawaato meesha lagu dabaqo.

Dabeecaddani waxay noqon kartaa mid qiimo leh marka yoolka wax-soo-saarku uusan ahayn dhexgalka qoto dheer.

Halka jidhka sare uu noqdo mid waxtar leh

Xaaladaha caadiga ah waxaa ka mid ah:

  • dildilaaca ballaaran;
  • godadka waaweyn;
  • hagaajinta cidhifka;
  • kala goysyada toosan;
  • tolliin ay tahay in ay buuxsamaan;
  • Codsiyada halka qulqulka qulqulaya loo baahan yahay in la yareeyo;
  • dayactirka u baahan dhismaha dusha sare; iyo
  • xaaladaha galitaanka xad-dhaafka ah ay kordhinayso isticmaalka xabagta.

Farqiga muhiimka ah ayaa ah in "viskosity-ga sare" uusan si toos ah macnaheedu ahayn "buuxiyaha ka wanaagsan."

Waxqabadka buuxinta faraqa waxay sidoo kale ku xirnaan kartaa thixotropy, buuxinyaasha, kimistariga resin, xiisadda dusha sare, xawaaraha daaweynta, dabeecadda yaraynta, sifooyinka fidinta, iyo dhumucda codsiga.

Tani waa sababta xulashada alaabada xirfadleyda u baahan tahay in ka badan hal lambar CPS.

Buuxinta Farqiga Dhagaxa ee Muuqda Sare

Viscosity Low vs Viscosity Sare: Farqiga Ugu Weyn

Qodobka Waxqabadka Hoos-u-muuqaalka Epoxy Aragga sare-sare/Xaq-dheer ee Jirka
Dhexdhexaadinta yar-yar Guud ahaan ka wanaagsan Oo xadidan
Socodka dusha sare ee waaweyn Fudud Si tartiib ah oo loo xakameeyo
Faleebo faleebo Caadi ahaan waa la door bidaa Waxay xaddidi kartaa dhaqdhaqaaqa xabagta
Buuxinta farqiga ballaaran Waxaa laga yaabaa inay daadi ama quusto daloollada ku hareeraysan Caadi ahaan waxay bixisaa sii hayn ka wanaagsan
Codsi toosan Daadad ka weyn ama khatarta hoos u dhacda Caadi ahaan way fududahay in booska lagu hayo
Dhagax aad u daloola Waxa laga yaabaa inay kordhiso isticmaalka xabagta Waxay yarayn kartaa socdaalka qoto dheer ee aan loo baahnayn
Mesh qoynta Guud ahaan sahlan Waxa laga yaabaa inay u baahato dadaal fidineed oo dheeraad ah
Dhisidda dusha sare Ka tagi kara dabool khafiif ah Caadi ahaan ka fiican
Siideynta hawada Inta badan way fududahay marka si sax ah loo qaso Hawada ku dheggan ayaa laga yaabaa inay si tartiib tartiib ah u socoto
Xakamaynta hawl wadeenada Dhaqso u ordi kara Sida caadiga ah way u fududahay meelaynta deegaanka

Waa maxay sababta Viscosity-ka Hoose u wanaajiso wax-is-dhexgalka

Cilladaha dhagaxa fiican waxay abuuraan wadooyin cidhiidhi ah.

Mar kasta oo dariiqu yar yahay, waa ay sii adkaanaysaa in dareere viscous ah uu dhex maro.

Viscosity hoose wuxuu yareeyaa caabbinta qulqulka waxayna wanaajisaa awooda resin si uu u galo kanaaladaas yar ka hor inta aan la daaweynin meel fog.

Mawduuca hoose ee Epoxy Dhagax Dilaaca

Granite madow cufan waa tusaale wanaagsan

Granite madow waxa laga yaabaa inay u muuqato mid aad u adag, haddana saqafyadu waxay ka koobnaan karaan jeexjeexyo yaryar, dalool dabiici ah, ama cillado yaryar oo la xidhiidha habaynta.

Sababtoo ah dhagaxu waa cufan, si fudud u dhejinta koolada qaro weyn ee dusha sare waxaa laga yaabaa inaanay bixin xoojin gudaha ah oo macno leh.

Nidaamka granite-madow ee Veropoxy wuxuu isticmaalaa lakabka galitaanka viscosity hoose si gaar ah si uu u gaadho qoto dheer ee dhagaxa ka hor inta aan la marin lakabka midabaynta iyo hagaajinta.

Caqligan labada marxaladood waa muhiim.

Xabagta sida ugu wanagsan ee laysugu geliyo uma baahna inay qabato hawl kale oo dhammayn isku mar ah.

Waa maxay sababta Viscosity-hooseeya uu muhiim ugu yahay faleebo vacuum ah

Faleebo faleebo waxay ku xiran tahay dhaqdhaqaaqa resinka.

Cadaadiska faakuumku waxa uu caawiyaa resin-ka gelitaanka daldaloollada, jeexjeexyada, iyo cilladaha gudaha, laakiin geeddi-socodku wali waxa ay ku xidhan tahay xabagta haray ee mobilada oo ku filan in uu ku dhex maro dhagaxa.

Resin-ka oo noqda mid aad u muuqda wuxuu hoos u dhigi karaa socodka hore, wuxuu abuuri karaa impregnation aan sinnayn, ama wuxuu ka tagi karaa meelaha si aan loo xoojin.

Veropoxy's Aragtida hoose ee faleebo dhagaxa ah ee faleebo-5080/B25Q-KG waxaa lagu daabacay ku dhawaad 400-600 CPS, oo leh 100:25 saamiga isku dhafka ah, ku dhawaad 24°C heerkulka habaynta, iyo 3-5 saac wakhtiga daaweynta.

Tilmaamahani waxay muujinayaan qodob kale oo muhiim ah:

Viscosity hoose wuxuu u baahan yahay waqti shaqo oo ku filan.

Resin-ku wuxuu bilaabi karaa dareere aad u sarreeya, laakiin haddii uu si dhakhso ah u falceliyo oo uu dhumucdo ka hor inta aan wareegga faakuumku dhammaanin, viscosity-kiisii hore aad ayuu u yaraadaa.

Faleebo vacuum ah, barbar dhig in ka badan CPS

Iibsadayaasha sidoo kale waa inay qiimeeyaan:

  • viscosity isku dhafan;
  • viscosity kor u kaca waqti ka dib;
  • nolosha dheriga;
  • waqti gel;
  • heerkulka dhagaxa;
  • muddada wareegga-vacuum;
  • habdhaqanka sii daynta hawada; iyo
  • qoto dheer galinta dhabta ah.

Marka Mugdigu Hooseeyo uu Noqdo Dhib

Khaladka ugu fudud ayaa ah in la qaato in haddii dhexgalka uu faa'iido leeyahay, xitaa wax badan oo dhexgalka waa in ay fiicnaadaan.

Taasi mar walba run maaha.

Biyo aad u badan

Xabagta dareeraha ah ee dareeraha ah waxay ka fogaan kartaa aagga dayactirka ka hor inta aan la daaweyn.

Tani waxay si gaar ah ugu adag tahay sagxadaha jilcan, geesaha, dhagxaanta taagan, iyo godadka furan.

Isticmaalka xabagta sare

Dhagaxa daloolka leh ayaa laga yaabaa inuu nuugo tiro badan oo ah resin-mug yar.

Qaar ka mid ah dhexgalkaas ayaa laga yaabaa inay hagaajiyaan xoojinta, laakiin qaar ayaa si fudud u kordhin kara isticmaalka alaabta iyada oo aan hagaajin dayactirka muuqda.

Sidaa darteed warshaduhu waa inay ku cabbiraan isticmaalka resin-ka halkiiba halkii ay ku xukumi lahaayeen badeecadaha qiimaha durbaanka oo keliya.

Dhisidda dusha sare ee aan ku filnayn

Haddii inta badan resinku u guuro dhagaxa, wax aan ku filnayn ayaa laga yaabaa inay ku sii sugnaadaan dusha sare.

Ka dib marka la shiidi karo oo la nadiifiyo, dildilaaca ama daloolada ayaa dib u furmi kara muuqaal ahaan sababtoo ah qaybta sare ee cilladda ayaa si hoose loo buuxin.

Hooska dhagax fudud

On marmar cad ama translucent, dhexgalka xad-dhaaf ah waxay bedeli kartaa muuqaalka muuqaalka ah ee dhagaxa agagaarka dayactirka.

Natiijadu waxay u ekaan kartaa wasakh ama calaamad biyood xataa haddii epoxy-ga la daweeyay laftiisu uu cad yahay.

Tani waa sababta ka-hortagga marmarka cad-cad inta badan u baahan yahay kontorool adag oo galitaanka marka loo eego granite madow oo cufan.

Marka Epoxy Jirka Sare uu yahay jihada ugu Wanaagsan

Dildilaacyo ballaadhan iyo godadka furan

Cilad ballaadhan waxay u baahan tahay waxyaabo badan si ay ugu sii jirto aagga dayactirka.

Haddii xabagta uu aad u dareero, waxaa laga yaabaa inay hoos u daadato, u guurto daloollada ku hareeraysan, ama ka tago meesha sare ee godka oo buuxin.

Dayactir toosan

Cufisjiidka arrimaha

Resin oo si qurux badan u koraya sariir toosan ayaa laga yaabaa inuu hoos u dhaco cidhif toosan ka hor inta aan la daaweyn.

Isku xidhka toosan ama buuxinta cidhifyada, habaynta thixotropic ee la xakameeyey ayaa aad u fududaan karta in lagu shaqeeyo.

Barbaarinta dusha sare

Qaar ka mid ah hawlgallada habaynta waxay u baahan yihiin resin si uu ugu sii jiro meel u dhow oogada si shiidid iyo turxaan bixin ay u soo saari karaan weji joogto ah.

Xaaladahan, dhexgalka qoto dheer waa qayb ka mid ah shuruudaha.

Warshadu waxa ay u isticmaali kartaa hal shay oo ah impregnation gudaha iyo mid kale oo buuxinta u dambeeya ama dhamaystirka dusha sare.

Ha u malayn in Epoxy-buuxitaanku ay tahay inuu haysto CPS aad u sarreeya

Halkani waa halka xeerarka fudud ee viscosity ay bilaabaan inay burburaan.

Veropoxy's Balaadhinta Hoose ee Buuxinta Tobban-Qiimaha Dhagaxa ah - 5090 / D30M-BS hadda waxaa lagu qeexay qiyaastii 400-600 CPS.

Tiro ahaan, taasi waxay la mid tahay dhowr habab oo Veropoxy ku jihaysan dhexgalka.

Haddana codsigu waa buuxinta tollaynta ee agate, onix, iyo dhagxaan qaali ah oo isku jira.

Waa maxay sababtu?

Sababtoo ah xulashada alaabta kuma salaysna viscosity oo keliya.

Nidaamku wuxuu kaloo xooga saarayaa:

  • ballaarinta hoose;
  • diiqad hoose oo hoose;
  • socodka la xakameeyey;
  • xasilloonida cabbirka;
  • daaweynta lebbiska;
  • jaale aad u hooseeya; iyo
  • tol siman ka dib dhalaalidda.

Kani waa cashar wax iibsiga oo faa'iido leh.

Qaadashada iibsadaha: Ha abuurin qaanuun adag oo warshadeed sida "400-600 CPS waxa kaliya oo loogu talagalay gelitaanka" ama "buuxinta tolitaanka had iyo jeer waxay u baahan tahay viscosity aad u sarreeya." Habaynta, substrate-ka, joomatari gap, hanuuninta codsiga, habdhaqanka daaweynta, fidinta, iyo thixotropy ayaa bedeli kara natiijada.

Sida Nooca Dhagaxu u Bedesho Doorashada Viscosity

granite cufan

Granite cufan ayaa badanaa door bida habka dhexgalka ku jihaysan marka dhibka ugu weyni uu yahay dilaac-yar ama xoojinta gudaha.

Nidaamka viscosity hoose wuxuu geli karaa cillado laga yaabo in walxaha qaro weyni ay ka gudbaan.

Haddii ciladu tahay jajab weyn oo furan ama jabka cidhifka ah, si kastaba ha ahaatee, resinka galitaanka oo keliya ma bixin karo dhismo ku filan.

marmar cad

Marble cad waxay u baahan tahay taxadar dheeraad ah.

Viscosity hoose wuxuu wanaajin karaa dhexgalka dildilaaca, laakiin nuugista xad dhaafka ah waxay soo saari kartaa halo madow ama hadh indhaha.

Marble-dareenka midabka leh, viscosity waa in si wadajir ah loo qiimeeyaa dabeecad aan wasakh lahayn iyo iska caabin jaale ah.

marmar midab leh

Marble midab leh ayaa laga yaabaa inay u dulqaadato xoogaa dhexgalka muuqaal ah oo ka wanaagsan walxaha cad ee saafiga ah, laakiin kobcinta midabka ayaa weli u baahan inay sii ahaato mid joogto ah.

Xabagta saxda ah waa in ay soo gasho si ku filan si ay u hagaajiso cilladaha yaryar iyada oo aan la abuurin aagag aan caadi ahayn ka dib marka la nadiifiyo.

Travertine

Travertine waxa ku jira daloolo iyo godadka u dhexeeya koofiyadaha yaryar ilaa godadka waaweyn ee furan.

Hal xabo ayaa laga yaabaa in aanu ku habboonayn labada shuruudood.

Nidaam hoose oo viscosity ah ayaa laga yaabaa inuu faa'iido u yeesho xoojinta gudaha, halka walxo badan oo buuxin ah ayaa laga yaabaa in loo baahdo godadka dusha sare ee waaweyn.

onix iyo dhagax qaali ah oo nus-qaali ah

Qalabkani waxa uu noqon karaa mid araga xasaasi u ah, hufan, iyo cabbir ahaan jilicsan.

Buuxinta tollaynta, balaadhinta resinka, walbahaarka gudaha, caddaynta, iska caabbinta jaalaha ah, iyo nadiifinta waxay muhiim u tahay inta uu le'eg yahay viscosity.

Tani waa sababta nadaamka buuxinta tolmada dhagaxa qaaliga ah waa in lagu qiimeeyaa qaab dhamaystiran oo aan ahayn CPS oo keliya.

Sidee Cabirka Ciladuhu u Saamayn Lahayd Doorashada Epoxy

Cilad ama Habka Jihada socodka la door biday Hadafka Doorashada ugu weyn
dildilaaca yar ee timaha Viscosity hoose Gaadhi jeexjeexyada gudaha ka hor inta aan la jarin
Daloollo fincan Hoos u dhac ku yimaadda viscosity Qoyan oo xooji iyada oo aan lumin resin-ka xad dhaafka ah
Faleebo faleebo Mawjad hoose Ku ilaali socodka wareegga faleebada oo dhammaystiran
Taageerada mesh Mawduuc hoose oo la xakameeyey Fiilooyinka qoyan iyadoo laga hortagayo qulqulka aan loo baahnayn
Dildilaaca dusha dhexdhexaadka ah Mawduuc dheeli tiran Ku dar dhexgalka iyo buuxin ku filan
Tolmo ballaadhan Socodka-socodka ama nidaamka jirka sare Ilaali qoto dheer oo buuxin kana fogow dareeraha
Godad waaweyn Jirka sare ama qaab buuxin ku habboon Ku hay qalab ku filan gudaha dayactirka
Dayactir toosan Jirka sare / dhaqanka thixotropic Iska yaree qulqulka iyo qulqulka

Heerkulka ayaa bedeli kara "mugsoon-hooseeya" xabeeb walxo badan

Viscosity waa heer-kulka xasaasiga ah.

Isla epoxy-ga si fudud ugu qulqula aqoon-is-weydaarsiga diirran ayaa laga yaabaa inay si muuqata u dhumuc weynaadaan xilliga jiilaalka.

Tani waxay ka dhigan tahay xulashada badeecadu waa inaysan ku salaysnayn oo keliya lambarka viscosity ee ku daabacan xaashida xogta farsamada.

Xaaladaha wax soo saarka qabow

Heerkulka hoose:

  • resin caadi ahaan wuu sii dhumucayaa;
  • faafitaanku wuu sii adkaanayaa;
  • dhexgalka micro-crack wuu yaraan karaa;
  • sii daynta hawadu waxay hoos u dhigi kartaa;
  • qoynta mesh waxay noqon kartaa mid aad u adag; iyo
  • daawaynta guud ahaan waxay noqotaa mid gaabis ah.

Xaaladaha wax soo saarka diiran

Heerkulka sare wuxuu guud ahaan wanaajiya socodka bilowga.

Laakin waxa kale oo ay dedejin kartaa falcelinta resin-hardener waxayna yaraynaysaa daaqada shaqada ee waxtarka leh.

Tani waxay abuurtaa isbeddel muhiim ah:

Xabagta ayaa laga yaabaa in ay si fiican u dhex gasho dhowrka daqiiqo ee ugu horeeya laakiin aad bay u falcelisaa ka hor inta aan la daweyn gogosha oo dhan.

Si aad u hesho sharaxaad qoto dheer oo ku saabsan xidhiidhkan, arag Waqtiga daawaynta Resin Epoxy iyo Hagaha Heerkulka.

Wakhtiga shaqadu wuu ka macno badan yahay mawqifka hore

Xaashida xogta farsamada ayaa laga yaabaa inay bixiso hal qiime oo viscosity ah oo la qiyaasay wax yar ka dib marka la isku daro.

Wax soo saarku ma dhaco hal mar.

Epoxy waxay noqon kartaa:

  • isku qasan dhowr daqiiqo;
  • loo qaaday saldhig kale;
  • ku fidsan saqaf weyn;
  • bidix hoostiisa vacuum;
  • shabag la soo dhex galiyey; ama
  • si gacan ah uga shaqeeyey dayactirro badan.

Inta lagu jiro wakhtigaas, daawaynta way sii socotaa, viscosity-ka ayaa kor u kaca.

Sababtan awgeed, warshadu waa inay waydiiso kaliya:

"Waa maxay bilawga CPS?"

laakiin sidoo kale:

"Intee in le'eg ayuu xabashidu ku sii jirayaa xadka socodka faa'iido leh?"

Sida Loo waafajiyo Qulqulka Epoxy iyo Baahiyaha Habaynta Dhabta ah ee Dhagaxa

Haddii dhibka ugu weyni yahay dildilaaca timaha gudaha granite cufan, dooro nidaamka galitaanka viscosity hoose oo leh waqti shaqo oo ku filan si loo gaaro cilladaha gudaha.

Haddii faleebo vacuum ah la isticmaalo, mudnaanta kala sii viscosity hoose oo isku dhafan iyo socodka deggan inta lagu jiro wareegga faakuumka.

Haddii mesh fiberglass ah ay qasab tahay in lagu qooyo gogol weyn, dooro viscosity hoose oo kontaroolan oo si fudud u fida laakiin aan cararin ka hor inta aan shabaggu si siman u daboolin.

Haddii tollayn ballaaran ay si isdaba joog ah u degto codsiga ka dib, u gudub qaabaynta leh haynta ama jirka halkii aad ku dari lahayd wax badan oo isku mid ah resin galinta.

Haddii cidhifka toosan uu hoos u dhaco, qiimee nidaamka thixotropic ama kuwa aan sag lahayn.

Haddii marmar cad uu ka soo baxo halo mugdi ah oo ku wareegsan dildilaaca, si toos ah ha u dooran indho-beelka hoose ee xitaa. Baadh dhexgalka xad-dhaafka ah iyo porosity dhagax marka hore.

Haddii dayactirka dusha sare uu dib u dhaco ka dib dhalaalidda, ka fiirso habraac laba heer ah: dhexgalka qoto dheer marka hore, oo ay ku xigto buuxinta dusha ku habboon.

Dhexgalka vs Buuxinta: Maxay Warshadaha Qaar Ugu Baahan Yihiin Labo Tallaabo

Isku dayga in la sameeyo hal resin wax kasta waxay abuurtaa tanaasul.

Alaabta dhuuban oo ku filan si ay u gaadho dildilaaca-yar-yar ee ugu qoto dheer waxaa laga yaabaa inaanay ku sii nagaan dusha sare.

Alaabta dhumuc weyni ku filan buuxinta cilad ballaadhan waxa laga yaabaa in aanay gaadhin jeexjeexyada gudaha ee wanaagsan.

Tallaabada 1: Xooji qaabdhismeedka

Isticmaal xabagta ku jihaysan dhexgalka si aad u gasho daloolada iyo dildilaaca yaryar oo aad u dejiso dhagaxa gudaha.

Tallaabada 2: dib u dhis dusha sare

Marxaladda dhexgalka ka dib, mari dusha ama nidaamka buuxinta meesha lagama maarmaanka ah si loo soo celiyo cilad qoto dheer, midab, siman, iyo dhalaalid diyaargarowga.

Nidaamka granite-madow ee Veropoxy wuxuu horeyba u muujinayaa mabda'a this iyada oo loo marayo saldhig hoose oo viscosity ah oo ay ku xigto midab-kordhinta iyo dhogorta sare.

Casharka ballaadhan ayaa faa'iido leh oo ka baxsan granite madow:

Xoojinta qoto dheer iyo dhamaystirka dusha sare waa shaqooyin kala duwan.

Waa maxay sababta Thixotropy ay muhiim ugu tahay Codsiyada Buuxinta Toosan iyo Farqiga

Viscosity waxaa badanaa loola dhaqmaa sidii inay tahay hal hanti oo go'an.

Qaababka dhabta ah waxay u dhaqmi karaan si ka duwan dhaqdhaqaaqa iyo nasashada.

Xabagta thixotropic waxay noqon kartaa mid sahlan in lagu faafiyo xiirta hoosteeda laakiin dib ayay u soo noqotaa jirka kadib codsiga.

Tani waxay noqon kartaa mid qiimo leh kala-goysyada toosan iyo dayactirka maxalliga ah sababtoo ah resinku waa la shaqeyn karaa inta lagu jiro faafinta laakiin wuxuu diidaa hoos u dhaca ka dib meelaynta.

Iibsadayaasha, tani waxay la macno tahay hal nambar wareeg-wareeg ah ayaa laga yaabaa inuusan si buuxda u qeexin habdhaqanka codsiga dhabta ah.

Weydii alaab-qeybiyaha in agabku yahay:

  • Newtonian ama si adag ugu tiirsan xiirid;
  • is-qiimaynta;
  • thixotropic;
  • aan sagxad lahayn;
  • loogu talagalay dhexgalka; ama
  • loogu talagalay haynta farqiga.

Khaladaadka Caadiga ah Marka la dooranayo Epoxy by Viscosity

Doorashada CPS ugu hooseysa sababtoo ah waxay u egtahay mid horumarsan

Viscosity aadka u hooseeya ayaa faa'iido leh kaliya marka codsigu ka faa'iidaysto qulqulka qoto dheer.

Cilladaha ballaaran, hagaajinta tooska ah, ama dhagaxa aadka u daloola, waxay abuuri kartaa dhibaatooyin aan loo baahnayn.

U yeerida resin kasta oo dhumuc weyn leh "viskosity sare"

Alaabooyinka qaarkood waxay bixiyaan waxqabadka buuxinta socodka la kantaroolo, buuxinta, thixotropy, yaraanshaha hoose, ama ballaarinta hoose halkii ay ka ahaan lahaayeen shaxan CPS ah oo aad u sarreeya.

Iska indhatirka heerkulka cabbirka

Qiimaha viscosity ee aan lahayn macnaha heerkulka ma dhamaystirna.

Iska indhatirka xawaaraha daawaynta

Viscosity hoose ee bilowga ah faa'iido ma leh haddii resinku uu dhumucdo ka hor inta aan codsiga la dhammaystirin.

Iska indha-tirka porosity-ka dhagaxa

Xabagta isku mid ah ayaa si aad u kala duwan ugu dhaqmi karta granite cufan iyo marmar.

Isticmaalka epoxy galinta godadka waaweyn

Xabagta waxaa laga yaabaa inay si fudud u baaba'do meel ka hooseysa dusha sare, taasoo kordhinaysa isticmaalka oo ka tageysa dayactirka oo aan buuxin.

Isticmaalka buuxinta culus ee dildilaaca yaryar

Maaddadu waxay isku xidhi kartaa albaabka dillaaca iyada oo ka tagaysa cilladda gudaha ee aan la daweyn.

Beddelida saamiga isku darka si loo beddelo viscosity

Si fudud ha u yaraysan ama ha u kordhin qallajiye si aad u samayso epoxy dhuuban, dhumuc weyn, dheereeya, ama gaabis ah.

Saamiga isku-darka waxaa iska leh kimistariga nidaamka.

Faahfaahin dheeraad ah, eeg Hagaha Isku-dhafka Isku-dhafka Epoxy Resin ee Habaynta Dhagaxa.

Sida loo Tijaabo Hooseeyo-iyo-ka-sare-Muuqaalka-mug-jiifka ka hor inta aan la dalbanin Bulk

Tallaabada 1: Isticmaal dhagaxa wax soo saarka dhabta ah

Ha isku hallayn kaliya muraayadaha, balaastigga, ama muraayadaha shaybaadhka guud.

Qaab dhismeedka dhagaxu wuxuu xakameeyaa nuugista resin-ka iyo dhexgalka.

Tallaabada 2: Xakamaynta heerkulka

Keen labada hab ee musharraxiinta isku xarfo, dhagax, iyo heerkul aqoon isweydaarsi.

Tallaabada 3: Isticmaal saamiga isku dhafka ee la cayimay

Isku darka khaldan wuxuu baabi'iyaa ansaxnimada isbarbardhigga.

Talaabada 4: Codso xadiga resin isku mid ah

Cabbir isticmaalka alaabta halkii aad ku shubi lahayd isha.

Tallaabada 5: U fiirso galitaanka

Hubi in resinku uu gaadhay qoto dheer ee cilladaha wanaagsan.

Tallaabada 6: U fiirso qulqulka iyo sii-haynta

Nusqaamaha ballaadhan, diwaangeli in resinku uu ku sii jiro booska ama uu ku quuso dhagaxa.

Tallaabada 7: Diiwaangeli wakhtiga shaqada

Ogow marka qulqulka uu noqdo mid la dareemo faa'iido yaraan.

Talaabada 8: Daawo oo nadiifi

Muuqaalka qoyan kuuma sheegayo in hawshu lagu guulaystay iyo in kale.

Kormeer sariirta ka dib isku xigxiga dhabta ah ee dhamaystirka.

Tallaabada 9: Cabbir isticmaalka alaabta

Xabagta u baahan 30% walxo dheeraad ah halkii salaxba waxa laga yaabaa inay lahaato kharash wax soo saar dhab ah oo aad uga duwan xataa haddii qiimihiisu hooseeyo.

Liiska hubinta u-qalmitaanka ee Epoxy Viscosity Stone

Shayga Qiimaynta Maxaa la duubayaa Maxaa Sabab U Ah
viscosity isku qasan CPS iyo heerkulka tijaabada Wuxuu bixiyaa bar bilow u dhigma
Nooca dhagaxa Granite, marmar, onix, travertine, dhagxaan la farsameeyay Porosity iyo qaabdhismeedku waxay beddelaan habdhaqanka socodka
Balaadhka ciladaysan Timo, dhexdhexaad ah, dalool ballaaran ama tollayn Wuxuu go'aamiyaa dhexgalka iyo shuruudaha sii haynta
Hanuuninta codsiga Horizontal, toosan, ama u janjeedha Waxay saamaysaa hoos u dhaca iyo qulqulka
Waqtiga shaqada Daqiiqado socodka waxtarka leh Viscosity-ga hore oo keliya kuma filna
Qoto galinta Qoto dheer ka dib codsiga Wuxuu xaqiijinayaa daaweynta qaabdhismeedka
Isticmaalka xabagta kg ama g halkii lakab / m² Wuxuu muujiyaa qiimaha wax soo saarka dhabta ah
Haysashada dusha sare Buuxinta hadhaaga daawaynta ka dib Muhiim u ah nadiifinta diyaargarowga
Muuqaalka ugu dambeeya Midab, dhalaal, hadh, iyo khadadka dayactirka muuqda Waxay xaqiijisaa waafaqid dhagax dhameestiran
Joogteynta Dufcada Natiijooyin badan oo badan Muhiim u ah wax soo saarka joogtada ah

Talo-soo-jeedin: Dooro Habdhaqanka Socodka, ee ma aha calaamadda Viscosity

Viscosity-hoose iyo epoxy-ga-sare ma aha kuwa ku tartamaya qaybaha badeecada halkaas oo mid ka mid ah uu ka fiican yahay kan kale.

Waxay xalliyaan mashaakilaadka habka kala duwan.

Haddii resinku u baahan yahay inuu galo dildilaaca yar yar, daldaloolada yaryar, ama qaab-dhismeed dhagax ah oo faakuum-ku caawiyay, mudnaanta sii viscosity hoose iyo wakhti shaqo oo ku filan.

Haddii resinku u baahan yahay inuu ku sii jiro faraq ballaadhan, hagaajin toosan, ama dalool dusha sare, mudnaanta sii haynta, jidhka, ama dabeecadda thxotropic.

Haddii codsigu u baahan yahay xoojinta gudaha iyo dusha sare ee si fiican labadaba, ka fiirso habsocod heersare ah intii aad ku qasbi lahayd hal resin si uu u qabto labada hawlood.

Haddii laba badeeco ay daabacaan qiyamka CPS ee isku midka ah laakiin ay si kala duwan u fuliyaan, is barbar dhig qaabaynta dhamaystiran: qoynta, thixotropy, profile bogsashada, balaadhinta, yaraynta, nolosha dheriga, kala duwanaanta heerkulka, waafaqid dhagaxa, iyo natiijada dhalaalaysa.

Maqnaanshaha saxda ah markaa maaha tirada ugu hooseysa ama ugu sareysa ee la heli karo.

Waa habdhaqanka socodka kaas oo u oggolaanaya epoxy-ga inuu gaaro meesha saxda ah - oo uu ku sii jiro halkaas muddo dheer oo ku filan si uu u dhamaystiro shaqada.

Su'aalaha Inta Badan La Isweydiiyo ee Ku Saabsan Hoos-u- iyo Aragti-sare

1. Epoxy-ka-muuqaalka hoose ma u roon yahay dhagaxa?

Epoxy-ga yar ee viscosity ayaa ka wanaagsan marka loo baahan yahay in la geliyo daldaloolo yaryar, dildilaaca yar yar, granite cufan, ama dhagax faaruq ah. Si toos ah uma roona nusqaamaha ballaaran, hagaajinta toosan, ama alaabta aadka u daloola halkaasoo socodka xad-dhaafka ahi uu kordhin karo qulqulka iyo isticmaalka resinka.

2. Waa maxay epoxy viscosity ee aan u isticmaalo dildilaaca dhagaxa?

Dildilaaca timaha dhuuban guud ahaan waxay ka faa'iidaystaan epoxy-ka hoose ee viscosity sababtoo ah resinku wuxuu u baahan yahay inuu gudaha galo. Dildilaaca ballaadhan waxa laga yaabaa inay u baahdaan nidaam jidheed oo dheelli-tiran ama ka sarreeya oo isku dara dhexgalka iyo haynta ku filan si ciladda si buuxda u buuxiso ka dib marka la daweeyo.

3. Epoxy-jilicsan oo sarreeya miyuu ka xoog badan yahay epoxy-ka-muuqaalka hoose?

qasab maaha. Viscosity-ka aan la daawayn si toos ah uma go'aamiyo xoogga ugu dambeeya ee farsamada. Xooggu waxa uu ku xidhan yahay chemistry resin, chemistry adke, saamiga isku darka, xaaladaha daawaynta, adhesion, qaabaynta qaabaynta, iyo isdhexgalka substrate-ka.

4. Waa maxay sababta epoxy-ka-muuqaalka yar uu u isticmaalo resin badan dhagaxa daloolka leh?

Maqaarka-mugdiga-hooseeya wuxuu si qoto dheer ugu socon karaa daldaloollo iyo faaruqyo isku xiran. Taasi waxay hagaajin kartaa xoojinta, laakiin sidoo kale waxay kordhin kartaa isticmaalka haddii dhagaxu nuugo resin ka baxsan aagga u baahan daaweynta. Cabbir isticmaalka resinka inta lagu jiro tijaabooyinka wax soo saarka ka hor inta aan la iibsan.

5. Epoxy isku mid ah ma loo isticmaali karaa galitaanka iyo buuxinta tollaynta?

Mararka qaarkood qaabaynta socodka-socodka ah ayaa qaban kara labada hawlood, laakiin jawaabtu waxay ku xidhan tahay nooca dhagaxa, ballaca tollaynta, resin rheology, habdhaqanka daaweynta, yaraynta ama ballaarinta, iyo shuruudaha dhamaystirka kama dambaysta ah. Hababka u baahan, heerar kala soocida iyo buuxinta ayaa laga yaabaa inay soo saaraan natiijooyin joogto ah.

Sida Loo waafajiyo Qulqulka Epoxy ilaa Habaynta Dhabta ah ee Dhagaxa

Xulashada Epoxy waa in ay ka bilaabataa meesha uu xabagta u baahan yahay in uu ku safro iyo meesha ay tahay in uu ku sii jiro. Dilaacyada yaryar iyo faleebada faakuumka waxay u baahan yihiin dhaqdhaqaaq. Cilladaha waaweyn iyo hagaajinta toosan waxay u baahan yihiin sii hayn. Dhamaystirka dusha sare wuxuu inta badan u baahan yahay dheelitirnaanta labada. CPS waxay bixisaa macluumaad faa'iido leh, laakiin had iyo jeer waa in si wada jir ah loo tarjumo iyadoo ay weheliso sinnaanta dhagaxa, joomatari cilladaysan, heerkulka, astaanta daaweynta, rheology, iyo shuruudaha dhamaystirka kama dambaysta ah.

Ka bilow cilada, ma aha calaamadda viscosity

Dildilaaca timaha, dalool travertine ah oo furan, fissure yar-yar oo madow-granite ah, dayactirka marmar-cad, iyo tolinka onika-ga ah isku dhib maaha. Balaadhka ciladaysan, dhuuqista dhagxaanta, hanuuninta, iyo dareenka aragga waa inay qeexaan habdhaqanka socodka loo baahan yahay ka hor inta aan la dooran baaxadda CPS.

Ku dhig habdhaqanka resinka iyo habka

Timaha granite dildilaaca:
Mudnaanta sii galitaanka viscosity hoose iyo wakhti shaqo oo ku filan si loo gaadho fisarada gudaha.

Vacuum infusion:
Mudnaan sii iska caabbinta hoose ee socodka, viscosity deggan, iyo daaqad daawaynta oo dheer oo ku filan si loo dhamaystiro impregnation.

Mesh backing:
Isticmaal socodka kontoroolka ah kaas oo si hufan u qooya fiilooyinka iyada oo aan la helin biyo badan.

Tolmo ballaadhan iyo godadka:
mudnaanta sii haysashada xabagta, dhisidda dusha sare, iyo xasilloonida cabbirka halkii aad ka geli lahayd ugu badnaan.

Dayactir toos ah:
qiimee dabeecadda thixotropic ama kuwa aan sag-caagnayn halkii aad ku tiirsanaan lahayd oo keliya qiimaha CPS ee taagan.

Qiimaha CPS ee la midka ah ayaa wali soo saari kara natiijooyin kala duwan

Alaabooyinka leh viscosity la mid ah oo la daabacay waxay u dhaqmi karaan si ka duwan sababtoo ah kiimiko samaynta, thixotropy, xiisadda dusha sare, xawaaraha daaweynta, sifooyinka fidinta hoose, qoynta, buuxinta, iyo isdhexgalka dhagxaan ayaa sidoo kale saameeya waxqabadka codsiga. Iibsadayaashu waa in ay isbarbardhigaan habdhaqanka alaabta oo dhamaystiran halkii ay ku kala sarayn lahaayeen alaab-qeybiyeyaasha hal lambar oo viscosity ah.

Maxay tahay inay iibsadayaashu isbarbar dhigaan ka hor intaysan dalban wax badan?

Is barbar dhig viscosity isku qasan heerkul la cayimay, wakhtiga shaqada, viscosity kor u kaca inta lagu jiro codsiga, qoto dheer ee dhexgalka, qulqulaya, isticmaalka resin, astaanta daawaynta, haynta dusha ugu dambaysa, habdhaqanka dhalaalka, xasiloonida midabka, iyo joogteynta dufcada. Ka dib tijaabi nidaamka liiska liiska ku yaal dhagaxa dhabta ah ee xaaladaha warshadaha caadiga ah.

Talo bixin Wax ku ool ah

Haddii resinku aanu gaadhi karin cilada, yaree caabbinta socodka. Haddii ay aad u fogaato ama ay ka dhamaato dayactirka, kordhi xakamaynta socodka ama dooro qaab buuxin ku habboon. Haddii xoojinta gudaha iyo dhamaystirka dusha sare labaduba ay yihiin kuwo muhiim ah, tixgeli dhexgalka iyo marxaladaha dhamaystirka goonida ah. Viscosity epoxy-ga ugu fiicani maaha doorashada ugu khafiifsan ama ugu dhumuc weyn - waa qaabaynta gaadhay qoto dheer ee loo baahan yahay, waxay ku hadhaysaa halka loo baahan yahay, oo waxay soo saartaa jeexan dhammays tiran oo xasilan ka dib markii la nadiifiyo oo la nadiifiyo.

Ma u baahan tahay inaad iswaafajiso Qulqulka Epoxy ee Codsigaaga Dhagaxa?

Nooca dhagaxa, ballaca dildilaaca, porosity, heerkulka habaynta, hanuuninta codsiga, wakhtiga daawaynta, iyo shuruudaha dhamaystirka dhamaantood waxay saameeyaan doorashada saxda ah ee epoxy. Kahor iibsashada bulk, tijaabi nidaamka musharaxiinta marmarkaada dhabta ah, granite, onikaga, dhagxaanta qaaliga ah, habka taageerada mesh, ama khadka faleebo vacuum.


Sahami Nidaamyada Epoxy Stone Veropoxy

Tixraacyo

  1. Ururka Caalamiga ah ee Habaynta.
    TS EN ISO 2555: 2018 caagadaha - Resins ee Gobolka dareeraha ah ama sida Emulsions ama kala firdhinta - Go'aaminta viscosity-ka muuqda iyadoo la adeegsanayo Habka Viscometer-ka Wareegga ah ee Kaliya.
    ISO/TC 61.
    Ururka Caalamiga ah ee Habaynta.
  2. ASTM International.
    ASTM D2196 - Hababka Tijaabada Caadiga ah ee Guryaha Rheological ee Agabka Aan Newtonian ee Viscometer Rotational.
    ASTM International.
    Heerarka ASTM iyo Maktabadda Dijital ah ee Injineerinka.
  3. NIDAAMKA GALBEED Shaqaale Farsamo.
    WEST SYSTEM User Manual & Product Guide.
    Gougeon Brothers, Inc.
    WEST SYSTEM Technical Publications.
  4. NIDAAMKA GALBEED Shaqaale Farsamo.
    Fahamka Dawaynta Epoxy iyo Saamaynta Heerkulka.
    Gougeon Brothers, Inc.
    Epoxyworks / WEST SYSTEM Ilaha Farsamada.
  5. Waaxda Farsamada Gurit.
    Nidaamyada Xabagta Xabagta: Habaynta, Viscosity iyo Astaamaha Daawaynta.
    Gurit.
    Xogta Farsamada ee Alaabta iyo Hagidda Habraaca Isku-dhafka ah.
  6. J. M. Dealy iyo K.F. Wissbrun.
    Melt Rheology iyo doorka ay ku leedahay habaynta caagagga: Aragti iyo Codsiyada.
    Van Nostrand Reinhold.
    Habaynta Polymer-ka iyo Suugaanta Tixraaca Rheology.
  7. Christopher W. Macosko.
    Mabaadi'da Rheological, Cabbiraadaha, iyo Codsiyada.
    Jaamacadda Minnesota.
    Wiley-VCH, 1994.
  8. Charles Selwitz.
    Resins Epoxy ee Ilaalinta Dhagaxa.
    Getty Ilaalinta Machadka.
    Cilmi-baarista Taxanaha Ilaalinta, Getty Publications, 1992.