Epoxy-viscosity nkeya muri rusange nibyiza mugihe gutunganya amabuye bisaba kwinjira cyane mubyobo na micro-crack, mugihe epoxy yumubiri wo hejuru itanga igenzura ryinshi kubyuho byinshi, gusana guhagaritse, hamwe nibisabwa aho gutemba bikabije ari ikibazo. Nyamara, viscosity yonyine ntigomba guhitamo ibicuruzwa. Ubwoko bwamabuye, ubugari bwinenge, ubushyuhe, ubuzima bwinkono, gukiza umwirondoro, kwaguka, guhanagura, nibisabwa bya nyuma byo gusya byose. Hitamo epoxy imyitwarire yimbere ihuye nibikorwa nyirizina aho kugura gusa CPS yo hasi cyangwa hejuru.

Epoxy yo hasi-viscosity yumvikana neza.

Yinjira kure, ikwirakwira byoroshye, ihanagura ibice byiza, kandi ikora neza mubikorwa bifashwa na vacuum. Ku nganda zamabuye zigerageza gushimangira ibisate mbere yo gusya, izo nyungu zirashobora kuba nziza cyane.

Ariko rero ikibazo gitandukanye cyumusaruro kiragaragara.

Ibisigarira biva mu nenge yagutse. Gusana guhagaritse gutangira kugabanuka. Ikidodo gikurura ibintu byinshi kuruta uko byari byitezwe. Icyapa kibisi gikoresha resin nyinshi. Nyuma yo gukira, gusana bikomeza gusubirwamo kuko igice kinini cya epoxy cyimukiye munsi yubutaka.

Icyo gihe, ibintu binini cyangwa byinshi bigenzurwa-bitangira kugaragara neza.

Iyi niyo mpamvu ikibazo cyingirakamaro atari:

“Epoxy yo mu bwoko bwa viscosity nkeya iruta epoxy yo hejuru cyane?”

Ikibazo cyiza ni:

“Epoxy ikenera ingendo zingahe mbere yo gukira, kandi ni hehe nkeneye ko ibisigarira bigumaho?”

Gutunganya amabuye bikubiyemo ibikorwa bitandukanye cyane: kwinjiza micro-crack, gusana hejuru ya marble, gushimangira granite, gushiramo vacuum, gushiramo inshundura, kuzuza ikidodo, guhuza vertical, kuzuza pore, no kuringaniza ubuso bwa nyuma. Buri porogaramu ikenera uburinganire butandukanye hagati yo kwinjira no kugumana.

Ibiriho bya Veropoxy Ibuye rya epoxy yibicuruzwa iragaragaza ubu buryo bushingiye kubikorwa, hamwe na sisitemu zabugenewe ya granite yumukara, marble, ibuye ryera, inyuma ya mesh, gushiramo vacuum, ibuye ryagaciro-igice, nibindi bikorwa byihariye.

Epoxy resin nkeya-yuzuye cyane ugereranije na progaramu zitandukanye zo gutunganya amabuye

Epoxy Resin ni iki?

Epoxy-viscosity nkeya ni sisitemu idakomeye ya resin-ikomera itanga imbaraga nke ugereranije no gutemba mugihe cyagenwe cyapimwe.

Mu gutunganya amabuye afatika, bivuze ko epoxy ivanze irashobora gukwirakwira muri rusange byoroshye, ikinjira mubice bito, imyenge itose, ikanyura mubikorwa byubaka, kandi ikagenda kure mbere yuko ububobere bwayo buzamuka mugihe cyo gukira.

Kuki inganda zamabuye zikoresha epoxy nkeya

Impamvu nyamukuru nukwinjira.

Inenge nyinshi zubatswe mumabuye karemano ni nto cyane kuruta uko bigaragara hejuru. Igice kigaragara kirashobora kugabanuka cyane munsi yisura. Granite yuzuye irashobora kuba irimo ibice byiza bidashobora kwinjira byoroshye.

Sisitemu yo hasi-viscosity sisitemu igabanya umuvuduko wamazi kandi igaha resin amahirwe meza yo kugera munzira zimbere.

Ibi ni ingirakamaro cyane kuri:

  • umusatsi;
  • uduce duto duto;
  • granite yuzuye;
  • marble nziza;
  • gutera akabariro;
  • gushimangira amabuye;
  • mesh; na
  • ahantu hanini ho kuvura mbere yo gusya.

Veropoxy's 2-Intambwe Nto-Viscosity AB Glue ya Black Granite, kurugero, ikoresha bike-viscosity, sisitemu yo kwinjira cyane kugirango yinjire mu byobo bya granite yuzuye na micro-fissure mbere yicyiciro cyo kurangiza.

Niki Cyinshi-Viscosity cyangwa Epoxy-Yumubiri-Hejuru?

Epoxy yo hejuru-viscosity irwanya gutemba cyane.

Aho gukwirakwira vuba hejuru cyangwa kuzimira mu byobo byiza, ibikoresho bikunda kuguma hafi yaho bikoreshwa.

Iyi myitwarire irashobora kuba iyagaciro mugihe intego yumusaruro itari kwinjira cyane.

Aho umubiri wo hejuru uba ingirakamaro

Ibihe bisanzwe birimo:

  • ibice binini;
  • imyenge minini;
  • gusana inkombe;
  • ingingo zihagaritse;
  • ingendo zigomba kuguma zuzuye;
  • Porogaramu aho amazi atemba agomba kugabanywa;
  • gusana bisaba kubaka hejuru; na
  • ibihe aho kwinjira cyane byakongera resin ikoreshwa.

Itandukaniro ryingenzi nuko "viscosity yo hejuru" idahita isobanura "kuzuza neza."

Imikorere yuzuza icyuho irashobora kandi guterwa na thixotropy, yuzuza, resin chimie, impagarara zubutaka, gukiza umuvuduko, imyitwarire mike yo kugabanuka, ibiranga kwaguka, hamwe nubunini bwikoreshwa.

Niyo mpamvu guhitamo ibicuruzwa byumwuga bikenera umubare urenze umwe wa CPS.

Byinshi-Viscosity Epoxy Kibuye Kuzuza icyuho

Viscosity nkeya vs Viscosity nyinshi: Itandukaniro nyamukuru

Ibikorwa Epoxy yo hepfo-Viscosity Hejuru-Viscosity / Hejuru-Umubiri Epoxy
Micro-crack kwinjira Muri rusange ni byiza Birenze
Genda unyuze hejuru Biroroshye Buhoro kandi bigenzurwa cyane
Vacuum Mubisanzwe bikunzwe Irashobora kugabanya kugenda
Kuzuza icyuho kinini Irashobora gutemba cyangwa kurohama mu byobo bikikije Mubisanzwe bitanga kugumana neza
Porogaramu ihagaritse Amazi menshi cyangwa impanuka Mubisanzwe byoroshye kugumana umwanya
Ibuye rinini cyane Urashobora kongera gukoresha resin Irashobora kugabanya kwimuka kwimbitse bitari ngombwa
Amashanyarazi Mubisanzwe byoroshye Birashobora gusaba imbaraga nyinshi zo gukwirakwiza
Kubaka hejuru Urashobora gusiga ibintu bitagaragara Mubisanzwe byiza
Kurekura ikirere Akenshi byoroshye iyo bivanze neza Umwuka wafashwe urashobora kugenda buhoro
Kugenzura ibikorwa Irashobora kwiruka vuba Mubisanzwe byoroshye kubibanza byaho

Impamvu Viscosity Ntoya Itezimbere

Inenge nziza yamabuye irema inzira zifunganye.

Inzira ntoya, niko bigorana kumazi ya viscous kuyinyuramo.

Ubukonje buke bugabanya kurwanya umuvuduko no kunoza ubushobozi bwa resin bwo kwinjira muri iyo miyoboro mito mbere yo gukira iterambere cyane.

Epoxy Ntoya-Viscosity Ibuye Kumeneka

Icyatsi kibisi granite ni urugero rwiza

Granite yumukara irashobora kugaragara nkigikomeye cyane, nyamara ibisate birashobora kuba birimo uduce duto, imyenge karemano, cyangwa gutunganya micro-inenge.

Kuberako ibuye rifite ubucucike, gusa ushyizeho umubyimba mwinshi hejuru ntishobora gutanga imbaraga zimbere imbere.

Sisitemu ya black-granite ya Veropoxy ikoresha urwego ruciriritse rwinjira cyane kugirango igere kure cyane mumabuye mbere yo gutandukanya ibara ryihariye-ryongera amabara.

Iyi mitekerereze y'ibyiciro bibiri ni ngombwa.

Ibisigarira bikora neza kugirango byinjire ntabwo byanze bikunze bigomba gukora indi mirimo yose yo kurangiza icyarimwe.

Impamvu Ubushuhe Buke Bwingenzi Kumwanya wa Vacuum

Vacuum infusion biterwa na resin igenda.

Umuvuduko wa Vacuum ufasha resin kwinjira mu byobo, ibice, ndetse nudusembwa twimbere, ariko inzira iracyaterwa na resin isigaye igendanwa bihagije kugirango inyure ibuye.

Ibisigarira bihinduka cyane birashobora gutinda imbere yimbere, bigatera inda zingana, cyangwa gusiga ahantu bidashimangiwe bihagije.

Veropoxy's Epoxy-Viscosity Epoxy ya Vacuum Yibuye - 5080 / B25Q-KG isohoka hafi ya 400-600 CPS, hamwe na 100: 25 ivanze, ubushyuhe bwo gutunganya hafi 24 ° C, nigihe cyo gukira cyamasaha 3-5.

Ibyo bisobanuro byerekana indi ngingo y'ingenzi:

Ubukonje buke bukeneye igihe gihagije cyo gukora.

Igisigarira kirashobora gutangira amazi menshi, ariko niba gikora vuba kandi kikabyimba mbere yuko cycle ya vacuum irangira, ububobere bwacyo bwa mbere biba bike cyane.

Kuri vacuum infusion, gereranya ibirenze CPS

Abaguzi nabo bagomba gusuzuma:

  • kuvangavanga;
  • ubwiza bwiyongera uko ibihe bigenda bisimburana;
  • ubuzima bw'inkono;
  • igihe cya gel;
  • ubushyuhe bw'amabuye;
  • igihe cyumwanya;
  • imyitwarire yo kurekura ikirere; na
  • ubujyakuzimu bwimbitse.

Iyo Viscosity nkeya ibaye ikibazo

Ikosa ryoroshye cyane ni ugutekereza ko niba kwinjira ari ingirakamaro, ndetse no kwinjira cyane bigomba kuba byiza.

Ntabwo buri gihe ari ukuri.

Amazi menshi

Amazi meza cyane arashobora kuva kure yagenewe gusanwa mbere yo gukira.

Ibi biragoye cyane cyane hejuru yubuso, impande, ibuye rihagaze, hamwe nu mwobo ufunguye.

Gukoresha resin nyinshi

Ibuye rinini rishobora gukurura ubwinshi bwa resin-viscosity resin.

Bimwe muribyo byinjira bishobora kunoza imbaraga, ariko bimwe bishobora kongera gusa ibikoresho bitarinze kunonosora bigaragara.

Inganda rero zigomba gupima imikoreshereze ya resin kuri buri cyapa aho gusuzuma ibicuruzwa ukoresheje igiciro cyingoma gusa.

Ubuso budahagije bwubaka

Niba ibyinshi mubisigara byimukiye mumabuye, ntabwo ibikoresho bihagije bishobora kuguma hejuru.

Nyuma yo gusya no gusya, ibice cyangwa imyenge birashobora gufungura muburyo bugaragara kuko igice cyo hejuru cyinenge cyuzuye.

Igicucu ku ibuye ryoroheje

Kuri marble yera cyangwa yoroheje, kwinjira cyane birashobora guhindura isura nziza yibuye ikikije gusana.

Ibisubizo birashobora kumera nkibara cyangwa ikirango cyamazi nubwo epoxy yakize ubwayo ikomeza kugaragara neza.

Niyo mpamvu gutunganya marble yera akenshi bisaba kugenzura cyane kuruta granite yijimye.

Iyo Hejuru-Umubiri Epoxy Nicyerekezo Cyiza

Igice kinini kandi gifunguye

Inenge yagutse ikenera ibikoresho byinshi kugirango igume imbere mugusana.

Niba ibisigazwa bitemba cyane, birashobora gutemba bikamanuka, kwimukira mu byobo bikikije, cyangwa gusiga hejuru yu mwobo bituzuye.

Gusana neza

Imbaraga rukuruzi.

Igisigara kiringaniye neza kumurongo utambitse kirashobora kumanuka kumurongo uhagaze mbere yo gukira.

Kuburyo buhagaritse cyangwa kuzuza impande, kugenzura cyane cyangwa thixotropic formulaire birashobora koroha cyane gukorana nayo.

Kuringaniza Ubuso

Ibikorwa bimwe byo gutunganya bikenera resin kugirango bigume hafi yubuso kugirango gusya no gusya bishobora kubyara isura ikomeza.

Muri ibi bihe, kwinjira cyane ni igice cyibisabwa.

Uruganda rushobora gukoresha ibikoresho bimwe byo gutera imbere imbere nibindi byo kuzuza cyangwa kurangiza hejuru.

Ntugatekereze ko Epoxy Yuzuza Ikimenyetso igomba kugira CPS Yisumbuye cyane

Aha niho amategeko yoroshye yo kwiyegereza atangira gucika.

Veropoxy's Kwiyongera Kwinshi Epoxy ya Semi-Igiciro Cyamabuye Yuzuza - 5090 / D30M-BS kuri ubu isobanuwe hafi ya 400-600 CPS.

Mubare, ibyo bisa na sisitemu nyinshi ya Veropoxy.

Nyamara gusaba ni kode yuzuza agate, onigisi, hamwe na kimwe cya kabiri cyagaciro.

Kubera iki?

Kuberako guhitamo ibicuruzwa bidashingiye kubwiza bwonyine.

Sisitemu ishimangira kandi:

  • kwaguka gake;
  • guhangayika imbere;
  • kugenzurwa;
  • ituze rihamye;
  • gukiza kimwe;
  • umuhondo muke cyane; na
  • ikidodo cyiza nyuma yo gusya.

Iri ni isomo ryingirakamaro ryo kugura.

Abaguzi: Ntugashyireho amategeko akomeye y'uruganda nka "400-600 CPS ni iyinjira gusa" cyangwa "kuzuza ubwato buri gihe bisaba ubwiza bwinshi cyane." Gutegura, substrate, icyuho cya geometrie, icyerekezo cyerekanwe, gukiza imyitwarire, kwaguka, na thixotropy birashobora guhindura ibisubizo.

Uburyo Ubwoko bwibuye buhindura amahitamo ya Viscosity

Granite yuzuye

Ubusanzwe granite ishyigikira uburyo bwo kwinjirira mugihe ikibazo nyamukuru ari micro-cracking cyangwa imbaraga zimbere.

Sisitemu yo hasi-yijimye irashobora kwinjiza inenge ibintu binini bishobora kurenga hejuru.

Niba inenge ari nini nini ifungura chip cyangwa kumeneka, ariko, resin yinjira yonyine ntishobora gutanga ibyubaka bihagije.

Marble yera

Marble yera isaba kwitonda.

Ubukonje buke burashobora kunoza gucengera, ariko kwinjiza cyane birashobora kubyara halos yijimye cyangwa igicucu cyiza.

Kuri marble yunvikana amabara, viscosity igomba gusuzumirwa hamwe nimyitwarire idahumanye hamwe no kurwanya umuhondo.

Amabara ya marble

Ibara rya marble irashobora kwihanganira kwinjirira neza kuruta ibintu byera byera, ariko kuzamura amabara biracyakenewe kuguma bihamye.

Ibisigarira bikwiye bigomba gucengera bihagije kugirango bikosore micro-inenge udashizeho uturere tudasanzwe nyuma yo gusya.

Travertine

Travertine irimo imyenge nu mwobo kuva kuri capillaries nziza kugeza kumyobo minini ifunguye.

Igisigarira kimwe ntigishobora kuba cyiza kubintu byombi.

Sisitemu yo hasi-viscosity sisitemu irashobora kuba ingirakamaro mugukomeza imbere, mugihe ibintu byinshi byuzuza-byerekanwa bishobora gukenerwa kubutaka bunini.

Onyx n'amabuye y'agaciro

Ibi bikoresho birashobora kuba byoroshye, byoroshye, kandi byoroshye.

Kuzuza ikidodo, kwaguka kwinshi, guhangayika imbere, kumvikana, kurwanya umuhondo, no guhindagurika birashobora kugira akamaro nkubwiza.

Iyi niyo mpamvu igice-cyagaciro cyamabuye yuzuye sisitemu bigomba gusuzumwa nkibisobanuro byuzuye aho kuba CPS yonyine.

Nigute Ingano Yuzuye igomba Guhindura Epoxy Guhitamo

Inenge cyangwa inzira Icyerekezo gitemba Intego nyamukuru yo guhitamo
Imisatsi mikoro Ubukonje buke Shikira ibice byimbere mbere yo gusohora
Amababi meza Hasi kugirango igenzurwe neza Wose kandi ushimangire nta gutakaza birenze urugero
Vacuum Ubukonje buke Komeza gutembera unyuze muburyo bwuzuye
Gushyigikira Kugenzura ubukonje buke Fibre itose mugihe wirinda gutemba bitari ngombwa
Ubuso buciriritse Uburinganire bwuzuye Huza kwinjira hamwe no kuzura bihagije
Ikirere kinini Igenzurwa-gutemba cyangwa sisitemu yo hejuru-yumubiri Komeza kuzuza ubujyakuzimu kandi wirinde gutemba
Imyobo nini Umubiri wo hejuru cyangwa ibyuzuye byuzuye Bika ibikoresho bihagije imbere yo gusana
Gusana neza Umubiri wo hejuru / imyitwarire ya thixotropic Mugabanye kugabanuka no gutemba

Ubushyuhe burashobora guhindura Epoxy "Ntoya-Viscosity" Mubikoresho Byinshi

Viscosity ni ubushyuhe bukabije.

Epoxy imwe itemba byoroshye mumahugurwa ashyushye irashobora kuba ndende cyane mugihe cy'itumba.

Ibi bivuze ko guhitamo ibicuruzwa bitagomba gushingira gusa kumubare wijimye wanditse kurupapuro rwa tekiniki.

Ubukonje bukonje

Ku bushyuhe bwo hasi:

  • resin mubisanzwe iba ndende;
  • gukwirakwiza biba bigoye;
  • micro-crack yinjira irashobora kugabanuka;
  • kurekura ikirere birashobora gutinda;
  • gushiramo mesh birashobora kuba ingorabahizi; na
  • gukira muri rusange bigenda gahoro.

Umusaruro ushushe

Ubushyuhe bwo hejuru muri rusange butezimbere urujya n'uruza.

Ariko irashobora kandi kwihutisha resin-gukomera no kugabanya idirishya ryakazi.

Ibi birema ubucuruzi bukomeye:

Ibisigarira birashobora kwinjira neza cyane muminota mike yambere ariko bigahinduka cyane mbere yuko icyapa cyose kivurwa.

Kubisobanuro byimbitse byiyi sano, reba Epoxy Resin Gukiza Igihe nubushyuhe bwo kuyobora.

Igihe cyakazi kirashobora kugira akamaro kuruta Viscosity Yambere

Urupapuro rwamakuru rwa tekiniki rushobora gutanga agaciro kamwe ko gupimwa nyuma gato yo kuvanga.

Umusaruro ntubaho mugihe kimwe.

Epoxy irashobora kuba:

  • bivanze mu minota mike;
  • bajyanwa ku yindi sitasiyo;
  • gukwira ku gisate kinini;
  • asigaye mu cyuho;
  • kuzunguruka muri mesh; cyangwa
  • yakoze intoki hirya no hino.

Muri kiriya gihe, gukira gutera imbere, kandi ubukonje burazamuka.

Kubera iyo mpamvu, uruganda ntirugomba kubaza gusa:

“CPS itangira iki?”

ariko kandi:

“Ibisigarira bimara igihe kingana iki bitembera neza?”

Nigute ushobora guhuza Epoxy itemba kubikenewe byo gutunganya amabuye nyayo

Niba ikibazo nyamukuru ari umusatsi wacitse imbere ya granite yuzuye, hitamo sisitemu yo hasi-viscosity sisitemu hamwe nigihe gihagije cyo gukora kugirango ugere ku nenge zimbere.

Niba ikoreshwa rya vacuum ryakoreshejwe, shyira imbere ububobere buke buvanze kandi bitemba neza mugihe cyizuba.

Niba mesh ya fiberglass igomba guhanagurwa hejuru yikibaho kinini, hitamo igenzura rito ryagutse bikwirakwira byoroshye ariko ntibihunge mbere yuko meshi itwikirwa kimwe.

Niba umugozi mugari urohamye inshuro nyinshi nyuma yo kubisaba, jya kuri formulaire hamwe no kugumana cyangwa umubiri aho kongeramo gusa ibintu byinshi byinjira.

Niba impande zihagaritse zo gusana zagabanutse, suzuma sisitemu ya thixotropique cyangwa itari sag.

Niba marble yera ikura halos yijimye ikikije ibice, ntugahite uhitamo nubwo bworoshye bwo hasi. Banza ukore iperereza ryinjira cyane hamwe nubutare bwamabuye.

Niba gusana hejuru byasubiwemo nyuma yo gusya, tekereza inzira ebyiri: kwinjira byimbitse, hanyuma ukurikire kuzuza neza.

Kwinjira vs Kuzuza: Impamvu Inganda Zimwe Zikeneye Intambwe ebyiri

Kugerageza gukora resin imwe ikora byose bitera ubwumvikane.

Igicuruzwa cyoroshye cyane kugirango kigere kuri micrike yimbitse ntishobora kuguma hejuru.

Igicuruzwa gifite umubyimba uhagije kugirango wuzuze inenge yagutse ntigishobora kugera mubice byimbere.

Intambwe ya 1: Shimangira imiterere

Koresha resin-yerekanwe kwinjirira kugirango winjire mu byobo na micro-crack hanyuma uhagarike ibuye imbere.

Intambwe ya 2: kongera kubaka ubuso

Nyuma yicyiciro cyo kwinjira, shyira hejuru cyangwa kuzuza sisitemu aho bikenewe kugirango ugarure ubujyakuzimu, ibara, ubworoherane, hamwe no kwitegura neza.

Sisitemu ya black-granite ya Veropoxy yamaze kwerekana iri hame binyuze mumyanya mito yo kwinjirira hasi ikurikirwa no kuzamura amabara no gusiga ikote hejuru.

Isomo ryagutse ni ingirakamaro kurenza granite yumukara:

Gushimangira byimbitse no kurangiza kurangiza ni imirimo itandukanye.

Impamvu Thixotropy Ibintu Byerekeranye na Vertical na Gap-Kuzuza Porogaramu

Viscosity ikunze gufatwa nkaho ari umutungo umwe uhamye.

Imiterere nyayo irashobora kwitwara ukundi mugihe cyo kuruhuka no kuruhuka.

Thixotropic adhesive irashobora koroha gukwirakwira munsi yintama ariko igarura umubiri nyuma yo kuyisaba.

Ibi birashobora kuba ingirakamaro mubice bihagaritse no gusana byaho kuko ibisigarira bikora mugihe cyo gukwirakwiza ariko bikanga kugabanuka nyuma yo kubishyira.

Kubaguzi, ibi bivuze umubare umwe wo kuzenguruka-viscosity numero ntishobora gusobanura neza imyitwarire nyayo yo gusaba.

Baza utanga isoko niba ibikoresho ari:

  • Newtonian cyangwa shear-biterwa cyane;
  • kwishyira hejuru;
  • thixotropic;
  • non-sag;
  • yagenewe kwinjira; cyangwa
  • yagenewe kubika icyuho.

Amakosa Rusange Mugihe Uhitamo Epoxy na Viscosity

Guhitamo CPS yo hasi cyane kuko byumvikana cyane

Ultra-low viscosity ningirakamaro gusa mugihe porogaramu yunguka ibintu byimbitse.

Kubinenge nini, gusana guhagaritse, cyangwa amabuye manini cyane, birashobora guteza ibibazo bitari ngombwa.

Hamagara buri mubyimba binini cyane "viscosity high"

Ibicuruzwa bimwe bitanga imikorere yuzuye binyuze mumigenzereze yagenzuwe, yuzuza, thixotropy, kugabanuka gake, cyangwa kwaguka gake aho kuba CPS hejuru cyane.

Kwirengagiza ubushyuhe bwo gupima

Agaciro ka viscosity nta bushyuhe bwubushyuhe ntabwo bwuzuye.

Kwirengagiza umuvuduko wo gukiza

Ubukonje buke bwambere ntabwo ari ingirakamaro niba resin yijimye mbere yo gusaba kurangiye.

Kwirengagiza amabuye y'agaciro

Ibisigarira bimwe birashobora kwitwara bitandukanye cyane kuri granite yuzuye na marble yuzuye.

Gukoresha penetration epoxy kuburwo bunini

Ibisigarira birashobora kuzimira munsi yubuso, kongera ibicuruzwa no gusana bituzuye.

Gukoresha ibyuzuzo biremereye kuri micro-crack

Ibikoresho birashobora guhagarika urugi rwinjira mugihe usize inenge yimbere itavuwe.

Guhindura igipimo cyo kuvanga kugirango uhindure ubwiza

Ntugabanye cyangwa ngo wongere gukomera kugirango ukore epoxy yoroheje, yijimye, yihuta, cyangwa buhoro.

Ikigereranyo cyo kuvanga ni icya chimie ya sisitemu.

Kubindi bisobanuro, reba Epoxy Resin Ivanga Ikigereranyo cyo gutunganya amabuye.

Nigute Wapima Hasi- na Hejuru-Viscosity Epoxy Mbere yo Gutumiza Byinshi

Intambwe ya 1: Koresha ibuye ry'umusaruro nyirizina

Ntukishingikirize gusa ku kirahure, plastiki, cyangwa laboratoire rusange.

Imiterere yamabuye igenzura resin iyinjira no kwinjira.

Intambwe ya 2: Kugenzura ubushyuhe

Zana sisitemu zombi z'abakandida kuri resin imwe, amabuye, n'ubushyuhe bw'amahugurwa.

Intambwe ya 3: Koresha igipimo cyagenwe cyo kuvanga

Kuvanga nabi byangiza agaciro ko kugereranya.

Intambwe ya 4: Koresha ingano ya resin imwe

Gupima ibyo ukoresha aho gusuka ijisho.

Intambwe ya 5: Itegereze kwinjira

Reba niba resin igera kubwimbitse bwuzuye inenge nziza.

Intambwe ya 6: Itegereze gutemba no kugumana

Kubyuho byinshi, andika niba ibisigara bigumye mumwanya cyangwa byiroha mumabuye.

Intambwe 7: Andika igihe cyakazi

Menyako iyo gutembera kugaragara ko bidafite akamaro.

Intambwe ya 8: Kiza kandi usukure

Kugaragara neza ntibikubwira niba inzira yagenze neza.

Kugenzura icyapa nyuma yukuri yo kurangiza.

Intambwe 9: Gupima ibyo ukoresha

Igisigarira gisaba 30% ibikoresho byinshi kuri buri cyapa birashobora kugira igiciro cyumusaruro utandukanye cyane nubwo igiciro cyacyo ari gito.

Urutonde rwa Epoxy Viscosity Impamyabumenyi Yurutonde

Ikintu cyo gusuzuma Ibyo Kwandika Impamvu bifite akamaro
Kuvangavanga CPS n'ubushyuhe bwo gupima Itanga intangiriro yo kugereranya
Ubwoko bwamabuye Granite, marble, onyx, travertine, ibuye ryakozwe Imyitwarire n'imiterere bihindura imyitwarire
Ubugari bwuzuye Umusatsi, uringaniye, ubugari bwagutse cyangwa ikidodo Kugena kwinjira no kugumana ibisabwa
Icyerekezo cyo gusaba Uhagaritse, uhagaritse, cyangwa uhengamye Ingaruka zo kugabanuka no gutemba
Igihe cyo gukora Iminota mike yingirakamaro Ubwiza bwambere bwonyine ntibuhagije
Ubujyakuzimu Ubujyakuzimu nyabwo nyuma yo gusaba Yemeza uburyo bwo kuvura
Koresha resin kg cyangwa g kuri buri cyapa / m² Yerekana ikiguzi cyukuri
Kugumana Ubuso Ibisigaye byuzuye nyuma yo gukira Nibyingenzi mugutegura kwitegura
Kugaragara kwanyuma Ibara, indabyo, igicucu, n'imirongo igaragara yo gusana Yemeza guhuza ibuye ryarangiye
Guhuza ibice Ibisubizo muri byinshi Ni ngombwa kubyara umusaruro uhoraho

Icyifuzo: Hitamo Imyitwarire Itemba, Ntabwo Ikirango Cyiza

Epoxy yo hasi cyane kandi yuzuye cyane ntabwo irushanwa mubyiciro byibicuruzwa aho umwe asanzwe arusha undi.

Bakemura ibibazo bitandukanye.

Niba ibisigara bikeneye kugenda muri micro-crack, pore nziza, cyangwa amabuye afashwa na vacuum, shyira imbere ubukonje buke nigihe gihagije cyo gukora.

Niba ibisigazwa bigomba kuguma mu cyuho kinini, gusana guhagaritse, cyangwa mu cyuho cyo hejuru, shyira imbere kugumana, umubiri, cyangwa imyitwarire ya thixotropique.

Niba porogaramu isaba imbaraga zombi imbere hamwe nubuso bwuzuye neza, tekereza inzira yatunganijwe aho guhatira resin imwe gukora imirimo yombi.

Niba ibicuruzwa bibiri bitangaza agaciro ka CPS ariko bigakora ukundi, gereranya nuburyo bwuzuye: guhanagura, thixotropy, gukiza umwirondoro, kwaguka, kugabanuka, ubuzima bwinkono, ubushyuhe bwubushyuhe, guhuza amabuye, hamwe nibisubizo bya polishing.

Ubukonje bukwiye rero ntabwo ari umubare muto cyangwa munini uhari.

Nimyitwarire yimikorere ituma epoxy igera ahantu heza-kandi igahaguma igihe kirekire kugirango irangize akazi.

Ibibazo Bikunze Kubazwa Kubijyanye na Epoxy yo hasi-na-Viscosity

1. Epoxy-viscosity nkeya epoxy iruta amabuye?

Epoxy-viscosity nkeya nibyiza mugihe icyifuzo nyamukuru ari ukwinjira mumyenge myiza, micro-crack, granite yuzuye, cyangwa ibuye ryatewe na vacuum. Ntabwo ihita iba nziza kubusa, gusana guhagaritse, cyangwa ibikoresho byoroshye cyane aho gutemba gukabije bishobora kongera amazi no gukoresha resin.

2. Ni ubuhe bwoko bwa epoxy ya viscosity nakagombye gukoresha kumenagura amabuye?

Imisatsi myiza yimisatsi isanzwe yungukirwa na epoxy yo hasi-viscosity kuko resin ikeneye kwinjira imbere. Igice kinini gishobora gusaba sisitemu iringaniye cyangwa yo hejuru-yumubiri ihuza kwinjiza no kugumana bihagije kugirango inenge yuzure neza nyuma yo gukira.

3. Epoxy yo hejuru cyane irakomeye kuruta epoxy nkeya?

Ntabwo ari ngombwa. Ubukonje budashidikanywaho ntibugaragaza neza imbaraga zanyuma. Imbaraga ziterwa na chimie resin, chimie ikomeye, kuvanga igipimo, gukiza indwara, gufatira hamwe, gushushanya, hamwe no guhuza ibikorwa.

4. Kuki epoxy idakabije cyane ikoresha resin nyinshi kumabuye?

Resin-viscosity resin irashobora kugenda cyane mumyenge ihuriweho nubusa. Ibyo birashobora kunoza imbaraga, ariko birashobora kandi kongera ibicuruzwa mugihe ibuye ryinjiza resin irenze akarere gakeneye kuvurwa. Gupima resin ikoreshwa mugihe cyibigeragezo mbere yo kugura byinshi.

5. Epoxy imwe irashobora gukoreshwa mukwinjira no kuzuza icyarimwe?

Rimwe na rimwe, kugenzura-gutemba birashobora gukora imirimo yombi, ariko igisubizo giterwa nubwoko bwamabuye, ubugari bwikigero, imvugo ya resin, gukiza imyitwarire, kugabanuka cyangwa kwaguka, nibisabwa kurangiza. Kubisaba inzira, gutandukana no kuzuza ibyiciro bishobora gutanga ibisubizo bihamye.

Nigute ushobora guhuza Epoxy itemba mugutunganya amabuye nyayo

Guhitamo Epoxy bigomba gutangirira aho resin ikenera ingendo n'aho igomba kuguma. Micro-crack na vacuum infusion ikenera kugenda. Inenge nini no gusana vertical ikeneye kugumana. Kurangiza ubuso bikenera kuringaniza byombi. CPS itanga amakuru yingirakamaro, ariko igomba guhora isobanurwa hamwe nububiko bwamabuye, inenge ya geometrie, ubushyuhe, gukiza umwirondoro, rheologiya, nibisabwa kurangiza.

Tangira ufite inenge, ntabwo ari ikirango cya viscosity

Kuvunagura umusatsi, umwobo wa travertine ufunguye, micro-fissure yumukara-granite, gusana marble yera, hamwe na sex ya onikike ntabwo ari ikibazo kimwe. Ubugari bwuzuye, kwinjiza amabuye, icyerekezo, hamwe no kwiyumvisha ibintu bigomba gusobanura imyitwarire isabwa mbere yuko CPS itoranywa.

Huza imyitwarire ya resin kubikorwa

Umusatsi granite ucamo:
shyira imbere-viscosity penetration nigihe gihagije cyo gukora kugirango ugere mubice byimbere.

Kwinjiza Vacuum:
shyira imbere imbaraga nke zo gutemba, guhindagurika neza, hamwe nidirishya ryo gukiza igihe kirekire kugirango urangize.

Gushyigikira Mesh:
koresha imigenzereze ihanagura fibre neza nta gutemba gukabije.

Ubugari bwagutse:
shyira imbere kugumana resin, kubaka hejuru, hamwe no guhagarara neza aho kwinjira cyane.

Gusana neza:
suzuma imyitwarire ya thixotropique cyangwa itari sag aho kwishingikiriza gusa ku gaciro ka CPS.

Indangagaciro zisa na CPS zirashobora gutanga ibisubizo bitandukanye

Ibicuruzwa bifite ibisa nkibi byasohotse bishobora kwitwara ukundi kuko chimie ya formulaire, thixotropy, impagarara zubutaka, gukiza umuvuduko, kwaguka kwinshi, kurasa, kuzuza, no guhuza amabuye nabyo bigira ingaruka kumikorere. Abaguzi rero bagomba kugereranya imyitwarire yuzuye yibicuruzwa aho gutondekanya abatanga numubare umwe wijimye.

Ni iki abaguzi bagomba kugereranya mbere yo gutumiza byinshi?

Gereranya ububobere buvanze ku bushyuhe bwasobanuwe, igihe cyakazi, kwiyongera kwijimye mugihe cyo gusaba, ubujyakuzimu bwinjira, gutemba, gukoresha resin, gukiza umwirondoro, kugumana ubuso bwa nyuma, imyitwarire ya polish, guhagarara neza, hamwe no guhuza icyiciro. Noneho gerageza sisitemu yatondekanye kumabuye nyirizina mubihe bisanzwe byuruganda.

Icyifuzo gifatika

Niba ibisigazwa bidashobora kugera ku nenge, gabanya kurwanya imigezi. Niba yinjiye kure cyane cyangwa ikabura gusana, ongera igenzura cyangwa uhitemo ibyuzuye byuzuye. Niba imbaraga zombi zimbere hamwe no kurangiza hejuru birakomeye, tekereza gutandukana no kurangiza ibyiciro. Ibyiza bya epoxy nziza ntabwo aribwo buryo bworoshye cyangwa bunini cyane - ni formule igera ku bujyakuzimu busabwa, iguma aho ikenewe, kandi ikabyara icyapa gihamye nyuma yo gukira no gusya.

Ukeneye guhuza Epoxy itemba kubisabwa bya Kibuye?

Ubwoko bwamabuye, ubugari bwagutse, ubukana, ubushyuhe bwo gutunganya, icyerekezo cyerekanwe, gukiza igihe, nibisabwa birangira byose bigira ingaruka nziza guhitamo epoxy. Mbere yo kugura byinshi, gerageza sisitemu yabakandida kuri marble yawe nyayo, granite, onyx, igice cyigiciro cyinshi, inzira yo gusubiza inyuma, cyangwa umurongo wa vacuum-infusion.


Shakisha Veropoxy Kibuye Epoxy Sisitemu

Reba

  1. Umuryango mpuzamahanga ushinzwe ubuziranenge.
    ISO 25.
    ISO / TC 61.
    Umuryango mpuzamahanga ushinzwe ubuziranenge.
  2. ASTM Mpuzamahanga.
    ASTM D2196 - Uburyo busanzwe bwo Kwipimisha Kubintu bya Rheologiya yibikoresho bitari Newtonian by Rotational Viscometer.
    ASTM Mpuzamahanga.
    Ibipimo bya ASTM nubuhanga bwububiko bwibitabo.
  3. CYIZA SYSTEM Abakozi ba tekinike.
    CYIZA SYSTEM Umukoresha Igitabo & Ubuyobozi.
    Gougeon Brothers, Inc.
    SYSTEM YIZA CYANE.
  4. CYIZA SYSTEM Abakozi ba tekinike.
    Gusobanukirwa Epoxy Umuti n'ingaruka z'ubushyuhe.
    Gougeon Brothers, Inc.
    Epoxyworks / WEST SYSTEM Ibikoresho bya tekiniki.
  5. Ishami rya tekinike rya Gurit.
    Epoxy Resin Sisitemu: Gutunganya, Viscosity no Gukiza Ibiranga.
    Gurit.
    Ibicuruzwa bya tekiniki hamwe nubuyobozi bwo gutunganya ibintu.
  6. J. M. Dealy na K. F. Wissbrun.
    Gushonga Rheologiya n'uruhare rwayo mugutunganya plastike: Theory and Applices.
    Van Nostrand Reinhold.
    Gutunganya Polymer hamwe na Rheologiya Yerekana Ubuvanganzo.
  7. Christopher W. Macosko.
    Amahame ya Rheologiya, Ibipimo, na Porogaramu.
    Kaminuza ya Minnesota.
    Wiley-VCH, 1994.
  8. Charles Selwitz.
    Epoxy isubira mu kubungabunga amabuye.
    Ikigo cyo Kubungabunga Getty.
    Ubushakashatsi muburyo bwo kubungabunga, Getty Publications, 1992.