Nchịkọta ngwa ngwa:

Epoxy ntupu na-akwado okwute ga-emerịrị ntupu nkwado ahụ, jikọta nke ọma na slab ahụ, wee gwọọ ya n'ọsọ nke dabara na okpomọkụ ụlọ nrụpụta. Mmepụta oyi chọrọ kemistri nke ka na-etolite ike n'ọnọdụ oyi, ebe mmepụta ahịrị oge ọkọchị ma ọ bụ ihicha kwesịrị njikwa reactivity nke mere na epoxy anaghị agbanye ngwa ngwa. Họrọ usoro site na okpomọkụ ụlọ akwụkwọ n'ezie, ntupu mmiri, oge ọrụ, omume ọgwụgwọ, ọnọdụ okwute na ọsọ ahịrị-ọ bụghị site na viscosity ma ọ bụ oge ọgwụgwọ naanị.

Nkwado ntupu na-adị mfe site na mpụga.

A na-atụgharị mbadamba nkume, a na-etinye eriri fiberglass n'azụ, a na-etinye epoxy, na mgbe ọ gwọchara slab ahụ na-alaghachi na mmepụta.

N'ezie, nke a bụ otu n'ime usoro ndị ahụ ebe ụlọ ọrụ nwere ike ịmegharị otu mmegharị ahụ kwa ụbọchị ma na-enweta nsonaazụ dị iche site na Jenụwarị ruo August.

N'oge oyi, resin nwere ike ibu oke ma ghara ịgwọ ya ngwa ngwa. A ka na-ahụ eriri eriri ntupu n'ihi na epoxy adịghị mmiri ha nke ọma. Slabs na-anọkọ ogologo oge karịa ka a tụrụ anya ya, ndị na-arụ ọrụ na-amalite ịkwagharị ihe tupu ike zuru oke amalite.

N'oge okpomọkụ, ihe dị iche nwere ike ime. Epoxy na-aga nke ọma na mbụ, mana windo na-arụ ọrụ na-adị mkpụmkpụ. Otu nnukwu ogbe na-amalite ikpo ọkụ n'ime akpa ahụ, resin na-eto eto tupu e kpuchie slab ahụ dum, ma ọ bụ otu akụkụ nke ntupu na-enweta resin karịa nke ọzọ.

Mmeghachi omume doro anya bụ ịta viscosity ụta.

Ma viscosity bụ naanị otu akụkụ nke azịza.

Ajụjụ dị mkpa bụ ma a haziri sistemu resin-hardener zuru oke ka ọ gwọọ ya n'oge okpomọkụ nke ahịrị nkwado na-arụ ọrụ n'ezie.

Veropoxy na-ekewa ọnọdụ ndị a ugbu a site na raara onwe ya nye nkume epoxy usoro maka nkwado ntupu dị ala na oke okpomọkụ karịa ịgwọ otu usoro dị ka nrapado zuru ụwa ọnụ n'afọ niile.

Epoxy ntupu na-akwado okwute etinyere na slab mabul n'oge mmepụta ụlọ ọrụ

Kedu ihe bụ Nkwado Mesh Nkume?

Nkwado ntupu okwute bụ usoro nkwado nke ejiri eriri fiberglass ma ọ bụ akwa akwa ọzọ na-eme ka ejikọta ya na azụ azụ nke mbadamba nkume ebumpụta ụwa ma ọ bụ arụrụ arụ.

Ebumnuche abụghị ime ka slab ọ bụla bụrụ otu.

Ntupu na resin na-arụkọ ọrụ ọnụ dị ka oyi akwa nkwado nke nwere ike inye aka mee ka ihe na-esighi ike guzosie ike, belata ihe ize ndụ nke ịgbasa, ma melite njikwa njikwa n'oge nhazi, mbugharị, nrụpụta na ntinye.

Kedu ihe kpatara slabs na-esighi ike chọrọ nkwado

Nkume eke dị iche iche.

Ngwongwo abụọ e bepụrụ site na otu ngọngọ nwere ike ịnwe oke ịnweta dị iche iche, veins, micro-cracks, pores, nha kristal, na nrụgide dị n'ime.

Ihe ịchọ mma nke ukwuu nwere ike bụrụ ihe ịma aka karịsịa n'ihi na njirimara a na-ahụ anya nke ndị na-azụ ahịa na-eji-nnukwu kristal, veins dị egwu, ngbanwe ịnweta, na usoro pụrụ iche-nwere ike ịmepụta adịghị ike mpaghara.

Nnyocha na nkume ụlọ na-enweghị isi na nke dị egwu egosiwo na sistemụ epoxy nke iko-fiber nwere ike igbochi mgbasa mgbasa ma melite omume arụ ọrụ, ọ bụ ezie na nkwado nkwado dịgasị iche dabere na nkume, resin, eriri usoro, na ngwa ngwa.

Nkwado ntupu na-emekarị tupu ihicha ya

Maka ọtụtụ ahịrị mmepụta slab, a na-eme nkwado tupu polishing ikpeazụ.

Okpokoro nkwado ahụ kwesịrị ịgwọta nke ọma tupu slab ahụ alaghachi na njikwa, ichikota, ihicha, ma ọ bụ njem mgbada.

Nke a na-eme ka ọgwụgwọ oge bụrụ okwu mmepụta, ọ bụghị naanị nkọwa ụlọ nyocha.

Kedu ihe Epoxy nkwado Mesh dị mma kwesịrị ime?

Epoxy na-akwado ntupu bara uru chọrọ ọtụtụ njirimara n'otu oge.

Weta ntupu fiberglass ahụ

Resin ga-agaferịrị na gburugburu eriri ntupu kama ịnọdụ n'elu akwa ahụ.

Mwepu mmiri nke ọma na-emepụta kọntaktị n'etiti eriri, epoxy, na mkpụrụ okwute.

Ọ bụrụ na a na-ahụ nnukwu ebe ọcha ma ọ bụ akọrọ na ntupu, nkwado agaghị ekwekọ.

Njikọ na nkume elu

Ịwe akwa eriri dị mma ezughị ma ọ bụrụ na epoxy anaghị agbaso nke ọma na slab.

Uzuzu, mmiri mmiri, ihe fọdụrụ slurry, mmanụ, wax, ihe ntọhapụ, na ihe ndị na-adịghị eme ihe niile nwere ike ịmepụta ihe na-adịghị ike.

Nọgide na-arụ ọrụ ogologo oge

Onye na-arụ ọrụ chọrọ oge zuru ezu iji gbasaa epoxy n'ofe slab ahụ niile wee mebie ntupu ahụ kpamkpam.

Usoro nke gels ọkara site na nnukwu slab nwere ike ịmepụta mpaghara siri ike na nke na-adịghị ike n'otu oyi akwa nkwado ahụ.

gwọọ ngwa ngwa maka ahịrị

Oge ọrụ enweghịkwa njedebe.

Ozugbo a na-ehichapụ ntupu ahụ nke ọma na resin dị, usoro ahụ ga-enwerịrị ike njikwa zuru oke iji mee ka slab ahụ site na mmepụta na ọsọ ọsọ bara uru.

Zere oke mmiri ozuzo

Ọ bụrụ na resin dị oke mmiri n'okpuru ọnọdụ nrụpụta n'ezie, ọ nwere ike isi na ntupu pụọ, gbakọta n'akụkụ ọnụ ala, ma ọ bụ mepụta nkesa resin na-enweghị isi.

Nọgide na-agbanwe agbanwe site na mgbanwe oge

Nke a na-abụkarị ihe kacha sie ike chọrọ.

Resin na-arụ ọrụ nke ọma na 22 Celsius nwere ike ịkpa àgwà dị iche na 10 Celsius ma ọ bụ 32 Celsius.

Kedu ihe kpatara nkwado nhịahụ oge okpomọkụ na oyi chọrọ atụmatụ dị iche iche

Ngwọta epoxy na-enwe mmetụta okpomọkụ.

Mgbe okpomọkụ dara, epoxy na-adịghị agwọta n'ozuzu na-aghọwanye viscous na mmeghachi omume kemịkal na-ebelata.

Mgbe okpomọkụ na-ebili, resin na-adịkarị mfe ịfesa, mana mmeghachi omume ọgwụgwọ na-emekwa ngwa ngwa.

Nke a na-emepụta ihe ize ndụ mmepụta ihe.

Ọnọdụ mmepụta Omume resin isi Ihe ize ndụ a na-ahụkarị Ihe Factory chọrọ
Ụlọ ọrụ oyi oyi Viscosity dị elu na mmeghachi omume nwayọ Mwe mmiri na-adịghị mma, ọgwụgwọ egbu oge, njikwa oge mbụ Chemistry na-agwọ obere okpomọkụ
Ọnọdụ adịghị mma Ntughari na mmeghachi omume ziri ezi Mgbanwe na mgbanwe okpomọkụ Window na-arụ ọrụ kwụsiri ike yana ọgwụgwọ enwere ike ịmegharị
Ụlọ ọrụ okpomọkụ na-ekpo ọkụ Viscosity mmalite dị ala na mmeghachi omume ngwa ngwa Oge ọrụ dị mkpirikpi, ịgbara ngwa ngwa, ngwa na-ezighi ezi Mmeghachi omume okpomọkụ dị elu achịkwara
Ahịrị ihicha kpụ ọkụ n'ọnụ Ntinye ọkụ ngwa ngwa ka emechara ngwa Ngwọta akabeghị aka ma ọ bụ mmepe gel na-ezighi ezi Sistemu emebere maka ọnọdụ ahịrị ihicha

Isi ihe dị mfe:

Oge oyi na ọkọchị chọrọ njikwa ọgwụgwọ dị iche iche ọbụlagodi mgbe viscosity ebumnuche dị na mpempe akwụkwọ.

Nkwado nchikota oyi: kedu ihe na-agbanwe n'obere okpomọkụ?

Onye ọrụ na-etinye epoxy dị ala maka nkwado ntupu okwute na ụlọ ọrụ oyi oyi

Resin na-esiwanye ike ịgbasa

Ka epoxy na-adịghị agwọ ọrịa na-ajụ oyi, viscosity na-ebilikarị.

Rola ma ọ bụ mgbasa ozi chọrọ mbọ karịa. Resin na-eji nwayọọ nwayọọ na-agafe na fiberglass, na eriri ntupu nwere ike ịnọgide na-adị ntakịrị.

Nke a na-apụta ìhè karịsịa na nnukwu slabs ebe onye ọrụ kwesịrị ikpuchi ọtụtụ mita square mgbe niile.

Ntinye n'ime nkume nwere ike ibelata

Nkwado ntupu anaghị adabere naanị na njikọta na akwa ahụ.

Resin ahụ chọkwara mmekọrịta zuru oke na pores, adịghị ike, na obere ntụpọ n'elu azụ nke slab ahụ.

Ọ bụrụ na resin na-adị oke oke, mmiri mmiri na ntinye elu nwere ike ghara ịdị irè.

Oge ọgwụgwọ na-aghọ enweghị atụ

Usoro okpomọkụ nke ụlọ nwere ike ka na-emecha gwọọ ọnọdụ oyi, ma "n'ikpeazụ" abụghị nkọwapụta mmepụta.

Ọ bụrụ na slab ahụ chọrọ ugboro abụọ ogologo oge tupu ejikwa ya, ebe a na-akwado ya ga-abụ ọkpọ.

Ụlọ ọrụ na-amalite ime mkpebi dị ize ndụ dịka:

  • slabs na-akpụ akpụ mgbe resin ka na-acha akwụkwọ ndụ akwụkwọ ndụ;
  • na-ekpokọ mbadamba nkume ndị agbasiri ike n'oge;
  • na-agbakwunye ike siri ike;
  • iji kpo oku na-achịkwaghị achịkwa; ma ọ bụ
  • na-anabata ntupu gwọrọ akụkụ.

Ụzọ mkpirisi ndị ahụ na-emepụtakarị mgbanwe.

Mgbe ntupu nkwado dị ala na-eme uche

Epoxy-ọkwa oyi ekwesịghị ịbụ naanị ihe e ji emepụta ihe na-esikwu ike nke agbakwunyere na ụlọ ọrụ mmepụta ihe.

Ekwesịrị ịhazi kemịkalụ ọgwụgwọ ahụ n'onwe ya ka ọ nọgide na-emeghachi omume n'okpuru ọnọdụ oyi kariri.

Veropoxy's Ọnọdụ okpomọkụ dị ala maka nkwado ntupu nkume - 4090 / WBA25Q A na-edobe ya ugbu a maka mmepụta ihe dịka 10 Celsius.

Sistemu ebipụtara ya na-eji:

  • Nchikota resin-hardener 4090 / WBA25Q;
  • 100:25 ngwakọta ngwakọta site na ibu;
  • 400–600 CPS viscosity;
  • ihe dị ka nkeji 50 nke ọgwụgwọ; na
  • ihe dịka 10°C tụrụ aro ka ọ rụọ ọrụ.

Akụkụ dị mkpa abụghị na "nkeji 50 dị mma karịa nkeji 60."

Ihe bara uru bụ na a na-emepụta usoro ahụ iji zụlite ọrụ ọgwụgwọ n'okpuru ọnọdụ oyi ebe onye na-agba ume nwere ike ịmalite ngwa ngwa ngwa ngwa.

Kedu onye kwesịrị ịtụle usoro oge oyi?

Ọ dị mkpa mgbe:

  • Okpomọkụ ụlọ ọrụ na-erute 10 Celsius mgbe niile;
  • nkume n'onwe ya bụ oyi mgbe nchekwa abalị;
  • nkwado ntupu na-eme na mpaghara mmepụta adịghị ọkụ;
  • slabs ga-akpali obere oge ka mkwado;
  • oyi ọgwụgwọ igbu oge na-ebelata akara throughput; ma ọ bụ
  • ndị na-arụ ọrụ na-eji aka na-akwụ ụgwọ maka ọgwụgwọ ngwa ngwa.

Nkwado Mesh Summer: Ihe kpatara na ọ naghị adị mma mgbe niile

Onye ọrụ na-etinye epoxy okpomọkụ dị elu maka ntupu okwute na-akwado ahịrị mmepụta kpụ ọkụ n'ọnụ

Ihu igwe na-ekpo ọkụ na-adị mfe na mbụ.

Epoxy na-aga nke ọma. Fiberglass na-apụta ìhè ngwa ngwa. Ndị na-arụ ọrụ nwere ike ibugharị resin gafee slab na obere mbọ.

Mgbe ahụ, elekere na-amalite ịrụ ọrụ megide ha.

Oge ọrụ na-adị mkpụmkpụ

Okpomọkụ dị elu n'ozuzu na-eme ka mmeghachi omume epoxy dị ngwa ngwa.

Resin nwere ike ịmalite na viscosity nwere ike ịrụ ọrụ mana ọ na-eto ngwa ngwa karịa ka a tụrụ anya ya.

N'elu slab buru ibu, ebe mbụ nwere ike ịsa mmiri nke ọma ebe mpaghara ikpeazụ na-enweta resin nke malitelarị wuo viscosity.

Nnukwu batches nwere ike ikpo ọkụ ọbụna ngwa ngwa

Ọgwụgwọ Epoxy bụ exothermic.

Nnukwu ngwakọta agwakọta na bọket miri emi na-ejigide okpomọkụ.

Okpomọkụ ejidere karịa nwere ike mee ka mmeghachi omume dịkwuo ngwa ngwa.

Nke a bụ otu ihe mere ndị na-arụ ọrụ n'oge okpomọkụ na-ahụ mgbe ụfọdụ ka ịwụ na-ekpo ọkụ mgbe resin agbasala n'ofe mbadamba ahụ ka na-arụ ọrụ ogologo oge.

Ahịrị ihicha na-agbakwunye mgbanwe okpomọkụ ọzọ

Ụlọ ọrụ ndị na-eji ahịrị ekpo ọkụ ma ọ bụ oven na-enye aka kwesịrị ịtụle ọ bụghị naanị ọnụ ụlọ kamakwa okpomọkụ ewepụtara mgbe etinyere ya.

Usoro ọgwụgwọ ahụ ga-anabatarịrị usoro ahụ na-enweghị ike ijide ngwa ngwa.

Mgbe Epoxy nkwado ntupu dị elu na-eme uche

Maka ụlọ ọrụ na-ekpo ọkụ na mmepụta ahịrị ihicha, ihe a na-achịkwa na-achịkwa mmeghachi omume.

The epoxy ka chọrọ ezigbo wet na eruba, ma usoro ọgwụgwọ kwesịrị ichekwa oge ngwa zuru ezu iji mechaa slab mgbe niile.

Veropoxy's Epoxy na-enweghị isi okpomọkụ dị elu maka nkwado ntupu nkume - 4090 / BCO25Q-14 emebere ya ugbu a maka 28°C+ na ọnọdụ ihicha.

Nkọwapụta ya ebipụtara gụnyere:

  • 4090 / BCO25Q-14 usoro;
  • 100:25 resin-to-hardener ruru n'ịdị arọ;
  • 400–600 CPS viscosity;
  • ihe dị ka nkeji 60 nke ọgwụgwọ;
  • ọnọdụ okpomọkụ dị elu / 28 ° C +; na
  • arụ ọrụ na-enweghị isi maka gburugburu mmepụta ihe na-aga n'ihu.

Kedu onye kwesịrị ịtụle usoro okpomọkụ dị elu?

Ọ dị mkpa mgbe:

  • Okpomọkụ ụlọ ọrụ okpomọkụ na-adịkarị karịa 28 Celsius;
  • nkwado ntupu na-eji oven ihicha ma ọ bụ ihe ebu ọkụ;
  • ọkọlọtọ epoxy amalite ndim tupu ngwa zuru ezu;
  • nnukwu slabs chọrọ ogologo oge nkwụsị mmiri;
  • ndị na-arụ ọrụ na-agwakọta ọtụtụ kilogram kwa ogbe;
  • factory na-agba ọsọ na-aga n'ihu akpaka ahịrị; ma ọ bụ
  • Nkwekọrịta oge ọrụ dị mkpa karịa ọsọ ọgwụgwọ kachasị.

Kedu ihe kpatara otu 400–600 CPS anaghị apụta otu ngwaahịa ahụ

Nke a nwere ike ịbụ nkuzi nke ndị na-azụ ihe kacha mkpa na akụkọ.

Sistemu nkwado ntupu Veropoxy abụọ na-ebipụta ugbu a ihe dị ka viscosity CPS 400–600.

Ha abụọ na-ejikwa nha 100:25 site na ịdị arọ.

Otu n'ime ha ka emebere ihe dịka 10 Celsius C mmepụta na nke ọzọ gburugburu 28 Celsius ma ọ bụ ọnọdụ ihicha.

Nke ahụ pụtara na ezigbo ọdịiche abụghị naanị viscosity.

Kemịlụ siri ike na ọgwụgwọ zuru oke na-arụ ọtụtụ ọrụ nke oge.

Nkọwapụta Usoro oyi Sistemu okpomọkụ/Okpomọkụ dị elu
Sistemu 4090 / WBA25Q 4090 / BCO25Q-14
Ojiji nke izizi Nkwado ntupu dị ala Nkwado ntupu nke oke okpomọkụ / ihicha
Ọnọdụ okpomọkụ akwadoro Ihe dị ka 10 Celsius C 28°C+/ ọnọdụ akara ọkụ
Ngwakọta ngwakọta 100:25 n’ịdị arọ 100:25 n’ịdị arọ
Ebipụtara viscosity 400-600 CPS 400-600 CPS
E bipụtara oge ọgwụgwọ Ihe dị ka nkeji iri ise Ihe dị ka nkeji iri isii
Isi nhọrọ kpatara Ngwọta a pụrụ ịdabere na ya na ọnọdụ oyi Ngwọta a na-achịkwa n'ọnọdụ ọkụ

Mwepu onye zụrụ: Ahọrọla oge ọkọchị na oyi ntupu na-akwado nkwado site na viscosity naanị. Sistemu abụọ nwere ike ibipụta otu CPS na oke ma na-akpa àgwà dị iche iche n'ihi na kemịkalụ siri ike na profaịlụ ha emebere maka oke okpomọkụ dị iche iche.

Mesh Wet-out dị mkpa karịa ịkpuchi akwa ákwà

Ntupu nwere ike ịdị ka “kpuchiri ekpuchi” ebe a na-etunye ya nke ọma.

Ebumnuche bụ ka resin mee ka eriri ndị ahụ dị mmiri wee mepụta mmekọrịta chiri anya n'etiti akwa akwa na elu nkume.

Kedu ihe ịsa mmiri kwesịrị ekwesị dị ka

Mgbe ejiri usoro epoxy doro anya wesara fiberglass mmiri nke ọma, eriri ndị ahụ na-aghọwanye nke ọma ma na-ejikọta ya na oyi akwa resin.

Mpaghara ọcha na-acha akọrọ nwere ike igosi afọ ime ezughị ezu.

Ntuziaka epoxy nke ụlọ ọrụ maka ngwa fiberglass n'otu aka ahụ na-emesi ike ịgbasa resin site na mpaghara mmiri mmiri n'ime akwa akọrọ na iwepu resin ngafe tupu gelation.

Obere resin na-emepụta ntupu akọrọ

Ọ bụrụ na ọnụọgụ ngwa dị obere:

  • eriri na-anọgide na-akọrọ;
  • kọntaktị nkume na-aghọ ekwekọghị ekwekọ;
  • oghere dị n'okpuru ntupu;
  • nkwado mpaghara na-esiwanye ike; na
  • ekpepụsịla nwere ike ịmalite site na mpaghara ejikọtara nke ọma.

Oke resin adịghị mma ozugbo

Oke resin na-agbakwunye ọnụ ahịa na ibu na-enweghị nkwalite nkwalite.

Nnukwu ọdọ mmiri nwekwara ike ịmepụta ọgwụgwọ na-enweghị isi, mpaghara nwere resin, na mmụba okpomọkụ na-enweghị isi.

Ebumnobi a zuru oke nke nwere oke resin a na-achịkwa.

Nkwadebe dị n'elu nwere ike ikpebi ma ntupu ahụ ga-ejikọta ya

Ọbụlagodi epoxy kacha mma enweghị ike ijikọ ntụkwasị obi na mmetọ.

Wepu uzuzu na slurry

Ịkpụcha nkume na nhazigharị na-ahapụ ezigbo uzuzu ịnweta na slurry fọdụrụnụ.

Ọ bụrụ na ụmụ irighiri ihe ndị ahụ anọgide na slab, epoxy nwere ike jikọta na ájá kama ịbụ nkume.

Nsonaazụ nwere ike ịdị ka nke a na-anabata na mbụ wee bee mgbe a na-ejikwa ya.

Ejikwa mmiri mmiri

Nkume dị mmiri mmiri nwere ike igbochi ọtụtụ usoro njikọ epoxy.

Ọ bụrụ na slabs na-ahapụ ahịrị ịsa ahụ tupu nkwado ntupu, ụlọ ọrụ mmepụta ihe kwesịrị ikwenye na elu azụ eruola ọnọdụ akọrọ na-anakwere tupu itinye resin.

Wepu ihe ndị rụrụ arụ

Nkume ndị na-emebi emebi nwere ike ịnwe ọka na-adịghị ike ma ọ bụ mpaghara ịnweta n'azụ.

Ijikọ ntupu na ihe ewepụrụla na slab anaghị edozi nsogbu dị n'okpuru.

Ngwakọta ọnụ ka dị mkpa n'oge okpomọkụ na oyi

E kwesịghị idozi nsogbu okpomọkụ site n'ịgbanwe nha ngwakọta.

Sistemu nkwado ntupu Veropoxy dị ugbu a na-akọwapụta 100:25 resin-to-hardener site n'ịdị arọ.

Oke ahụ kwesịrị ịdịgide belụsọ ma onye na-ebubata ya nyere usoro akwadoro dị iche.

E tinyekwala ihe siri ike n'oge oyi

Hardener ọzọ anaghị atụgharị epoxy nkịtị ka ọ bụrụ epoxy dị ala.

Ịgwakọta ọnụ na-adịghị nwere ike ibelata ogo ọgwụgwọ ma mepụta akụrụngwa na-ekwekọghị ekwekọ.

Emela ka ike sie ike n'oge okpomọkụ

N'otu aka ahụ, ibelata hardener abụghị ụzọ kwesịrị ekwesị iji mepụta usoro okpomọkụ dị nwayọọ.

Ụzọ ziri ezi bụ iji kemistri ọgwụgwọ emebere maka mmepụta okpomọkụ dị elu.

Maka nkọwa miri emi, lee Ntuziaka Ratio Mixing Epoxy Resin maka Nhazi Nkume.

Kedu ka viscosity si emetụta nkwado ntupu

Nkwado ntupu chọrọ nguzozi.

Resin ga-adị gịrịgịrị iji mee ka eriri ndị ahụ wee gbasaa n'ofe mbadamba ahụ, mana ejiri ya nke ọma nke na ọ bụghị naanị na ọ ga-agbapụ na oyi akwa nkwado ahụ.

Ọ bụrụ na viscosity dị oke elu

Onye ọrụ nwere ike ịhụ:

  • adịghị mma ntupu impregnation;
  • nnukwu ihe mgbochi rola;
  • Mpaghara akwa akọrọ;
  • Ikuku ọnyà ọzọ;
  • elu ọrụ mgbalị; na
  • nkesa resin na-enweghị isi.

Ọ bụrụ na viscosity dị obere

Nsogbu nwere ike gụnyere:

  • mkpọpu n'akụkụ slab;
  • nchịkọta resin n'okpuru slab;
  • oke nnabata n'ime nkume porous;
  • wuo elu ala; na
  • elu ihe oriri.

Nke a bụ ya mere "nchịkwa obere viscosity" ji abụkarị asụsụ bara uru karịa "CPS kacha ala enwere ike."

Maka nkọwa ndị ọzọ na mkpebi a, lee Viscosity dị ala vs ntuziaka Epoxy dị elu.

Akwụkwọ nkwado ntupu vs ahịrị mmepụta akpaaka

Imepụta akwụkwọ ntuziaka chọrọ oge ọrụ enyi na onye ọrụ

Ndị ọrụ ntuziaka chọrọ oge zuru ezu iji:

  • dobe ntupu;
  • ngwakọta epoxy;
  • wụsa resin;
  • gbasaa ya n'ofe mbadamba;
  • arụ ọrụ resin n'ime akọrọ ebe;
  • wepụ ihe ngafe; na
  • dozie wrinkles ma ọ bụ ntụpọ akọrọ mpaghara.

Ọ bụrụ na epoxy na-emeghachi omume ngwa ngwa, ogo ngwa na-adabere oke na ọsọ onye ọrụ.

Ahịrị akpaghị aka chọrọ nkwugharị

Ahịrị akpaaka ma ọ bụ nke ọkara akpaka nwere ike itinye resin ngwa ngwa, mana ha na-ewebata ihe dị iche iche: oge okirikiri nwere ike imegharị.

Otu ogbe ekwesịghị ịmalite gelling ọtụtụ nkeji tupu oge ọzọ naanị n'ihi na okpomọkụ ihe gbanwere.

Maka sistemụ akpaaka, nyochaa:

  • metering ziri ezi;
  • ngwakọta agbanwe agbanwe;
  • resin okpomọkụ;
  • ọsọ ahịrị;
  • nrụgide rola;
  • nhazi nri ntupu;
  • oven okpomọkụ; na
  • njikwa oge mgbe ọgwụgwọ gasịrị.

Ọdịda nkwado ntupu a na-ahụkarị yana ihe ha na-apụtakarị

Nsogbu achọpụtara Ihe nwere ike ime Ihe mbụ ị ga-enyocha
Ntupu peels site na nkume Elu emetọọ, mmiri na-adịghị mma, ọgwụgwọ ezughị ezu Nhicha elu, mmiri mmiri, mkpuchi resin na ọnọdụ ọgwụgwọ
Ebe ntupu na-acha ọcha ka dị Ezughị oke mmiri ma ọ bụ resin dị oke viscous Ọnụọgụ ngwa, viscosity na usoro rola
Epoxy na-adị nro n'oge oyi Okpomọkụ dị n'okpuru oke nhazi Ambient, nkume na resin okpomọkụ
Epoxy gels ngwa ngwa n'oge okpomọkụ Okpomọkụ dị elu ma ọ bụ nnukwu ogbe exothermic Batch size, ihe onwunwe okpomọkụ na hardener usoro
Resin na-agbapụ n'akụkụ slab Ihe karịrị oke ma ọ bụ sistemu mmiri karịrị akarị Ọnụọgụ ngwa na viscosity na okpomọkụ mmepụta
Afụ ma ọ bụ oghere n'okpuru ntupu Mmiri na-adịghị mma, ikuku tọrọ atọ ma ọ bụ ntụgharị na-enweghị isi Usoro ngwa na kọntaktị akwa
Ebe dị iche iche na-agwọta dị iche iche Ngwakọta na-adịghị mma ma ọ bụ okpomọkụ na-adịghị mma Ịgwakọta otu, oke na okpomọkụ slab
slab na-agbaji ma ọ kwadochara ya Nkwalite ezughị oke maka nhazi ntụpọ nkume Ọnọdụ nkume, nkọwa ntupu, mkpuchi resin na ihe achọrọ n'ezie

Ihe kpatara na “akọrọ iji metụ aka” abụghị ọkọlọtọ njikwa a pụrụ ịdabere na ya

Ngwongwo nwere ike ịdị na-akpọ nkụ n'elu ebe usoro nkwado na-emepụtabeghị arụmọrụ zuru oke maka njikwa.

Nnyocha na-enyocha nkwado okwute ụlọ ọrụ achọpụtala kpọmkwem na ụlọ ọrụ mgbe ụfọdụ na-alaghachi slabs na mmepụta dabere na "mmetụta akọrọ" siri ike karịa ihe ndị na-emepụta resin chọrọ ọgwụgwọ.

Nke a na-ebute ihe egwu na-enweghị isi.

Kọwaa ezigbo njikwa njikwa

Ụlọ ọrụ mmepụta ihe kwesịrị ịchọpụta ihe slab gbasiri ike ga-adị ndụ na-esote:

  • ebuli;
  • ntụgharị;
  • ụgbọ njem ụgbọ;
  • ikpokọta;
  • nhazi nhazi;
  • polishing; ma ọ bụ
  • imepụta ihe.

Mgbe ahụ, ntozu ọgwụgwọ kwesịrị kwekọọ na ibu ahụ n'ezie.

Otu esi ahọrọ Summer vs Winter Mesh Backing Epoxy

Ọ bụrụ na ọnọdụ mmepụta gị bụ… Nye ụzọ… Ntak
Ụlọ ọrụ dị nso 10 Celsius Chemistry na-agwọ obere okpomọkụ Sistemu ọkọlọtọ nwere ike gwọta nwayọ nwayọ ma weta ntupu na-adịghị mma
Nkume oyi sitere na nchekwa dị n'èzí Lelee okpomọkụ nkume tupu ngwa Ala ahụ nwere ike ịnọgide na-ajụ oyi karịa ikuku ụlọ ọrụ
Ụlọ ọrụ okpomọkụ dị elu karịa 28 Celsius Mmeghachi omume okpomọkụ dị elu achịkwara Na-echekwa oge ọrụ bara uru
Na-ekpocha oven ma ọ bụ akara ọkụ Sistemụ dakọtara na oke okpomọkụ / ahịrị Na-ezere ọgwụgwọ akabeghị aka n'oge ikpo ọkụ
Nkwado nnukwu slab akwụkwọ ntuziaka Ogologo oge oghere zuru oke Ndị na-arụ ọrụ chọrọ oge maka mmiri zuru ezu
Ahịrị na-aga n'ihu na-akpaghị aka Ogbe-na-ogbe ọgwụgwọ agbanwe agbanwe Ọsọ ahịrị kwụsiri ike dabere na omume mmeghachi omume enwere ike imegharị
Nkume porous nke ukwuu Achịkwara eruba na oriri resin Mfefe resin nwere ike ịla n'iyi n'ime efere ahụ
Nkume osisi osisi na-emebi emebi nke ukwuu Kwado njupụta ntupu na sistemu nkwado zuru oke Epoxy naanị anaghị ekpebi ike ikpeazụ

Otu esi anwale Epoxy nkwado ntupu tupu ịtụ ahịa nnukwu

Nzọụkwụ 1: Jiri ezigbo mmepụta nkume

Nwalee epoxy n'otu granite, marble, nkume arụpụtara arụ ọrụ, ma ọ bụ slabs dị egwu nke usoro mmepụta ihe.

Nzọụkwụ 2: Jiri ntupu n'ezie

Njupụta ntupu, nhazi eriri, na ọgwụgwọ elu nwere ike imetụta ọchịchọ resin na wetting.

Kwụpụ 3: Nwalee na ọnọdụ okpomọkụ nke oge

Ekwesịrị ịnwale epoxy oyi n'akụkụ ọnọdụ nhazi oyi a na-atụ anya ya.

A ga-anwale ngwaahịa okpomọkụ n'ezie n'ọnọdụ ahịrị okpomọkụ dị elu.

Nzọụkwụ 4: Dekọọ oge ngwa

Tụọ oge site na ịgwakọta ruo mgbe mmiri niile na-agbakọta.

Kwụpụ 5: Dekọọ oriri resin

Soro gram ma ọ bụ kilogram kwa square mita ma ọ bụ kwa mbadamba.

Nke a dị oke mkpa iji tụnyere ezi ọnụ ahịa mmepụta.

Nzọụkwụ 6: Lelee ntupu na anya

Nyochaa mpaghara akọrọ, afụ, wrinkles, ibuli ọnụ, na mkpuchi resin na-enweghị isi.

Kwụpụ 7: Nye ohere ọgwụgwọ akọwapụtara

Ebibila oge ọgwụgwọ naanị n'ihi na elu ahụ na-akpọ nkụ.

Kwụpụ 8: Gbaa slab ahụ site na njikwa n'ezie

Bulite ya, bugharịa ya, tụgharịa, ma weghachi ya na mmepụta dịka usoro ụlọ ọrụ nkịtị si dị.

Kwụpụ 9: Tulee ọtụtụ slabs

Otu ihe nlele na-aga nke ọma ezughị maka nnabata nnukwu.

Ngbanwe okwute pụtara na ekwesịrị ịlele sistemu ahụ n'ofe mbadamba ihe nnọchi anya.

Ndepụta nlebanya azụ ahịa Epoxy Mesh

Ajụjụ ndị na-eweta ngwaahịa Ihe Mere O Ji Dị Mkpa
Kedu oke okpomoku ka emere ike siri ike maka? Na-ekpebi ịdị mma ọgwụgwọ oge
Kedu ihe bụ viscosity agwakọta na okpomọkụ ule ekwuputara? Na-enyere aka ịkọ ntupu mmiri ga-apụ na mpụta
Gịnị bụ oke resin-to-hardener? Achọrọ maka ọgwụgwọ ugboro ugboro
Ọ̀tụ̀tụ̀ a bụ site n'ịdị arọ ma ọ bụ olu? Na-egbochi mperi doses
Ogologo oge ole ka windo ọrụ bara uru? Na-ekpebi ma enwere ike mechaa slab zuru ezu
Kedu mgbe enwere ike ijikwa slab ahụ n'enweghị nsogbu? Ọ bara uru karịa “oge ọgwụgwọ” na-edoghị anya
Ngwaahịa a dabara adaba maka ahịrị akwụkwọ ntuziaka ma ọ bụ akpaaka? Ọsọ ngwa na-agbanwe profaịlụ ọgwụgwọ achọrọ
Ọ dị mma maka ihicha-ahịrị ma ọ bụ ikpo ọkụ oven? Dị oke egwu maka usoro mmepụta ọkụ
Anyị nwere ike ịnwale ihe nlele na nkume na ntupu anyị? Nnwale ụlọ mmepụta ihe n'ezie na-ekpughe ndakọrịta
Kedu ka arụmọrụ si agbanwe n'etiti batches? Mmepụta na-aga n'ihu na-adabere na nkwughachi

Mmejọ nkwado ntupu a na-ahụkarị iji zere

Iji otu epoxy n'afọ niile na-enweghị nnwale oge

Ọ bụrụ na okpomọkụ ụlọ ọrụ na-agbanwe n'ụzọ dị ịrịba ama n'etiti oyi na okpomọkụ, otu usoro nwere ike ọ gaghị enye otu windo usoro ahụ n'afọ niile.

Na-agbakwunye ike ike n'oge oyi

Nke a abụghị ihe a na-achịkwa maka kemistri na-agwọ obere okpomọkụ.

Mbelata hardener n'oge okpomọkụ

Nke a abụghị usoro dị mma maka ịgbatị oge ọrụ.

Na-etinye ntupu n'elu nkume uzuzu uzuzu

Epoxy nwere ike ijikọ na mmetọ kama ịkọbe mbadamba.

Na-eche na mkpuchi a na-ahụ anya pụtara mmiri zuru oke

Resin ga-emerịrị ntupu ahụ ma mepụta kọntaktị a pụrụ ịdabere na ya na nkume.

Na-ebugharị slabs ozugbo elu ahụ kpọrọ nkụ

Ọnọdụ nkụchi aka anaghị egosi ike njikwa zuru oke.

Na-eleghara okpomọkụ nkume anya

Ala ahụ n'onwe ya nwere ike ịdị oyi ma ọ bụ dị ọkụ karịa ikuku ụlọ ọrụ.

Atụle epoxy naanị site na ọnụahịa kwa kilogram

Ngwaahịa dị ọnụ ala nke na-eri ọtụtụ resin, na-ebelata ahịrị, ma ọ bụ mepụta nrụpụta ọrụ nwere ike ịdị ọnụ karịa otu slab emechara.

Nkwanye: Họrọ usoro ọgwụgwọ gburugburu oge mmepụta

Epoxy na-akwado ntupu kacha mma abụghị naanị ngwaahịa nwere ọgwụgwọ kachasị ọsọ ma ọ bụ viscosity kacha ala.

Ọ bụ usoro na-ahapụ ụlọ ọrụ mmepụta ihe n'ụzọ zuru ezu mmiri ntupu, na-ejigide njikọ a pụrụ ịdabere na ya, ma rute ike njikwa dị mma n'oge mmepụta okpomọkụ.

Ọ bụrụ na ụlọ ọrụ mmepụta ihe na-arụ ọrụ n'akụkụ 10 Celsius C n'oge oyi, buru ụzọ gwọọ kemịkalụ obere okpomọkụ.

Ọ bụrụ na mmepụta na-aga n'ihu karịa 28 Celsius C ma ọ bụ na-eji ahịrị ihicha ọkụ, dobe mmeghachi omume okpomọkụ dị elu na-achịkwa.

Ọ bụrụ na otu nọmba viscosity ahụ pụtara na ngwaahịa abụọ a, echela na ha na-agbanwe agbanwe.

Tulee usoro resin-hardener zuru oke, oge ọrụ bara uru, omume ọgwụgwọ, ntupu mmiri, okpomoku slab, ọsọ ahịrị, na nsonaazụ njikwa n'ezie.

Ma ọ bụrụ na nkume ahụ adịchaghị emebi emebi, gbawara nke ukwuu, ma ọ bụ na-ahazi ya, were nkwado ntupu dị ka usoro nkwado zuru oke-ọ bụghị naanị ịzụrụ nrapado.

Ajụjụ ndị a na-ajụkarị gbasara Epoxy Nkwado Nkume

1. Kedu epoxy kacha mma maka nkwado ntupu nkume?

Epoxy kacha mma dabere na okpomoku ogbako, ọnọdụ okwute, ụdị ntupu, ọsọ mmepụta na ihe achọrọ ọgwụgwọ. Ụlọ ọrụ na-emepụta oyi nwere ike ịchọ usoro ọgwụgwọ okpomọkụ dị ala, ebe ebe ọmụmụ ihe na-ekpo ọkụ n'oge okpomọkụ ma ọ bụ ahịrị ihicha chọrọ ịchịkwa mmeghachi omume okpomọkụ dị elu. Ntupu ntupu dị mma, mgbakwunye nkume a pụrụ ịdabere na ya, na oge ọrụ zuru oke dị mkpa karịa ịhọrọ site na viscosity naanị.

2. Enwere ike iji otu ntupu nkwado epoxy n'oge okpomọkụ na oyi?

Mgbe ụfọdụ, mana e kwesịghị iche ya. Nnukwu mgbanwe okpomọkụ nke oge na-emetụta ma viscosity epoxy yana ọsọ ọsọ. Ụlọ ọrụ na-arụ ọrụ gburugburu 10 Celsius C n'oge oyi na karịa 28 Celsius n'oge okpomọkụ nwere ike irite uru site na usoro ọgwụgwọ dị iche iche e mere maka oke okpomọkụ ndị ahụ.

3. Gịnị mere epoxy ntupu na-akwado ji nwayọọ nwayọọ na-agwọ ọrịa n'oge oyi?

Okpomọkụ dị ala na-abawanye viscosity epoxy anaghị agwọta ma na-ebelata mmeghachi omume resin-hardener. Ọ bụrụ na emebereghị usoro a maka ọnọdụ oyi, mmiri ntupu na mmepe ike nwere ike ịdị ngwa ngwa maka mmepụta nkịtị.

4. Gịnị mere epoxy jel ngwa ngwa n'oge okpomọkụ ntupu nkwado?

Okpomọkụ dị elu na-eme ngwa ngwa ọgwụgwọ epoxy. Nnukwu batches agwakọta nwekwara ike idowe okpomoku exothermic, na-eme mmeghachi omume ngwa ngwa n'ime akpa agwakọta. Jiri kemistri dabara adaba, jikwaa nha batch, wee nyochaa resin na okpomoku slab kama ịgbanwe oke ngwakọta akọwapụtara.

5. Kedu ka ụlọ ọrụ okwute ga-esi nwalee epoxy nkwado ntupu tupu ịtụ ọtụtụ?

Jiri okwute mmepụta na ntupu n'ezie, nwalee n'okpuru ọnọdụ okpomọkụ oge, dekọọ oriri resin na oge ọrụ bara uru, lelee eriri mmiri zuru oke, kwe ka ọgwụgwọ akọwapụtara, wee jikwaa slab ahụ site na usoro mmepụta nkịtị. Tulee ọtụtụ slabs tupu ịnakwere nnukwu ọkọnọ.

Otu esi edobe Nkume Mesh na-akwado kwụsie ike n'oge ọkọchị na oyi

Nkwado ntupu a pụrụ ịdabere na ya dabere na ndakọrịta resin eruba yana gwọọ kemịkalụ na gburugburu ebe nrụpụta n'ezie. Ọnọdụ oyi na-abawanye viscosity na ngwa ngwa mmeghachi omume, ebe okpomọkụ okpomọkụ na-eme ka mmalite nke mbụ ma na-ebelata windo ọrụ. Usoro ziri ezi kwesịrị ịsacha ntupu ahụ nke ọma, jikọta ya na elu nkume dị ọcha, ma mepụta ike njikwa a na-ahụ anya na-enweghị ịmanye ndị na-arụ ọrụ iji kwụọ ụgwọ okpomọkụ site na ijikọta ọnụ ma ọ bụ kpo oku a na-achịkwaghị achịkwa.

Họrọ hardening gburugburu ezigbo ụlọ ọrụ okpomọkụ

Ọ bụrụ na mmepụta oyi na-erute 10 Celsius C, jiri kemistri emebere iji gwọọ nke ọma na obere okpomọkụ. Ọ bụrụ na mmepụta oge okpomọkụ gafere 28 Celsius ma ọ bụ na-eji ahịrị ikpo ọkụ na-ekpo ọkụ, jiri usoro okpomọkụ dị elu nke na-echekwa oge ọrụ zuru oke maka nsị ntupu zuru oke.

Dakọtara usoro ahụ na ọnọdụ mmepụta

Ụlọ ọrụ oyi oyi:
nye ụzọ ọgwụgwọ kemịkalụ dị ala ma chọpụta na mmiri dị na nkume oyi.

Mmepụta oge okpomọkụ:
chebe windo na-arụ ọrụ bara uru ma zere nnukwu batches exothermic.

Mmepụta ahịrị ịkpọ nkụ:
jiri usoro emebere maka ọgwụgwọ a na-achịkwa n'okpuru okpomọkụ dị elu.

Nkwado ntupu aka:
jide n'aka na ndị na-arụ ọrụ nwere oge oghere zuru oke iji mebie slab ahụ zuru oke.

Nkume na-emebi emebi ma ọ bụ osisi:
nyochaa njupụta ntupu, usoro epoxy, ntụpọ nkume, na njikwa ihe achọrọ ọnụ.

Ekpela ikpe nkwado site na ọdịdị akpọnwụrụ

N'elu nke na-eche na ọ kpọrọ nkụ adịghị njikere ozugbo maka ibuli, ịtụgharị, ihicha ma ọ bụ ibuga. Kọwaa usoro njikwa ihe achọrọ wee kwado ya na slabs n'ezie. Oge ọgwụgwọ ziri ezi bụ oge dị mkpa iji ruo usoro mmepụta nchekwa na-esote - ọ bụghị naanị mgbe elu ahụ kwụsịrị inwe mmetụta.

What should buyers compare between suppliers?

Tulee oke okpomọkụ, viscosity agwakọtara, oge ọrụ, omume ọgwụgwọ, nha ogbe akwadoro, wet ntupu, nrapanye okwute, profaịlụ isi, ndakọrịta ihicha-ahịrị, oriri resin, na nkwụsi ike nke ogbe. Wee nwalee sistemụ ndị edepụtara aha site na iji okwute, ntupu, ndị na-arụ ọrụ na ọnọdụ mmepụta oge.

Practical Recommendation

Ọ bụrụ na ọgwụgwọ oyi na-adị ngwa ngwa, gbanwee gaa na kemistri na-ekpo ọkụ karịa itinyekwu ike. Ọ bụrụ na gels resin n'oge okpomọkụ tupu ekpochapụ slab ahụ zuru oke, jiri usoro okpomọkụ dị elu nke nwere mmeghachi omume na-achịkwa kama ibelata ike ike. Ọ bụrụ na ntupu na-akpụ akpụ, lelee nkwadebe elu, wepụta mmiri, wee gwọọ tupu ịta ụta fiberglass ahụ. Ma ọ bụrụ na slab na-esighi ike ka na-agbaji mgbe nkwado, nyochaa nhazi nkwado zuru oke kama iche na epoxy naanị ga-edozi nsogbu ahụ.

Achọrọ Epoxy nkwado ntupu maka ezigbo okpomọkụ nrụpụta gị?

Ụdị okwute, ntupu fiberglass, okpomọkụ ụlọ akwụkwọ, okpomoku slab, ọsọ ahịrị, usoro ọgwụgwọ na nhazi oge niile na-emetụta arụmọrụ nkwado ntupu. Nyochaa usoro zuru oke n'okpuru ezigbo oyi na ọnọdụ okpomọkụ tupu ịkwado mmepụta nnukwu.


Nyochaa Veropoxy Mesh Backing Epoxy Systems

Ntụaka

  1. A. A. Pazeto, P.M. Amaral, J.R. Pinheiro na A. B. Paraguassú.
    Mmetụta nke Glass Fiber-Reinforcement na Mechanical Properties of Coarse grained Building Stone.
    Center for Mineral Technology na Mahadum Lisbon.
    Ihe owuwu na ihe owuwu ụlọ, Vol. 155, 2017, p. 79–87 .
  2. A. A. Pazeto, P.M. Amaral na R. L. Arcanjo.
    Arụmọrụ Analysis nke Conventional Nkwado Ụzọ maka "Exotic" Nkume Ụlọ Dị ka Nka na-adị ugbu a chọrọ.
    Center for Mineral Technology na IDMEC, Mahadum Lisbon.
    International Journal of Rock Mechanics and Mining Sciences, Vol. 135, 2020, edemede 104507.
  3. WEST SYSTEM Technical Staff.
    Na-etinye fiberglass Cloth na teepu.
    Gougeon Brothers, Inc.
    WEST SYSTEM Epoxy Technical Resources.
  4. WEST SYSTEM Technical Staff.
    Ihe ndabere nke Epoxy Chemistry: Ịghọta oge ọgwụgwọ na okpomọkụ.
    Gougeon Brothers, Inc.
    WEST SYSTEM Epoxy Technical Resources.
  5. WEST SYSTEM Technical Staff.
    Akwụkwọ ntuziaka onye ọrụ sistemụ WEST & Ntuziaka ngwaahịa.
    Gougeon Brothers, Inc.
    WEST SYSTEM Technical Publications.
  6. ASTM International Committee C18 na Dimension Stone.
    ASTM C880/C880M-25 - Usoro nnwale ọkọlọtọ maka ike mgbanwe nke nkume akụkụ.
    ASTM International.
    Akwụkwọ kwa afọ nke ụkpụrụ ASTM, Vol. 04.07.
  7. ASTM International Committee C18 na Dimension Stone.
    ASTM C99/C99M - Usoro nnwale ọkọlọtọ maka Modulus nke mgbawa nke nkume akụkụ.
    ASTM International.
    Akwụkwọ kwa afọ nke ụkpụrụ ASTM, Vol. 04.07.
  8. Charles Selwitz.
    Epoxy Resins na Nchekwa Nkume.
    Getty Conservation Institute.
    Nnyocha na usoro nchekwa, Getty Publications, 1992.