Soo koobid degdeg ah:
Viscosity resin Epoxy wuxuu go'aamiyaa sida fudud ee xabagta uu ugu qulqulo dusha dhagaxa, u galo dildilaaca yar yar, qoynta mesh xoojinta, buuxisa daldaloolada, ama ku harta cilado ballaaran. Viscosity hoose guud ahaan waxa ay wanaajisaa dhexgalka, laakiin CPS ugu hooseysa si toos ah uma aha doorashada ugu fiican. Soo-saareyaasha dhagxaantu waa inay doortaan viscosity epoxy si waafaqsan nooca dhagaxa, cabbirka dildilaaca, habka codsiga, heerkulka aqoon-is-weydaarsiga, wakhtiga shaqada, hab-dhaqanka daaweynta, iyo waxqabadka dhammaystirka ee loo baahan yahay halkii ay is barbar dhigi lahaayeen qiyamka CPS oo keliya.
Viscosity dhawaaqa sida line yar on xaashida xogta farsamada epoxy, laakiin warshad dhagax ah waxay go'aansan kartaa in resin gaadho gunta hoose ee dildilaaca yar ama si fudud u fadhiisan dusha. Waxay saamayn kartaa isticmaalka resin-ka, qoynta mesh, hawada sii daynta, heerka sareynta, qoto-dheeraanta dhexgalka, muuqaalka dhalaalaysa, xawaaraha habka, iyo ugu dambaynta joogteynta saqafyada la dhammeeyey.
Tani waxay si gaar ah muhiim u noqonaysaa marka la farsameeyo granite madow oo cufan, granite khafiif ah, marmar cad ama midab leh, dhejisyo jilicsan, walaxda mesh-taageertay, ama dhagax lagu daweeyo impregnation vacuum-caawiyay. Xabagta dareemaysa “dhuuban” ee hal aqoon iswaydaarsi waxa laga yaabaa in uu u dhaqmo si aad uga duwan mid kale sababtoo ah heerkulka deegaanka, heerkulka dhagaxa, xiirid, kimistari hardener-hardener, iyo daawaynta horumarka dhamaantood waxay isbedelaan habdhaqanka socodka.
Taasi waa sababta iibsadayaasha xirfadleyda ah aysan weydiin kaliya, "Waa maxay viscosity?" Su'aasha ugu fiicani waa: "Waa maxay viscosity ee epoxy-kani ku leeyahay xaalado tijaabo ah oo qeexan, iyo miyuu rheology ku habboon yahay dhagaxayga, cilladda, heerkulka, iyo habka wax soo saarka?" Veropoxy hadda dhagax epoxy kala duwan Tani waxay si cad u muujineysaa: Nidaamyo badan ayaa ku dhex fadhiisan kara noocyo isku mid ah oo viscosity ah iyadoo loo qaabeynayo codsiyo kala duwan.

Waa maxay macnaha Epoxy Resin Viscosity ee ka shaqaynta dhagaxa?
Viscosity wuxuu qeexayaa caabbinta dareeraha ee socodka. Maqaarka hoose ee viscosity ayaa si fudud u qulqulaya, halka maaddada viscosity-ga sare ay ka hortagto dhaqdhaqaaqa oo u egtahay in ay ku sii jirto meesha la dhigo.
Marka la eego qeexida resin epoxy, viscosity waxaa caadi ahaan lagu soo warramey centipoise, oo u qoran cP. Qaar ka mid ah xaashiyaha farsamada-dhagaxa-warshada ganacsiga ayaa sidoo kale cutubka u qoraa sida "CPS." Eray bixinta SI, 1 cP waxa ay tiro ahaan la mid tahay 1 mPa·s.
Si kastaba ha ahaatee, mashiinka dhagxaanta, si kastaba ha ahaatee, viscosity ma aha oo kaliya lambar shaybaar. Waxay si toos ah u saamaysaa sida resinka isku qasan uu u dhaqmo marka uu la kulmo daldaloolada, dildilaaca xididada, calaamadaha wax lagu arko, mesh fiberglass, sagxadaha aan sinnayn, cidhifyada toosan, ama godadka waaweyn.
Viscosity hoose wuxuu door bidaa dhaqdhaqaaqa iyo dhexgalka
Marka viscosity la yareeyo, resin guud ahaan si fudud ugu dhaqaaqi karaa meel bannaan oo ganaax ah. Tani waxay faa'iido leedahay marka ujeedadu tahay impregnation gudaha halkii si fudud loo dabooli lahaa dusha sare.
Tusaalaha wanaagsani waa granite madow oo cufan oo ay ku jiraan fissures-yar oo ay adagtahay in lagu gaadho xabag qaro weyn. Veropoxy's Aragtida aadka u hooseeya ee galitaanka qoto dheer ee Granite Black waxay si gaar ah u taagan tahay dhexgalka daldaloolo iyo dildilaacyo ka hor inta aan la nadiifin. Xogta badeecadeeda la daabacay waxay nidaamka gelisaa heer aad u hooseeya oo viscosity ah oo loogu talagalay in lagu hagaajiyo dhexgalka gudaha.
Jirka sare wuxuu jecel yahay joogitaanka awoodda iyo buuxinta farqiga
Socodka had iyo jeer maaha hadafka. Haddii ciladu ballaaran tahay, codsigu waa mid toosan, ama resinku waa inuu ku sii jiraa tollayn halkii uu ku lumin lahaa daloollada ku hareeraysan, qaab-dhismeedka sare ee thixotropic ayaa laga yaabaa inay ku habboon tahay.
Tani waa sababta isticmaalka resinka wax gelinta sidii uu yahay mastic buuxinaya farqiga u abuuri kara natiijooyin niyad jab leh. Xabagta ayaa laga yaabaa inay si aad ah ugu daadato dhagaxa, ka baxdo aagga dayactirka, ama waxay ku dhaafi kartaa wax aan ku filnayn oogada agteeda.
Taa beddelkeeda, adigoo isticmaalaya koolada buuxinta faraqa culus ee timaha timaha ayaa laga yaabaa inay abuurto dhibaatada ka soo horjeeda: waxay isku xirtaa albaabka dillaaca iyada oo aan la gaarin qoto dheerkeeda gudaha.
Waa maxay sababta CPS kaligeed aysan ku filneyn
Mid ka mid ah khaladaadka wax iibsiga ee ugu caansan waa isbarbardhigga laba badeecadood oo epoxy ah oo keliya iyadoo la raacayo qiyamka CPS ee la daabacay.
Isbarbardhiggaas wuxuu noqon karaa mid marin habaabin ah haddii aan labada lambar lagu cabbirin xaalado isbarbardhigga ah.
Heerkulka cabbiraadda arrimaha
Viscosity Epoxy waa heerkul xasaasi ah. Resin qabow wuxuu noqdaa mid dhumuc weyn oo adag in la bamgareeyo, la qaso, la faafiyo, oo qoyano substrate-ka. Xabagta diirran ayaa guud ahaan si fudud u socota.
Tani aad ayey muhiim ugu tahay warshadaha dhagxaanta ee caalamiga ah. Resin-ka loo isticmaalo aqoon-is-weydaarsiga xilliga qaboobaha ee 10°C wuxuu u dhaqmi karaa si ka duwan isla badeecada lagu maamulo aagga wax-soosaarka 30°C.
Heerkulka sidoo kale wuxuu abuuraa saameyn labaad: halka kulaylku guud ahaan hoos u dhigo viscosity, heerkulka sare wuxuu soo dedejin karaa falcelinta epoxy waxayna soo gaabin kartaa wakhtiga shaqada ee la isticmaali karo. Ficil ahaan, warshadu si fudud uma kululayn karto resinka si ay u hesho socodka wanaagsan. Socodka, nolosha dheriga, xawaaraha daaweynta, iyo laxanka wax soo saarka waa in la isku dheellitiro.
Viscosity-ka isku-dhafan ayaa ka faa'iido badan marka loo eego xuubka-kaliya resin-ga
Qaybaha A waxa laga yaabaa inay lahaadaan hal muuqasho iyo qayb B mid kale. Marka resinka iyo qallafsanaanta la isku daro, nidaamka isku dhafan wuxuu u dhaqmi karaa si ka duwan mar kale.
Go'aannada wax-soo-saarka dhabta ah, weydii haddii viscosity-ka la daabacay uu tixraacayo:
- qaybta resin kaliya;
- qayb adag oo kaliya;
- A + B oo si buuxda isku dhafan;
- isku dhafka isla markiiba ka dib marka la isku daro; ama
- isku darka ka dib markii muddo cayiman falcelinta.
Habaynta dhagaxa, hab-dhaqanka nidaamka isku-dhafan ayaa inta badan khuseeya sababta oo ah taasi waa waxa dhabta ah ee gasha dildilaaca, qooya mesh-ka, ama ku faafo saabka.
Heerka jeexjeexa iyo habka tijaabada waa arrin
Xayawaanka dareeraha ah oo badan ayaa lagu qiimeeyaa viscometers wareeg ah. Walxaha aan Newtonian ahayn, viscosity-ka muuqdaa wuu isbeddeli karaa iyadoo ku xidhan xawaaraha dunta ama xaaladaha dhogorta. Tani waa sababta qeexitaanka xirfadlaha ay tahay inuu si fiican u sheego habka cabbirka iyo xaaladaha tijaabada halkii uu soo bandhigi lahaa lambar qaawan.
TS ISO 2555 waxay qeexaysaa cabbirka-muuqaalka-muuqaalka ee resins-ka dareeraha iyadoo la adeegsanayo viscometer wareeg ah, halka ASTM D2196 ay wax ka qabato viscosity muuqda iyo dabeecadda rheological ee agabyada aan Newtonian ahayn ee lagu cabiray xaaladaha wareeg ee la qeexay.
Sharciga wax iibsiga ee dhabta ah: haddii alaab-qeybiyaha A uu yiraahdo "400 cP" iyo alaab-qeybiyaha B uu yiraahdo "550 cP," isla markiiba ha u qaadan in alaab-qeybiyaha A uu si fiican u soo galayo. Marka hore is barbar dhig heerkulka tijaabada, qalabka ama habka, xaaladaha spindle/xawaaraha, xaalada isku darka A/B, iyo habaynta arjiga gaarka ah.
Sida Viscosity-ku u saameeyaa Waxqabadka Dhagxaanta
Gelitaanka dildilaaca-yar-yar
Dildilaaca timaha iyo jeexjeexyada gudaha ayaa ka mid ah kiisaska ugu cadcad halkaas oo resin-mug yar uu faa'iido u leeyahay. Granite cufan ayaa laga yaabaa inay ku jiraan dildilaacyo la arki karo marka la eego kormeerka laakiin aad u cidhiidhi ah. Resinku waa inuu qoyo furitaanka oo uu sii wadaa inuu dhex maro dariiqyada xididdada ka hor inta uusan jeexjeexin aad u fogaan.
Sababtan awgeed, Veropoxy's Black Granite Solution kala duwan waxaa ka mid ah dhowr nidaam oo qoto-dheer iyo nidaam epoxy-qulqulaya oo loogu talagalay daaweynta micro-crack iyo xoojinta.
Haddii dhexgalka aan ku filnayn, dayactirku wuxuu u ekaan karaa mid la aqbali karo isla markaaba daaha ka dib halka cilladaha gudaha aan la daweyn. Dhibaatooyinku waxay soo bixi karaan hadhow inta lagu jiro hagaajinta, suufka, jarista, gaadiidka, ama rakibaadda.

Qooynta daloolada iyo meelaha dhagaxa ah
Qoynta wanaagsani waxay caawisaa in resin la taabto dusha sare ee dildilaaca iyo daloolada halkii ay ka ahaan lahayd dhibco go'doonsan. Viscosity hoose guud ahaan waxay taageertaa fidinta sahlan, laakiin kiimiko iyo xaalada dusha sare ayaa iyana muhiim ah.
Boodhka, qoyaanka, saliidda, hadhaaga dhalaalaysa, ama heerkulka dhagaxa ee xad-dhaafka ah ayaa carqaladayn kara qoynta xitaa marka mawgu u muuqdo mid habboon. Sidaa darteed, tirada CPS hoose ma magdhabi karto diyaarinta dusha sare ee liidata.
Siideynta hawada iyo habdhaqanka xumbo
Nidaam aad u qaro weyn ayaa ka dhigi kara hawo ku xanniban mid adag si looga baxsado, gaar ahaan xilliga uurka ama qoynta mesh. Maqaarka hoose ee viscosity wuxuu wanaajin karaa dhaqdhaqaaqa agagaarka fiilooyinka iyo daloolada, laakiin isku darka gardarrada ayaa wali soo kordhin kara hawada.
Warshadaha isticmaalaya farsamaynta faakuumku caawiyay waa inay fiiro gaar ah siiyaan dheelitiran. Veropoxy's Xalalka faleebada Vacuum waxay ku salaysan yihiin kor u qaadida dhaqdhaqaaqa resin galay daloolo-yar-yar iyo cilladaha gudaha ee hoos yimaada xaaladaha faakuum-kaalmay.
Isticmaalka xabagta
Xabagta dareere badan ayaa si qoto dheer u geli karta, taas oo inta badan la jecel yahay. Laakiin taasi waxay sidoo kale kordhin kartaa isticmaalka dhagaxa aadka u daloola haddii aan la xakameynin tirada codsiga.
Tani waxay si gaar ah u khusaysaa travertine, marmar dalool, dhagxaan cimilo leh, iyo saqafyo ka kooban meelo bannaan oo isku xidhan. Hawl-wadeenku waxa laga yaabaa inuu sii wado ku shubista resinka sababtoo ah dusha ayaa u muuqda mid engegan halka tiro aad u badan ay mar hore ka haajirtay dusha sare.
Isticmaalka sarreeya si toos ah uma luminayo haddii ujeedadu tahay xoojinta qoto dheer. Arrintu waa haddii resinka dheeriga ahi uu abuuro isku xidhid gudaha ah oo faa'iido leh ama si fudud u baaba'o meel bannaan oo ay ku kordhiso qiimo yar.
Diyaarinta simida dusha sare iyo turxaan bixinta
Dayactirka dildilaaca ka dib, xariijimo badan oo dhagax ah ayaa u dhaqaaqa shiidi ama turxaan bixin. Viscosity Resin wuxuu saameeyaa haddii cilladuhu ay si buuxda u buuxsameen daawaynta ka dib iyo haddii dusha laga baaraandegi karo iyada oo aan la soo bandhigin godad ama khadadka dayactirka.
Resin galinta oo si qurux badan ugu qulqula dhagaxa ayaa laga yaabaa inuu weli u baahdo daawayn labaad marka dusha sare u baahan yahay jidh ama simi. Tani waa mid ka mid ah sababaha qaar ka mid ah hababka farsamaynta xirfadleyda ay u kala soocaan impregnation qoto dheer buuxinta ama dhamaystirka dusha sare.
Waa maxay Range CPS ee ay tahay inaad u doorato Dhagax?
Ma jiro xeer caalami ah oo sheegaya in hal kala duwan oo CPS ah oo go'an ay sax u tahay marble kasta, granite, mesh support, ama habka faakuumka. Erayada kala soocida sida "muwajis hoose", "mugsoon hoose" iyo "qulqul sare" waxay ku xiran yihiin habaynta, alaab-qeybiyaha, xaaladaha tijaabada, iyo codsiga loogu talagalay.
Weli, badeecadaha Veropoxy ee hadda jira waxay bixiyaan tusaalooyin waxtar leh oo adduunka dhabta ah oo ku saabsan sida nidaamyada viscosity-ka hooseeya loogu dabaqo wax soo saarka dhagaxa xirfadleyda ah.
| Baahida Habaynta Dhagaxa | Jihada Viscosity | Waxa Iibsaduhu isku dayayo inuu gaadho | Tusaalaha Codsiga Veropoxy |
|---|---|---|---|
| Granite madow cufan oo leh fissures-yar | viscosity aad u hooseeya | Gelid qoto dheer oo gudaha ah ka hor inta aan la nadiifin | CP83-60 / B25Q-KG nidaamka qoto-dheer |
| Dayactirka dildilaaca granite fudud iyo kor u qaadida midabka | Viscosity hoose, socodka la xakameeyey | Gaadhi cilladaha wanaagsan iyadoo la ilaalinayo daboolida dusha sare | 4099-BBS / D30M-BS |
| Dayactirka marmar diiran-cimilada | Mawjad hoose oo la xakameeyey | Qoynta wanaagsan, hagaajinta dildilaaca, hagaajinta iyo midabka | 5099 / B25Q-KG |
| Taageerada mesh dhagaxa | Mawduuc hoose oo la xakameeyey | Mesh xoojinta qoyan iyada oo aan lahayn qulqulo xad dhaaf ah | 4090 mesh-taageer hababka |
| Vacuum impregnation | Viscosity hoose oo leh waqti shaqo oo ku filan | Ku dhaq resin dhex daloolada iyo dildilaaca yar yar ka hor dhalmada | Xalalka faleebada Vacuum |
| Nusqaamaha ballaaran ama buuxinta tollaynta | Jirka sare ama dhaqanka thixotropic | Ku hay resin gudaha aagga dayactirka halkii aad ka ahaan lahayd dheecaan xad-dhaaf ah | Isticmaal nidaamka buuxinta gaarka ah ee arjiga halkii aad dooran lahayd oo kaliya CPS |
Tusaale ahaan, Veropoxy waxay daabacdaa qiyaastii 400-600 cP oo loogu talagalay alaabooyin badan oo dhagax ah oo ay ku jiraan Kobcinta Midabka Epoxy ee Granite Iftiin ah iyo cimilada diiran Dayactirka Marble & Nidaamka Kobcinta Midabka. Dhanka kale, alaabteeda madow-granite-ka qoto-dheer ee qoto-dheer ayaa loo dhigayaa xitaa hoos u dhaca cilladaha gudaha ee wanaagsan.
Qaadashada muhiimka ah maaha in "400-600 cP uu yahay dhuxul dhagax oo sax ah." Waa in kala duwanaanta viscosity tirooyinka la mid ah ay u adeegi karaan hawlo kala duwan sababtoo ah xawaaraha daaweynta, xasilloonida heerkulka, isdhexgalka dusha sare, kimistariga adag, caabbinta jaalaha ah, iyo habka codsigu way kala duwan yihiin.
Sida loo doorto Viscosity by Nooca Dhagaxa
Granite madow cufan
Granite madow cufan ayaa inta badan ka faa'iideysta habka dhexgalka sare marka dildilaaca yar yar ama jeexjeexyada gudaha ay yihiin cilladda ugu weyn. Dhagaxa laftiisa waxaa laga yaabaa in uu hooseeyo guud ahaan porosity, laakiin dildilaaca qaab dhismeedka wanaagsan ayaa wali u baahan kara xoojin.
Haddii resinku uu aad u vis-beelo, waxa laga yaabaa inuu ku sii jiro meel u dhow albaabka dildilaaca. Haddii ay aad u dareere tahay iyada oo aan la xakameynin ku filan, si kastaba ha ahaatee, si xad dhaaf ah ayey u haajiraan oo waxay kordhin kartaa isticmaalka.
Haddii habkaagu uu ku lug leeyahay ilka-daadin ka hor, kala hormari dhexgalka qoto dheer, waqti shaqo oo ku filan, isku xirnaanta gudaha ee xooggan, iyo natiijooyinka muuqaal deggan ka dib dhalaalidda.
granite khafiif ah
Granite-midab khafiif ah waxay abuurtaa caqabad dheeraad ah: tayada dayactirku waa inay noqotaa qaab dhismeed iyada oo aan la abuurin mugdi muuqda, midabayn, ama isbarbardhig muuqaal ah.
Viscosity waa in si wada jir ah loo qiimeeyaa hufnaan, dhaqanka kobcinta midabka, caabbinta jaalaha ah, iyo muuqaalka ugu dambeeya ee dhalaalaya.
The Nidaamka granite iftiinka Veropoxy wuxuu isku daraa 400-600 cP oo la daabacay oo leh midab-kor u qaadis iyo hawlaha dhexgalka, taasoo tusinaysa sababta viscosity-ku aanu waligii uga go'in waxqabadka indhaha.
marmar cad iyo midab leh
Marble si aad ah ayey ugu kala duwanaan kartaa xagga porosity, qaab-dhismeedka micro-crack, ka kooban macdanta, daahfurnaanta, iyo dareenka midabka. Xabagta si wax ku ool ah u soo gasha waxay sidoo kale bedeli kartaa muuqaalka muuqaalka marmarka iftiinka haddii kiimiko iyo sifooyinka indhaha aysan ku habboonayn.
Marble cad iyo midab leh, qiimee viscosity-ga oo ay la socdaan dabeecad aan wasakhayn, caabbinta jaalaha ah, khatarta calaamadda biyaha, heerkulka shaqada, iyo nadiifinta.
Veropoxy waa ka sii ballaaran Epoxy ee Marble Qaybta codsigu waxay bixisaa macnaha marble xoojinta iyo hagaajinta, halka alaabta kulaylka leh ee gaarka ah ay wax ka qabtaan xaaladaha habaynta ee aad u qeexan.
Travertine iyo dhagxaan aad u daloolsan
Travertine wuxuu u dhaqmaa si ka duwan sababtoo ah daloolada furan iyo godadka waxay nuugi karaan xaddi badan oo ah resin-mug yar. Qulqulka qoto dheer ayaa laga yaabaa inuu u baahan yahay xasilinta, laakiin istaraatijiyad galinta saafiga ah had iyo jeer kuma habboona marka godadka waaweyni ay tahay in la buuxiyo si fiican.
Xaaladdaas, processor-ku waxa uu u baahan karaa hab habaysan: dhexgalka ama xidhitaanka marka hore, oo ay ku xigto walxo buuxinaya jirka sare.
Veropoxy's Epoxy ee Travertine qaybta waxay ka hadlaysaa doorka epoxy ee daaweynta daloolka, dayactirka dillaaca, iyo ilaalinta dhagxaanta.
Sida Heerkulka u Bedesho Go'aanka Viscosity
Heerkulka waa mid ka mid ah doorsoomayaasha aadka loo dhayalsado ee iibsiga epoxy.
Xabagta qabow waxay noqotaa mid aad u muuqata. Waxay qaadataa waqti dheer in la qulqulo, waxaa laga yaabaa inay adagtahay in si sax ah loo bixiyo, waxaa laga yaabaa in xoojinta qoyan si tartiib tartiib ah, oo si fudud u dabin kara hawada inta lagu jiro habaynta.
Xabagta diirimaadku guud ahaan si degdeg ah ayay u socotaa, laakiin fal-celinta kiimikaad ee u dhexeeya resin iyo hardeer sidoo kale way kordhisaa marka heerkulku kordho. Sidaa darteed warshadu waxay u baahan tahay socodka iyo habdhaqanka daaweynta labadaba si ay u ahaato mid la jaanqaadi karta wakhtiga wareeggeeda.
Tani waa sababta laba badeecooyin leh oo isku mid ah viscosity magacu waxay u qaban karaan si kala duwan jiilaalka iyo xagaaga.
Kala duwanaanshaha mesh-taageerada Veropoxy waa tusaale faa'iido leh. Waa Heerkulka Sare ee ur aan ur lahayn ee Taageerida Mesh Dhagaxa waxay daabacdaa 400-600 cP viscosity kala duwan waxaana loo qaabeeyey wax soo saarka heerkul sare. Nidaamka taageerka mesh-heerkulka hooseeya ee shirkadu sidoo kale waxay isticmaashaa kala duwanaansho yar-yar oo la kontoroolo laakiin waxaa loo qaabeeyey xaaladaha habaynta qabow.
Casharka iibsadaha waa mid fudud: viscosity iyo chemistry-ga waa in si wadajir ah loo doortaa.
Haddii warshaddaadu ku shaqayso meel u dhow 10°C jiilaalka, ha u qaadan in epoxy-ga si fiican u shaqaynaya 25°C ay u dhaqmi doonto si isku mid ah.
Haddii aqoon-is-weydaarsigaagu si joogto ah uga sarreeyo 30°C, ha xallin dhibaatooyinka socodka si fudud adiga oo dooranaya xabagta ugu khafiifsan. Nolosha dheriga iyo daawaynta degdega ah waxay noqon kartaa khataraha ugu waaweyn.
Viscosity Low vs Epoxy Dheecaan Sare ee Dhagaxa
| Qodobka Go'aanka | Hoos-u-muuqaalka Epoxy | Aragga sare-sare/Xaq-dheer ee Jirka |
|---|---|---|
| Dhexdhexaadinta yar-yar | Caadi ahaan ka fiican | Waxaa laga yaabaa inay ku harto meel u dhow oogada |
| Vacuum impregnation | Guud ahaan la door biday | Waxa laga yaabaa inay xaddiddo socodka |
| Mesh qoynta | Waxay hagaajin kartaa impregnation fiber | Waxaa laga yaabaa inay adagtahay in si isku mid ah loo faafiyo |
| Buuxinta farqiga ballaaran | Meel aad u fog buu daadin karaa | Caadi ahaan way fiicantahay inaad ku sii jirto farqiga |
| Dayactir toosan | Halis sare oo sag/dhal ah | Caadi ahaan way fududahay in la xakameeyo |
| Isticmaalka dhagxaanta daloola | Si qoto dheer ayuu u geli karaa oo kordhin karaa isticmaalka | Socdaal qoto dheer oo yar |
| Siideynta hawada | Guud ahaan way fududahay marka si habboon loo qaso | Hawada way adkaan kartaa in la sii daayo |
Labada dhinac midna si caalami ah uma roona. Viscosity saxda ah waa kan abuura astaanta socodka loo baahan yahay inta lagu jiro daaqada shaqada ee la heli karo.
Sida Loo waafajiyo Viscosity Epoxy iyo Baahiyaha Habaynta Dhagaxa ee Kala Duwan
| Haddii Xaaladaada Wax soo saarku tahay… | Dooro ama Hubi… | Waa maxay sababta |
|---|---|---|
| Granite cufan oo leh dildilaacyo yaryar oo timo ah | Nidaamka galitaanka qoto-dheer ee hoose | Resin waa inuu galaa jeexjeexyada gudaha ka hor inta aan la daweyn |
| Dul weyn oo dusha sare ah ama tol furan | Jirka sare ama nidaamka buuxinta farqiga | Xabagta dhuuban ee aadka u dhuuban ayaa laga yaabaa inay daadato |
| Faleebo faleebo | Mawduuc hoose iyo nolol dheri oo ku filan | Socodku waa inuu ku sii socdaa daloolada inta lagu jiro wareegga faleebada |
| Shabakadda muraayadda si buuxda looma qoysin | Hubi viscosity isku qasan, heerkulka, qadarka codsiga iyo habka fidinta | Qoynta liidata had iyo jeer ma aha dhibaato xoog resin |
| Epoxy waxay noqotaa mid adag in la faafiyo jiilaalka | Hubi heerkulka alaabta iyo qaabaynta qaboojinta | Heerkulka hoose wuxuu kordhiyaa viscosity |
| Epoxy si fiican ayey u socotaa laakiin si degdeg ah ayey u daaweysaa xagaaga | Hubi nidaamka qallafsanaanta iyo qaabaynta heer-kulka gaarka ah | Xaaladaha diiran waxay kordhin karaan socodka iyagoo gaabinaya wakhtiga shaqada |
| Resinku wuu dhex galaa laakiin dib u hagaajintu dib ayuu u noqdaa ka dib marka la nadiifiyo | Tixgeli gelida marxaladda leh iyo buuxinta dusha sare | Qulqulka qoto dheer oo keliya ayaa laga yaabaa inuusan bixinin dhismo ku filan oo dusha sare ah |
| Laba alaab-qeybiyeyaal ayaa soo xiganaya qiyamka CPS ee isku midka ah laakiin natiijooyinku way kala duwan yihiin | Is barbar dhig habka tijaabada, heerkulka, saamiga isku dhafka ah, astaanta daawaynta iyo substrate-ka | Adeegyada Badbaadinta Ilmuhu Keliya ma sifaynayso habaynta dhamaystiran |
Sida Loo Akhriyo Tilmaamaha Viscosity Epoxy Sida Iibiyaha Xirfadlayaasha ah
Kahor intaanad ansixin resin, codso in ka badan hal lambar.
1. Xaqiiji heerkulka tijaabada
Shaxda viscosity ee aan lahayn heerkulku waxa uu leeyahay qiime xadidan. Weydii in cabbirka laga qaaday 20°C, 23°C, 25°C, ama xaalad kale.
2. Xaqiiji in nambarku yahay resin-kaliya ama isku qasan A+B
Khadka wax soo saarka ayaa isticmaala nidaamka isku dhafan. Hubi in tilmaanta aad is barbardhigtay ay ka tarjumayso xaaladda ku habboon codsiga.
3. Xaqiiji habka cabbirka
Weydii in habka viscometer-ka wareeg ah la isticmaalay iyo in xaaladaha cirifka/xawaaraha la heli karo. Tani waxay si gaar ah muhiim u noqonaysaa marka la barbar dhigo alaabada alaab-qeybiyeyaal kala duwan.
4. Hubi saamiga isku darka
Beddelka saamiga resin-to-hardener si loo sameeyo epoxy "dhuuban" maaha wax soo saar gaaban oo la aqbali karo. Nidaamyada Epoxy waxaa loo qaabeeyey agagaarka stoichiometry cayiman iyo dheelitirnaanta qaabaynta. Saamiyada aan sax ahayn waxay keeni karaan daawo aan dhamaystirnayn, oog jilicsan, jajaban, ama sifooyin farsamo oo aan waafaqsanayn.
5. Hubi wakhtiga shaqada oo daawo profile
Epoxy dareere ah oo aad u sarreeya oo bilaaba gelling ka hor inta aanu gaadhin qoto dheer ee dildilaaca la doonayo maaha nidaam lays guulaysto.
Daawaynta qoto dheer, viscosity waa in uu ahaado mid faa'iido leh inta lagu jiro wakhtiga loo baahan yahay faafinta, dhex galka, farsamaynta faakuumka, ama soo saarista mesh.
6. Hubi dulqaadka viscosity ee u dhexeeya qaybaha
Warshadaha dhagaxa ah ee ku shaqeeya wax soo saar joogto ah waxay u baahan yihiin dib u soo celin. Haddii viscosity si weyn u kala duwan yahay Dufcaddii ilaa Dufcaddii, tirada codsiga, qoto dheer ee dhexgalka, farsamada hawlwadeenka, iyo xawaaraha line dhamaantood waxay u baahan karaan hagaajin.
Tani waa sababta qiimeynta alaab-qeybiyaha ay tahay inay ku jirto joogteynta dufcada, maaha kaliya natiijo wanaagsan oo ka timid hal muunad.
Sida loo tijaabiyo viscosity Epoxy ka hor inta aan la dalban
Nambarka shaybaadhka waa in had iyo jeer lagu xidhaa shaybaadhka dhabta ah.
Talaabada 1: Shardi alaabta
Keen xabagta, qallajiye, iyo shaybaar dhagax oo mataleya heerkul la kantaroolo oo la duubay. Tijaabinta hal alaab-qeybiye 15°C iyo mid kale oo ah 25°C ayaa ka dhigaysa isbarbardhigga mid aan la isku halayn karin.
Tallaabada 2: Isku qas si waafaqsan saamiga la cayimay
Isticmaal miisaan ama qiyaas sax ah. Ha beddelin saamiga si aad u hagaajiso socodka.
Tallaabada 3: Diiw habdhaqanka maaraynta bilowga ah
U fiirso shubista, isku darka, fidinta, qoynta, iyo sii deynta xumbo. Resinku waa inuu u dhaqmaa si joogto ah oo ku filan hawl-wadeenada ama qalabka tooska ah si loo xakameeyo.
Tallaabada 4: Ku dalbo dhagaxa wax soo saarka dhabta ah
Isticmaal granite matale ah, marmar, travertine, ama walxo dhoobo ah oo la xoojiyay halkii aad ka isticmaali lahayd guddi tijaabo ah oo guud.
Codsiyada dhexgalka, ka baar in resinku uu gaaro cilladda halkii aad si fudud u daboolin lahayd dusha sare.
Tallaabada 5: Diiwaangeli isticmaalka resinka
Cabbir inta shay ee loo baahan yahay salaxkiiba ama mitirkii laba jibbaaran ee xaaladaha la xakameeyey. Resin ka jaban oo isticmala walxo aad uga badan waxa laga yaabaa in aanu ka jabnayn wax soo saarka.
Tallaabada 6: U fiirso daaqada shaqada oo buuxda
Lasoco sida dhaqsaha leh u kororka viscosity ka dib marka la isku daro. Hawl-wadeenadu waxay u baahan yihiin inay ogaadaan marka qulqulka qulqulku bilaabo inuu dhaco iyo marka nidaamku noqdo mid aan ku habboonayn codsi dheeraad ah.
Talaabada 7: Daawo oo dhame suunka
Ha xukumin kaliya muuqaalka qoyan. Shiidi, dhalaal, gooy, ama gacanta ku dheji suufka sida habka wax soo saarka dhabta ah uu u baahan yahay.
Hubi:
- dildilaaca yar yar ee haray;
- godad;
- geesaha dayactirka muuqda;
- midabka beddelka;
- jaalaha;
- adhesion liidata;
- buuxinta nasashada;
- tackness dusha sare;
- jajab aan la filayn; iyo
- iswaafaqla'aanta dhalaalaysa.
Khaladaadka ugu badan ee Epoxy Viscosity ee Warshadaha Dhagaxa
Doorashada CPS ugu hooseysa sababtoo ah waxay u egtahay mid horumarsan
Hoose si toos ah uma roona. Xabagta dareeraha aadka u badan ayaa laga yaabaa inay si qoto dheer u dhex gasho laakiin waxay abuurtaa isticmaalka xad dhaafka ah, qulqulaya, ama dhismo aan ku filnayn oo dusha sare ah.
Isbarbardhigga tirooyinka lagu cabbiray heerkul kala duwan
Tani waxay ka dhigi kartaa mid ka mid ah resin-ku inuu si aad ah u khafiifsan yahay inkasta oo faraqa u badan yahay uu ka yimid xaaladaha tijaabada.
Dhagaxa laftiisa oo iska indha tiraya
Dilaaca granite madow ee cufan iyo dalool travertine ah oo furan ma aha dhib la mid ah dayactirka. Waa inaysan si toos ah u isticmaalin xabuub isku mid ah.
Isticmaalka hal epoxy xilli kasta
Heerkulka aqoon-is-weydaarsiga xilliyeedku wuxuu bedeli karaa socodka iyo xawaaraha labadaba. Warshado leh kala duwanaansho jiilaal/xagaaga oo xoogan waa in ay tijaabiyaan agabka xaaladaha heerkulka dhabta ah.
In la iska indhatiro nolosha dheriga
Socodka bilawga ah ee aadka u wanaagsan faa'iido ma laha haddii viscosity uu si dhakhso ah u kaco inta lagu jiro daaqada codsiga dhabta ah.
Isticmaalka xabagta galitaanka sida buuxinta faraqa caalamiga ah
Xabagta ayaa laga yaabaa inay ku baaba'do dhagaxa oo ka tago dusha oo buuxa.
Beddelida saamiga isku darka si loo hagaajiyo viscosity
Tani waa mid ka mid ah marinnada gaaban ee ugu khatarta badan. Socodka waa in lagu xakameeyaa qaabaynta saxda ah iyo shuruudaha habaynta, ma aha in si aan kala sooc lahayn loo beddelo saamiga A: B ee la cayimay.
Liiska hubinta iibsadaha Epoxy Stone
| Su'aasha la Weydiinayo Alaabta | Maxaa Sabab U Ah |
|---|---|
| Waa maxay viscosity isku qasan? | Tani waxay matalaysaa habdhaqanka codsiga dhabta ah ee ka fiican xogta resin-ka keliya. |
| Heerkulkee ayaa lagu qiyaasay viscosity? | Qulqulka Epoxy wuxuu si weyn isu beddelaa heerkulka. |
| Habka tijaabada viscosity-kee ayaa la isticmaalay? | Xaaladaha cabbirka kala duwan waxay soo saari karaan qiimeyaal muuqda oo kala duwan. |
| Waa maxay dhagaxa iyo habraaca loo sameeyay xabagta? | Habka gaarka ah ee codsiga ayaa ka muhiimsan bartilmaameedka CPS ee guud. |
| Waa maxay saamiga resin-to-hardener? | Loo baahan yahay daawaynta soo noqnoqda iyo waxqabadka. |
| Waa maxay nolosha dheriga ama daaqada shaqada? | Wuxuu go'aamiyaa ilaa inta socodka waxtarka leh uu sii jiro. |
| Sidee badeecadu u dhaqantaa heerkulka xagaaga iyo jiilaalka? | Muhiim u ah wax soo saarka xasilloon ee sanadka oo dhan. |
| Miyaynu ku tijaabin karnaa xabagta dhagaxeena? | Tijaabada suufka dhabta ah waxay daaha ka rogtaa dhexgalka, midabka iyo waxqabadka turxaan bixinta. |
| Waa maxay dulqaadka dufcadda-ilaa-dufcada la filayo? | Muhiim u ah wax soo saarka otomaatiga ah iyo joogtada ah. |
Talo soo jeedin: Dooro habka marka hore, ka dibna CPS
Habka ugu fiican ee lagu dooran karo resin epoxy ee farsamaynta dhagaxa waa in lagu bilaabo dhibaatada habka halkii lambarka viscosity.
Haddii ujeedadu tahay xoojinta qoto dheer ee granite-yar-fissured, mudnaanta sii nidaamka viscosity hoose oo leh waqti shaqo oo ku filan iyo isku xirnaan gudaha ah oo xooggan.
Haddi hadafku yahay xoojinta mesh, dooro resin si siman u qoysin kara fiilooyinka iyada oo aan la xakameynin qulqulka biyaha oo si la isku halleyn karo ugu daaweeya heerkulka aqoon isweydaarsigaaga.
Haddi hawshu isticmaasho vacuum impregnation, mudnaan sii iska caabbinta socodka hoose, viscosity xasiloon, sii dayn hawo, iyo daaqad shaqo oo dheer oo ku filan faleebo dhamaystiran.
Haddii dayactirku ku lug yeesho godadka ama tolida ballaaran, jirka sare ama nidaamka thixotropic ayaa laga yaabaa inuu bixiyo koontarool ka fiican tan galka galka aadka u hooseeya.
Haddii aadan hubin meesha aad ka bilaabayso, dib u eeg Veropoxy's portfolio alaabta epoxy dhagax oo la socda shirkadda dhagax epoxy qaybta Aqoonta, dabadeed is barbar dhig hababka musharraxiinta adiga oo isticmaalaya dhagaxaaga dhabta ah, heerkulka aqoon-is-weydaarsiga, habka codsiga, wareegga daaweynta, iyo habka nadiifinta.
Su'aalaha Inta Badan La Isweydiiyo ee Ku Saabsan Viscosity Resin Epoxy
1. Waa maxay epoxy viscosity ee ugu fiican farsamaynta dhagaxa?
Ma jiro hal-ku-jiid wanaagsan oo geeddi-socod kasta oo dhagax ah. Dildilaaca yaryar ee granite guud ahaan waxay ka faa'iidaystaan resinka galka hoose ee viscosity, halka godadka waaweyn iyo hagaajinta toosan ay inta badan u baahan yihiin jidh dheeraad ah. Taageerada mesh iyo faleebada faakuumka waxay sidoo kale u baahan yihiin socod wanaagsan, laakiin xawaaraha daweynta, heerkulka, iyo wakhtiga shaqada waa in isla mar la tixgeliyo.
2. 400-600 cP ma loo arkaa viscosity hoose ee epoxy dhagaxa?
Qaar badan oo ka mid ah qaababka habaynta dhagxaanta ee Veropoxy, ku dhawaad 400-600 cP ayaa loo isticmaalaa araji yar ama codsiyada socodka sare sida dayactirka granite, hagaajinta marmar, iyo taageerada mesh. Si kastaba ha ahaatee, "muwadixii hoose" maaha kala soocida caalamiga ah. Had iyo jeer is barbar dhig xaaladaha tijaabada iyo codsiga loogu talagalay ka hor inta aan la daweyn tirada tirada sida heerka warshadaha.
3. Heerkulku ma saameeyaa viscosity resin epoxy?
Haa Heerkulka hoose wuxuu guud ahaan kordhiyaa viscosity ee epoxy-ga aan la dawayn, taas oo adkeynaysa in la shubo, la qaso, la faafiyo, oo la dhex galo. Heerkulka sare wuxuu guud ahaan yareeyaa viscosity laakiin sidoo kale wuxuu dedejin karaa daaweynta. Si loo farsameeyo dhagaxa warshadaha, heerkulka resin, heerkulka dhagaxa, iyo heerkulka aqoon isweydaarsiga waa in dhamaantood la tixgeliyaa.
4. Miyay ka xoog badan tahay muuqaalka hoose ee epoxy?
qasab maaha. Viscosity wuxuu qeexayaa habdhaqanka socodka ka hor daawaynta; lafteedu ma qeexdo xoogga ugu dambeeya ee farsamada. Maqaarka-mugdiga-hooseeya wuxuu ku siin karaa dhexgalka wanaagsan ee dildilaaca yar yar, laakiin waxqabadka kama dambaysta ah wuxuu sidoo kale ku xiran yahay kimistariga resin, kimistariga adag, saamiga isku dhafka ah, xaaladaha daaweynta, dhejinta, iyo qaabka dhagaxa.
5. Sidee bay warshadda dhagaxu u barbar dhigi kartaa viscosity epoxy ka hor inta aan la dalbanin bulk?
Is barbar dhig viscosity isku qasan isla heerkul iyo, sida ugu fiican, adoo isticmaalaya habab tijaabo ah oo barbar dhig ah. Ka dib ku samee tijaabooyinka la xakameeyey dhagaxaaga. Diiwaangeli galitaanka, isticmaalka resinka, wakhtiga shaqada, daawaynta, muuqalka dabaysha, midabka midabka, buuxinta cilada, iyo joogteynta wax soo saarka. Alaabada sida ugu fiican ugu shaqeysa khadka wax soo saarka dhabta ah ayaa ka qiimo badan kan leh lambarka CPS ee ugu soo jiidashada badan ee warqadda.
Sida loo doorto viscosity-ka saxda ah ee Epoxy ee Habaynta Dhabta ah ee Dhagaxa
Viscosity epoxy-ga saxda ah maaha bartilmaameedka caalamiga ah ee CPS. Waa dheellitirka u dhexeeya qulqulka resin, qaab-dhismeedka dhagaxa, cabbirka cilladda, heerkulka aqoon-is-weydaarsiga, wakhtiga shaqada, habdhaqanka daaweynta, iyo dusha sare ee loo baahan yahay. Warshadaha dhagxaanta, viscosity waa in loola dhaqmaa sidii halbeeg-soo-saar halkii ay ka ahaan lahaayeen tiro go'doonsan oo xaashida xogta farsamada ah.
Ka bilow dhibaatada habaynta
Daloolada yaryar iyo dildilaaca yaryar waxay u baahan yihiin qulqul ku filan si uu resinku u dhex galo ka hor intaysan bilaabin gelitaanka. Nusqaamaha ballaaran waxay u baahan yihiin jir dheeraad ah si ay walxuhu ugu sii jiraan gudaha aagga dayactirka. Taageerada mesh waxay u baahan tahay qoynta la kontoroolo iyo qulqulka la maarayn karo, halka faleebada faakuumku ay ku xidhan tahay iska caabbinta socodka hooseeya iyo wakhti shaqo oo ku filan oo uu resin u dhex maro daldaloolada iyo jeexjeexyada gudaha.
CPS hoose had iyo jeer ma roona
Epoxy viscosity aadka u hooseeya waxa ay wanaajin kartaa dhexgalka, laakiin waxa ay sidoo kale kordhin kartaa qulqulka biyaha, isticmaalka resinka, ama lumitaanka alaabta daldaloolada waaweyn. Waxa kale oo laga yaabaa inay ku dhaafto wax aan ku filnayn oogada agteeda marka codsigu u baahan yahay buuxinta farqiga ama dhismaha dusha sare. Doorashada ugu fiican waa viscosity ugu hooseeya kaas oo bixiya dhexgalka loo baahan yahay iyada oo aan la hurin xakamaynta habka ama tayada dhamaystirka.
Ku dhig viscosity arjiga
Dildilaaca yaryar ee granite cufan:
Mudnaanta sii galitaanka hoose ee viscosity-hoose si uu resin-ku u gaadho fiix gudaha ah ka hor inta aan la daaweyn.
Dayactirka marmar:
dheellitirka viscosity leh xasilloonida midabka, dhexgalka, caabbinta jaalaha ah, iyo muuqaalka la filayo.
Taageerada mesh dhagaxa:
dheellitirka awoodda qoynta, xakamaynta socodka, dhejinta, caabbinta sagxada, iyo daaweynta waxqabadka heerkulka dhabta ah ee aqoon-is-weydaarsiga.
Vacuum infusion:
kala horraysii viscosity hoose, nolosha dheriga oo ku filan, socodka deggan, iyo sii daynta hawo wanaagsan si uu xabagta u dhex maro daldaloolada iyo dildilaaca yar yar ka hor inta aan la jarin.
Tolmo ballaaran ama godadka:
Tixgeli hababka jirka-sare ama thixotropic halkii aad ka malaysan lahayd resin-ka galitaanka ultra-hooseeya inuu bixin doono awood ku filan oo buuxin ah.
Ha barbar dhigin Adeegyada Badbaadinta Ilmaha (CPS) la'aanteed xaaladaha tijaabada
Heerkulka cabbirka, isku dhafan oo ka soo horjeeda viscosity-ka aan la isku qasin, xaaladaha tijaabada wareega, A: saamiga B, waqti dhaaftay isku darka ka dib, heerkulka dhagaxa, xilliga aqoon-is-weydaarsiga, xawaaraha wax-soo-saarka, iyo joogteynta dufcadda ayaa dhammaantood saameyn kara dabeecadda dhabta ah ee adduunka. Tilmaamaha wax iibsiga ee diiwaangeliya kaliya "500 CPS" ma bixiso macluumaad ku filan isbarbardhigga alaab-qeybiyaha la isku halayn karo.
Maxaa iska beddelaya farsamaynta dhagxaanta xirfadleyda ah?
Soo-saareyaal-yaqaannada dhagxaanta ayaa si isa soo taraysa uga fogaanaya hal koolo oo caalami ah codsi kasta. Warshado badan ayaa isticmaalaya nidaamyo gaar ah oo codsi ah oo loogu talagalay gelitaanka granite madow, xakamaynta midabka iftiinka-dhagaxa, wax-qabadka cad-maarble aan wasakh lahayn, taageeridda mesh heerkulka hooseeya, wax soo saarka heerkulka sare, faleebo faaruq ah, iyo xaalado kale oo si cad loo qeexay.
Tani waxay sidoo kale beddeshaa sida iibsadayaashu ay tahay inay u qiimeeyaan alaab-qeybiyeyaasha. Xogta farsamada, tijaabada muunada, talooyinka heerkulka gaarka ah, joogteynta dufcada, iyo taageerada codsigu waxay noqonayaan kuwo aad uga muhimsan sheegashooyinka guud sida "xoog sare", "daawaynta degdega ah," ama "mugsoon hoose."
Talo bixin Wax ku ool ah
Haddii dildilaaca-yar-yar ay yihiin dhibaatada, ka bilow dhexgalka. Haddii daadku yahay dhibka, kordhi xakamaynta jidhka ama socodka. Haddii heerkulka xilliyeedku isbeddelo waxqabadka, qiimee viscosity iyo daaweynta kiimikada si wadajir ah. Haddii laba hab oo epoxy ay leeyihiin qiime isku mid ah CPS laakiin ay soo saaraan natiijooyin kala duwan, is barbar dhig wakhtiga shaqada, qoynta, rheology, isdhexgalka dhagxaan, iyo dabeecadda daawaynta. Epoxy-ka saxda ah ma aha si fudud sheyga leh viscosity-ka ugu hooseeya - waa nidaamka qulqulkiisu uu faa'iido u leeyahay inta lagu jiro wareeggaaga wax-soo-saarka dhabta ah.
Kahor intaadan dalban bulk, ku tijaabi xabagta granite adiga kuu gaar ah, marmar, travertine, seeraha mesh-backed, ama habka faleebo faleebo. La wadaag nooca dhagaxa, xaalada dildilaaca, heerkulka aqoon isweydaarsiga, habka codsiga, wakhtiga daawaynta ee loo baahan yahay, iyo dhibaatada wax soo saarka ee hadda jirta si nidaamka epoxy-ga lagu qiimeeyo xaaladaha habaynta dhabta ah ee aan ahayn bartilmaameedka guud ee CPS.
Tixraacyo
- TS EN ISO 2555: 2018 caagadaha - Resins ee gobolka dareeraha ah - Go'aaminta viscosity muuqda iyadoo la adeegsanayo Viscometer wareeg ah
- ASTM D2196 - Hababka Tijaabada Caadiga ah ee Guryaha Rheological ee Walxaha Aan Newtonian ahayn ee Viscometer Rotational
- NIDAAMKA GALBEEDKA – Buugga Isticmaalaha Epoxy & Hagaha Alaabta
- Gurit – GR110 Xaashida Xogta Alaabta Qaab-dhismeedka Resin System
- Veropoxy-Uur-U-hooseeya indho-beelka Galitaanka Deep Granite
- Veropoxy- Midabka Kobcinta Epoxy ee Granite Iftiinka
- Veropoxy – Resin Epoxy oo loogu talagalay Dayactirka Marble & Kobcinta Midabka
- Veropoxy – High Temperature Odorless Epoxy for Stone Mesh Backing
- Veropoxy – Vacuum Infusion Solutions