Chidimbu chekukurumidza:

Usati wahodha epoxy resin yakawanda, fekitori yematombo inofanirwa kuedza chigadzirwa pamarble, granite, onyx, kana dombo rakagadzirwa pasi pemamiriro chaiwo ekugadzira. Tarisa kusanganisa maitiro, viscosity, nguva yekushanda, kurapa, kupinda, kunamatira, shanduko yeruvara, kupenya kuita, kushandiswa kweresin, uye batch kuenderana. Usabvumira epoxy nekuti imwe sampuli "inotaridzika zvakanaka." Tsanangura nzira yekupasa / yekutadza kutanga, edza akati wandei anomiririra slabs, enzanisa zvichienderana neyako ikozvino yekugadzira yekutanga, uye simbisa mashandiro patembiricha yezhizha nechando.

Kutenga maindasitiri epoxy resin kwakasiyana nekutenga chikamu chakapedzwa.

Mutengesi anogona kutumira chigadzirwa chehunyanzvi, asi icho chigadzirwa chinogona kuramba chisina kunaka kune dombo rako, tembiricha yako yekugadzira, kurongedza kwako kutevedzana, vashandisi vako, kana nguva yako yekutenderera.

Ichi ndicho chikonzero fekitari yematombo haifanire kubata sampuli sechipo chidiki chekusimudzira.

Sample mudziyo wekukodzera.

Chinangwa hachisi chekungopindura:

"Iyi epoxy inoshanda here?"

Mubvunzo uri nani ndewekuti:

"Iyi epoxy inogona kudzokorodza kuburitsa inogamuchirwa yakapedzwa slab pasi pemamiriro edu chaiwo ekugadzira pamutengo unogamuchirwa wekutengesa?"

Musiyano iwoyo unokosha.

Resin inogona kupinda zvakanaka asi ichidya zvinhu zvakawandisa. Imwe inogona kurapa nekukasira asi ichisiya vashandi nguva shoma yekushanda. Iyo yakanyatsojeka sisitimu inogona kuramba ichigadzira rima rakasviba pane porous chena marble. Kunamira kwakasimba kunogona kunetsa kukwenenzvera. Muenzaniso unogona kuita zvakanaka pa 24°C asi wozononoka muchando kana kunyanyo shanda muzhizha.

Veropoxy ikozvino dombo epoxy chigadzirwa portfolio inoratidza iyi nzira yekushandiswa-chaiyo, ine masisitimu akasiyana egranite, marble, dombo jena, mesh backing, vacuum infusion, semi-akakosha dombo, uye mamwe mamiriro ekugadzirisa.

Mapeji mazhinji echigadzirwa cheVeropoxy anopawo samples chaizvo kuitira kuti mafekitori akwanise kuongorora mashandiro asati atenga zvakawanda. Ndiwo chaiwo mashandisirwo anofanirwa kuitwa nehunyanzvi hwekutenga zvinhu.

Nei Sample Kuedza Zvine Basa Pamberi peBulk Epoxy Order

Iyo epoxy technical data sheet inokuudza maitiro echigadzirwa pasi pemamiriro akatsanangurwa.

Fekitari yako inogona kusashanda pasi pemamiriro iwayo.

Dombo rinoshanduka-shanduka

Dombo rechisikiro harisi rakagadzika repurasitiki pani.

Mabhii maviri emarble kubva kune imwechete quarry anogona kusiyana mu:

  • porosity;
  • micro-crack density;
  • mineral structure;
  • kubatwa kwemvura;
  • translucency;
  • pamusoro roughness;
  • kunzwa kwemavara; uye
  • utera hwemukati.

Iyo epoxy inoita zvakanaka pane rimwe dombo inogona kuburitsa mhedzisiro pane imwe.

Maitiro ako ekugadzira anoshandura mhedzisiro

Performance inogonawo kuchinja ne:

  • tembiricha yemusangano;
  • dombo tembiricha;
  • kusanganisa midziyo;
  • batch size;
  • manual kana otomatiki application;
  • vacuum pressure;
  • mesh tsanangudzo;
  • nguva yekuzorora;
  • kugaya kutevedzana; uye
  • polishing abrasives.

Ichi ndicho chikonzero mupi werabhoritari data achifanira kupfupisa resin-kwete kutsiva muyedzo wako wefekitori.

Mutengi takeaway: Iyo inonyanya kubatsira epoxy sampuli bvunzo haisi iyo yakanyanya kuoma murabhoritari bvunzo. Ndiyo bvunzo inoburitsa mamiriro ayo anozoona kuti chigadzirwa chinobudirira here kana kutadza pamutsetse wako wekugadzira.

Tsanangura Kupfuura/Kukundikana Maitiro Asati Sample Yasvika

Uyu ndiwo mumwe wemisiyano mikuru pakati pehunyanzvi hwekuita uye bvunzo dzenguva dzose.

Usaisa epoxy kutanga uye wosarudza mushure mekunge "unoida."

Tsanangura maitiro ekugamuchirwa usati waedzwa.

Tanga neyako ikozvino kugadzira baseline

Kana fekitori yako yatoshandisa epoxy yakatenderwa, nyora kuti chigadzirwa ichocho chinoita sei.

Somuenzaniso:

  • resin kushandiswa pa square mita;
  • avhareji yenguva yekushanda;
  • nguva yekuzorora;
  • nhamba yema slabs akagadziriswa pabatch;
  • reject rate;
  • polishing result;
  • kugadzirisa kuonekwa;
  • mesh-backing kubata nguva; uye
  • mutengo pa slab yakapera.

Iyo itsva epoxy inofanira kuenzaniswa neinotangira pane kuongororwa iri yega.

Sarudza kuti kukundikana kupi kusingagamuchirwi

Kune marble machena, halo yero inooneka inogona kunge iri kurambwa otomatiki.

Kune dema regraniti, kusakwana kupinza mutswe kungave kwakakosha zvakanyanya.

Kune mesh kutsigirwa, kupepeta mushure mekubata kungave kusingatenderwe.

Kune vacuum infusion, kusakwana kudzika kwekupinda kunogona kuita kuti muyedzo wese ushaye basa.

Muedzo 1: Ongorora Zvinyorwa zveTekinoroji Usati Wavhura Sample

Muenzaniso unofanirwa kusvika uine ruzivo rwakakwana kuti uishandise nemazvo.

Ongorora iyo TDS

Iyo Technical Data Sheet inofanirwa kujekesa ma paramita anoenderana nekugadzirwa, akadai se:

  • chigadzirwa chiziviso;
  • yakakurudzirwa application;
  • A: B kusanganisa ratio;
  • kana reshiyo inoenderana nehuremu kana huwandu;
  • viscosity;
  • tembiricha inokurudzirwa;
  • kushanda kana kuporesa nguva;
  • kuchengetedza mamiriro; uye
  • mirayiridzo yekushandisa.

Ongorora iyo SDS

Iyo Safety Data Sheet haisi gwaro rekuita.

Inopa ruzivo rune chekuita nenjodzi, kubata, kuchengetedza, kudzora kudzora, PPE, rubatsiro rwekutanga, kutakura, uye kuraswa.

Mutengi akakomba weindasitiri anofanira kutarisira zvese zvinyorwa zvehunyanzvi uye zvekuchengetedza.

Tarisa uone kana mamiriro ebvunzo akatsanangurwa

A viscosity value yakadai se "500 CPS" inoreva zvishoma kana mutengesi asina kutaura kana kudzora mamiriro akakodzera ekuyera.

Saizvozvo, "60-maminetsi kurapwa" haina kukwana kunze kwekunge iwe wanzwisisa tembiricha uye kuti chii chinorehwa nemupi wekurapa.

Muedzo 2: Simbisa Chigadzirwa Kuzivikanwa uye Mamiriro

Usati wasanganisa chero chinhu, ongorora sampuli pachayo.

Tarisa mavara

Confirm:

  • resin code;
  • harder code;
  • batch number;
  • ruzivo rwekugadzira kana kupera kana rwapihwa;
  • mixing ratio; uye
  • mirairo yekuchengetedza.

Ongorora chitarisiko

Tsvaka:

  • sediment isingatarisirwi;
  • crystallization;
  • kusvibiswa kwakanyanya;
  • kupatsanurwa kwechikamu;
  • midziyo inodeuka; kana
  • kusvibiswa.

Usafunge kuti shanduko yese yekuona inoreva kuti chigadzirwa hachina kukwana, nekuti mamwe masisitimu eresin anogona kupenya kana kugadzikana mune mamwe mamiriro.

Kana chitarisiko chakasiyana nemirairo yemugovera, mira uye bvunza usati waedza.

Muedzo 3: Tarisa Kusanganisa Maitiro

Iyo yekugadzira-inoshamwaridzika epoxy inofanirwa kuve iri nyore kuyera uye kusanganisa nguva dzose.

Shandisa reshiyo chaiyo yakatarwa

Veropoxy's stone epoxy systems havasi vese vanoshandisa chiyero chakafanana.

Somuenzaniso, its Marble Repair & Color Enhancement system inoshandisa 100:25 nehuremu, nepo iyo Ruvara Runowedzera Epoxy yeChiedza Granite inoshandisa 100:30 nekurema.

Usamboshandisa zvakare reshiyo imwechete nekuda kwekuti zvigadzirwa zviviri zvinotaridzika zvakafanana.

Cherechedza kusanganisa kufanana

Rekodha kana:

  • zvikamu zviviri izvi zvinosanganiswa nyore;
  • mitsetse yasara;
  • mhepo yakawanda inotangwa;
  • musanganiswa unopisa nokukurumidza; kana
  • viscosity inoshanduka zvisina kujairika panguva yekusanganiswa.

Pakugadzirwa kwakakosha, shandisa nzira yakamisikidzwa yekusanganisa kuitira kuti mupi wega aenzaniswe zvakaringana.

Muedzo wechina: Kuyera kana Enzanisa Viscosity uye Kuyerera

Viscosity ndeimwe yeanonyanya kubatsira maitiro-kutonga maparamita mumatombo epoxy.

Asi haifanirwe kubatwa sechibodzwa chemhando yepamusoro.

Epoxy Resin QC Kuedza

Nei viscosity ichikosha

Zvinokanganisa:

  • micro-crack kupinda;
  • kupararira kwepamusoro;
  • mesh wetting;
  • vacuum infusion;
  • resin kushandiswa;
  • runoff; uye
  • gap retention.

Enzanisa pasi pekushisa kwakafanana

Viscosity inoshanduka zvakanyanya nekushisa.

Kana Mutengesi A akaedzwa pa15 ° C uye Mutengesi B pa25 ° C, kuenzanisa kwako hakuna simba.

Condition samples kune imwe tembiricha usati waita mutongo.

Shandisa bvunzo yepamutemo kana viscosity iri chibvumirano chechibvumirano

ISO 2555 inopa yakajairika nzira yekutenderera yekuona inooneka viscosity yemvura resins.

ASTM D2196 inopa nzira dzekuratidzira kutenderera viscosity uye rheological maitiro ezvisiri zveNewtonian zvinhu.

Yemazuva ese ekuongorora fekitori, zvisinei, inodzorwa yekuenzanisa kuyerera bvunzo inogona kuramba ichibatsira kana tembiricha yakafanana, huwandu, substrate, uye nguva zvichichengetwa.

Muedzo 5: Yera Hupenyu Hwehari uye Inobatsira Nguva Yekushanda

Usavhiringa hupenyu hwehari nenguva yekushanda yekugadzira.

Hupenyu hwehari hunongotaura chikamu chenyaya

Iyo yakasanganiswa epoxy inogona kuramba iri mvura mumudziyo uchiri kutonyanya kukora kuti micro-crack ipinde.

Nekugadzira matombo, nguva yekushanda inobatsira inofanira kutsanangurwa nekushandiswa.

Somuenzaniso:

  • Kupinda kwe crack kunodzikira rinhi?
  • Ndirini panoita mesh yakaoma kunyorova?
  • Kuyerera kwevacuum kunononoka riini?
  • Kupararira kwepamusoro kunove kusina kuenzana riini?

Shandisa realistic batch saizi

Kapu ye100 g yemurabhoritari inogona kuita zvakasiyana kubva ku5 kg yekugadzira batch nekuti kurapa epoxy kunoburitsa kupisa.

Mazhinji mahombe anogona kuchengetedza kupisa kwakanyanya uye kupfupisa hupenyu hwepoto hunoshanda.

Muedzo wechitanhatu: Ongorora Mushonga Profile

"Zvakaoma" hazvina kukwana.

Fekitori inofanirwa kunzwisisa kana iyo epoxy ichisvika zvakasiyana siyana zvekugadzira.

Record kubata nguva

Ndeipi iyo slab inogona kuve yakachengeteka:

  • lifted;
  • turn;
  • stacked;
  • kuendeswa kungoro;
  • kutumirwa ku calibration; kana
  • kutumirwa kunokwenenzvera?

Tarisa kuti hauna kupora here

Yambiro zviratidzo zvinosanganisira:

  • tackiness;
  • nzvimbo dzekugadzirisa rubbery;
  • zvinhu zvinyoro pasi pekumanikidzwa;
  • kuzora panguva yekupenya;
  • kunhuhwirira kusina kujairika mushure mekurapa kunotarisirwa; kana
  • kuoma kwakasiyana pakati pezvikamu.

Murabhoritari kurapwa kuyedzwa kunogona kudzika zvakadzika

Kuti uwane dhigirii repamusoro remupi, Differential Scanning Calorimetry inogona kushandiswa kuratidza maitiro ekuita uye dhigirii rekutendeuka pasi pemamiriro akatsanangurwa.

ISO 11357-5 inopa yakamisikidzwa DSC chimiro chekutarisa tembiricha yekuita, nguva yekuita, enthalpy, uye dhigirii rekutendeuka.

Iri rudzi rwebasa rerabhoritari rinobatsira kune yakadzama tekinoroji kusimbiswa asi haina kudikanwa kune yega yega sampu fekitori.

Muedzo wechinomwe: Ongorora Kupinda padombo chairo

Iyi ndeimwe yebvunzo dzakanyanya kukosha dzedombo epoxy uye imwe yeakaomesesa kutsiva neiyo generic laboratory data.

Shandisa zvinomiririra kukanganisa

Edza pane chaiyo:

  • micro-cracks;
  • natural fissures;
  • vhura pores;
  • dense granite;
  • marble akapfava; kana
  • vacuum-infusion slabs.

Usatonga kupinda kubva panzvimbo yakanyorova

A glossy wet slab inokuudza chero chinhu nezve mukati mekupinda.

Mushure mekurapa, ongorora zvikamu zvakachekwa, matunhu ekumucheto, akaputsika anomiririra pazvinenge zvakakodzera, kana dzimwe nzira dzakatenderwa dzebvunzo dzemukati.

Tarisa kupinda-pamusoro zvakare

Kupinda kwakawanda hakusi nani nguva dzose.

Pane porous chena marble, kupinda kwakanyanya kunogona kugadzira rima halos kana kunyorova-kutaridzika kushanduka kwemaziso.

Pachikumbiro ichocho, kupinda kunodzorwa kunogona kukosha kudarika kudzika kwepamusoro.

Muedzo wechisere: Tarisa Kuchinja Kwemavara, Yellowing uye Optical Effects

Muedzo uyu wakakosha kune chena marble, light granite, onyx, uye translucent ibwe.

Mufananidzo usati uye shure kwechiedza chinodzorwa

Shandisa mwenje wakafanana, kona yekamera, uye mamiriro epamusoro.

Mapikicha efoni akatorwa mumakamuri akasiyana humbowo husina kunaka.

Siyanisa kutsvuka kwechokwadi kubva pamumvuri

Nzvimbo ine rima yakatenderedza mutswe inogona kubva mukupinzwa kweresin pane kutsvuka kwekemikari.

Izvi zvakakosha nekuti kuchinja kune yakajeka epoxy hakuzogadzirise dambudziko rekupinda-pamusoro.

Veropoxy's Kwete-Yellowing Epoxy for Hard White Marble yakanyatsoiswa padhuze nekupinda kwakadzora uye kuderera zvakanyanya kutsvuka kwedombo rinonzwa ruvara.

Funga kuchembera kune mapurojekiti ekutanga

Kana ibwe richizoiswa padyo nechiedza chezuva chakasimba kana kana kuchena kwenguva refu kwekuona kuchikosha, yakakwidziridzwa UV kana kupisa kuenzanisa kuyedzwa kunogona kubatsira chinzvimbo chemumiriri.

Usadudzire kukurumidza kuchembera sekufungidzira chaiko kwehupenyu hwesevhisi kunze kwekunge nzira yekuyedza inotsigira mhedziso iyoyo.

Muedzo 9: Ongorora Kunamatira uye Kukundikana Mode

"Kubatana kwakasimba" ndechimwe chezvinhu zvinowanzozivikanwa zvekutengesa epoxy.

Fekitari yehunyanzvi inofanirwa kutarisa kuti chisungo chinokundikana sei.

Adhesive kukundikana

Kana epoxy yakanyatsoparadzanisa kubva padombo pamusoro, iyo interface inogona kunge isina simba.

Kukundikana kwakabatana

Kana kutadza kukaitika mukati meyakarapwa resin layer, chisungo kune substrate chinogona kunge chakasimba kupfuura simba remukati resin pachiitiko ichocho.

Kukundikana kwedombo

Kana ibwe richitsemuka apo chinonamira chinoramba chakabatanidzwa, iyo substrate inogona kunge isina kusimba chikamu chegungano.

Musiyano uyu unogona kuve unodzidzisa kupfuura imwe mbishi nhamba yesimba.

Formal adhesive bvunzo dzine mashoma akananga kutamisa

ISO 4587 inotsanangura kuyedzwa kwe-lap-shear kune akaomeswa akasungwa magungano.

ASTM C882 inoongorora epoxy bond simba mune kongiri slant-shear kumisikidzwa.

Idzi nzira dzinogona kuzivisa kufunga kwemurabhoritari, asi hadzifanire kungobatwa sepasi rose / kutadza mwero wemarble kana granite epoxy pasina kusimbisa kushanda.

Kune dombo rechisikigo, bvunzo dhizaini inofanirwa kuratidza iyo chaiyo substrate uye mamiriro ekuremedza.

Muedzo 10: Tarisa Kuoma-Asi Usashandise Kuoma senzira yekudimbudzira kune zvese

Iyo epoxy yakarapwa iyo inoramba isingatarisirwe yakapfava inogona kukonzera kupukuta kana kusimba matambudziko.

Durometer yekuyedza inogona kupa inodzokororwa yekugadzira-yekudzora chiratidzo.

ISO 868 inotsanangura kuomarara kweShore kuyedzwa kwemapurasitiki uchishandisa durometer nzira.

Asi kuoma kwega hakuratidzi kunamatira kwakanaka, kusimba, kupinda, kana kusimba kwenguva refu.

Iyo epoxy yakaoma kwazvo inogona kuramba yakabatana zvisina kunaka kune dombo.

Shandisa kuomarara seimwe QC metric, kwete mutongo wekupedzisira.

Muedzo wechi11: Mhanya iyo chaiyo yekukuya uye yekupukuta Sequence

Apa ndipo apo akawanda ma laboratory-akakwana samples anokundikana.

Ibwe epoxy chikamu chegadziriro yekugadzira.

Kana slab ichizopedzwa, muyedzo wekukodzera unoda kukwenenzverwa.

Epoxy Resin Polishing Mhedzisiro

Tarisa kune resin kudhonza-kunze

Resin yakapfava kana isina kusungwa zvakanaka inogona kubviswa kubva pakatsemuka panguva yekukuya.

Tarisa kuzora

Zvinhu zvisina kupora zvinogona kuzora pamusoro pedombo.

Tarisa gloss kuenderana

Iyo nzvimbo yakagadziridzwa haifanire kugadzira chigamba chakasvibira chakajeka, ridge rakasimudzwa, kana chitarisiko chakasiyana kunze kwekunge iyo yakarongwa application ichibvumira.

Tarisa mapinhole mushure mekupukuta

Kurapwa kwepamusoro kunogona kutaridzika kuzere kusati kwakuya uye kuburitsa mapinhole chete kana zvinhu zvabviswa.

Ichi ndicho chikonzero iyo yekupedzisira yakakwenenzverwa slab-kwete iyo yakanyorova epoxy-ndicho chigadzirwa chaicho.

Muedzo 12: Kuyera Resin Kushandiswa

Iyi ndeimwe yebvunzo dzakanyanya kukosha mune zvekutengesa uye imwe yeinonyanya kufuratirwa.

Mutengo wekutenga pakirogiramu haukuudze mutengo pane yapera slab.

Rekodha magiramu kana makirogiramu pane slab

Shandisa chikero.

Usayere kubva pamari yasara mubhaketi.

Enzanisa mutengo pa square mita

Kana Epoxy A ichidhura 10% zvishoma pakirogiramu asi ichidya 25% yakawanda, inogona kunge iri sarudzo inodhura yekugadzira.

Batanidza mutengo wekugadzirisa zvakare

Mutengo chaiwo unofanirwa kufunga nezve:

  • epoxy kushandiswa;
  • labour;
  • kuporesa kunonoka;
  • rejects;
  • re-polishing;
  • akaputsika slabs; uye
  • yakarasika nguva yekugadzira.

Muedzo wechi13: Dzokorora Muedzo panguva yeZhizha neChando Tembiricha

Muenzaniso unotenderwa pane imwe tembiricha yekamuri yakanaka unogona kutadza mwaka.

Kutonhora mamiriro

Kudzikira tembiricha kazhinji:

  • kuwedzera viscosity isina kupora;
  • kuderedza kuyerera;
  • kunonoka kupinda;
  • kuwedzera kupora; uye
  • kuchinja kubata nguva.

Hot conditions

Tembiricha dzakakwirira kazhinji:

  • kuderedza viscosity yekutanga;
  • kuwedzera kuyerera;
  • accelerate reaction;
  • kupfupisa nguva yekushanda; uye
  • kuwedzera exothermic njodzi mumapoka makuru.

Kune mafekitari ane mutsauko wakakura wemwaka, mutengesi angangoda kurumbidza masisitimu ekuomesa akasiyana.

Veropoxy, semuenzaniso, parizvino inopa zvakasiyana kuderera-kupisa uye high-temperature mesh-backing systems.

Muedzo wechi14: Ongorora Batch-to-Batch Consistency

Imwe sampuli yakakwana haikodzeri mutengesi.

Kugadzirwa kwehuwandu kunoenderana nekudzokorora.

Sei kusachinja-chinja kuchikosha

Kusiyana pakati pemabheti kunogona kuchinja:

  • viscosity;
  • nguva yekushanda;
  • cure speed;
  • color;
  • kupinda;
  • resin kushandiswa; uye
  • hunhu hwekukwenenzvera.

Usabvumira mutengesi zvichibva pane imwe chete yakagadzirwa neruoko

Sezvineiwo, qualification inofanira kufambira mberi nematanho:

Murabhoritari kana diki sampuli → muyedzo wefekitori → kurongeka kwekuyedza → kurongeka kwakawanda.

Izvi zvinopa mutengi mukana wekuona kana mabheti ekugadzira ekutengesa achiburitsa mhedzisiro yemuenzaniso.

Mangani Slabs Unofanira Kuedza?

Iko hakuna nhamba yepasirese nekuti njodzi inoenderana nekushandisa, kukosha kwedombo, kusiyanisa kwemaitiro, uye saizi yehurongwa.

Asi imwe slab kashoma kukwana.

Shandisa akawanda anomiririra samples

Seti inoshanda yekukodzera inofanira kusanganisira misiyano yakadai se:

  • dense slabs;
  • mamwe porous slabs;
  • slabs ane micro-cracks;
  • slabs ane hurema hwakakura;
  • mavara akasiyana kana veining; uye
  • yakajairika kugadzirwa-mhando yezvinhu, kwete chete akakwana samples.

Iyo yakakwira mutengo wekukundikana, kusimba kwechirongwa chekufanirwa kunofanirwa kuve.

Epoxy Resin Factory Qualification Scorecard

Test Area Zvekurekodha Yakakurudzirwa Factory Sarudzo
Zvinyorwa TDS, SDS, zvigadzirwa makodhi, batch data Ramba kana chitupa chehunyanzvi chisina kujeka
Kusanganisa Ratio kurongeka, kufanana, mhepo sumo Inofanirwa kudzokororwa nevashandisi vakajairwa
Viscosity / Flow Flow at controlled tembiricha Inofanirwa kuenderana nekupinda kana kuzadza application
Nguva Yekushanda Inobatsira application window Inofanira kudarika nguva chaiyo yekuita nekuchengetedza margin
Mushonga Kubata nekukwenenzvera kugadzirira Inofanirwa kukodzera kutenderera kwekugadzira
Kupinda Kudzika uye kufanana Inofanirwa kusvika kune inodiwa kuremara pasina kutama zvakanyanya
Kugadzikana Kwemavara Yellow, staining, shadowing Inofanirwa kusangana nematombo-zvakananga kutaridzika zvinodiwa
Adhesion Bond simba uye kukundikana muoti Hapana isingagamuchirwi interface kutadza
Kuoma Kuenzanisa kwakapora kuoma Hapana nzvimbo dzakapfava kana dzisingawirirani
Kupukuta Gloss, pinholes, smear, dhonza-kunze Kugadziriswa kwapera kunofanirwa kugamuchirwa mune zvekutengesa
Kushandiswa kg/slab kana g/m² Inofanirwa kuzadzisa chinangwa chemutengo
Mwaka Kugadzikana Kutonhora uye kupisa miedzo Inofanira kuramba ichidzoreka kwegore rose
Batch Consistency Mijenya yakawanda kana kurongeka kwekuedza Migumisiro inofanira kudzokororwa

Red Flags Panguva yeEpoxy Supplier Qualification

Mutengesi haakwanisi kupa chiyero chakajeka chekusanganiswa

Ichi chinhu chakakosha tekinoroji chinodiwa kune maviri-chikamu masisitimu.

Viscosity inopiwa pasina mamiriro anobatsira

Nhamba yeCPS yakashama haina kukwana kuenzanisa kwakakomba.

Dombo rimwe nerimwe rinokurudzirwa kushandisa epoxy yakafanana

Dense dema granite, yakapfava chena marble, mesh inotsigira, uye vacuum infusion haina zvakafanana kugadzirisa zvinodiwa.

Mutengesi haakurudzire kuyedzwa kwemuenzaniso

Pakutenga kwakawanda kwemaindasitiri, izvi zvinofanirwa kumutsa mibvunzo.

Muenzaniso unoita zvakanaka chete pasi pemamiriro ekutengesa-anodzorwa

Izvo zvinhu zvinoda kushanda mufekitori yako, kwete murabhoritari yemutengesi chete.

Mutengesi anogadzirisa dambudziko rega rega nekushandura chiyero cheA: B

Tembiricha, viscosity, kukurumidza kuporesa, uye kupinda kunofanirwa kudzorwa kuburikidza nekugadzirisa kwakakodzera uye mamiriro ekugadzirisa-kwete kushanduka kwechiyero.

Hapana anogona kutsanangura muenzaniso wakakundikana

Tsigiro yehunyanzvi inonyanya kukosha kana chimwe chinhu chisina kumira zvakanaka.

Mutengesi anokwanisa anofanira kubatsira kusiyanisa kutadza kwechigadzirwa kubva kune isiriyo reshiyo, tembiricha, kusvibiswa, kukanganisa kwekushandisa, kana dombo risina kukodzera.

Maitiro ekufananidza Vaviri Epoxy Suppliers Zvakanaka

Usaedze Mutengesi A pane imwe slab mangwanani uye Mutengesi B pane rimwe dombo rakasiyana mazuva matatu gare gare.

Shandisa masamples ematombo anoenderana

Kana zvichiita, cheka zvienzaniso kubva kune imwechete slab kana zvinhu zvakanyatsoenderana.

Kudzora tembiricha

Chengetedza resin, kuomesa, uye dombo munzvimbo imwechete yekuyedza.

Shandisa chiyero chakakodzera chechigadzirwa chimwe nechimwe

Kuenzanisa kwakaringana hakurevi kumanikidza zvigadzirwa zvese kushandisa chiyero chakafanana chekusanganisa.

Chigadzirwa chega chega chinofanira kugadzirirwa zvinoenderana nekwacho.

Shandisa zvinangwa zvekushandisa zvakaenzana

Kana bvunzo iri kupinda, enzanisa kupinda.

Kana bvunzo iri mesh kutsigira, enzanisa mesh kuita.

Usaite chinzvimbo chekupinda epoxy pakatarisana nemusono-inozadza resin uchishandisa imwe generic mamakisi.

Vaka Muedzo weOdha pakati peSample uye Yakazara Yakazara Kutenga

Kune zvine musoro maodha emaindasitiri, panowanzo batsira nhanho yepakati pakati pediki yemahara sampu uye yekutenga-chikero chekutenga.

Danho iroro ndiro danho rekutongwa.

Sei mutemo wekutongwa uchikosha

Inobatsira mutengi kuongorora:

  • kutengesa kurongedza;
  • batch consistency;
  • kubata warehouse;
  • opareta kudzidza curve;
  • production throughput;
  • chaiyo resin kushandiswa;
  • kusiyanisa kwemhando kune mamwe slabs; uye
  • mutengesi logistics.

Sample yerabhoritari ye1 kg inogona kuratidza kuenderana.

Haikwanise kuratidza zvizere kuvimbika kwekugadzirwa kwehuwandu.

Kurudziro: Bvumira Maitiro, Kwete Chete Chigadzirwa

Izvo zvakanakisa epoxy qualification zvirongwa hazvibvunze chete kana resin inosangana nehunyanzvi data sheet.

Vanobvunza kana maitiro ese ekugadzira achidzokororwa.

Kana viscosity yakarurama asi vashandi havagoni kupedzisa slab pamberi pegelation, iyo system haina kukodzera.

Kana kunamatira kwakasimba asi marble chena ikagadzira halos inooneka, iyo system haina kukodzera dombo iroro.

Kana resin ichiita zvakakwana muzhizha asi ichimisa mutsara munguva yechando, maitiro egore rose haana kukodzera.

Kana iyo epoxy yakachipa ichida zvinhu zvakawanda pa square mita, enzanisa yakapera-slab mutengo pane kutenga mutengo.

Kana sampuli imwe ikashanda asi mabheji ekutengesa achisiyana, ongorora kuenderana kwemupi usati wazvipira kuvhoriyamu.

Uye kana epoxy ikapfuura bvunzo dzemurabhoritari asi ikatadza panguva yekupenya chaiko, vimba neslab rakapera.

Mutengi wako anotenga dombo rakapedzwa-kwete epoxy data sheet.

Mibvunzo Inowanzo Kubvunzwa Nezve Kuyedza Epoxy Pamberi Kwekuodha Kwakawanda

1. Chii chinofanira kuedza fekitari yematombo isati yatenga epoxy resin muhuwandu?

Fekitori yematombo inofanirwa kuongorora zvinyorwa, kusanganisa maitiro, viscosity, nguva yekushanda, kurapa, kupinda, kunamatira, kugadzikana kwemavara, kupenya kuita, kushandiswa kweresin, kuita kwemwaka tembiricha, uye batch kuenderana. Miedzo inofanirwa kushandisa iro chairo rekugadzira dombo uye maitiro pese pazvinogoneka.

2. TDS yemupi inokwana here kubvumidza epoxy?

Kwete. A TDS yakakosha pakunzwisisa magadzirirwo uye mamiriro ebvunzo, asi haigoni kufanotaura zvizere kushanda kwemarble, granite, onyx, kana dombo rakagadzirwa. Shandisa tekinoroji data kupfupisa chigadzirwa, wobva wasimbisa mashandiro kuburikidza nemiedzo inodzorwa fekitori.

3. Mangani ematombo ematombo anofanirwa kuongororwa pamberi pekuraira kwakawanda?

Hapana nhamba yepasi rose. Imwe slab kazhinji haina kukwana nekuti dombo rechisikigo rinosiyana. Edza akawanda anomiririra slabs anovhara zvakajairika misiyano muporosity, makatsemuka, ruvara uye chimiro. Iyo yakakwira mutengo wekukundikana kana kuti yakakura kurongeka kwakarongwa, ndiko kuwedzera kwakasimba kwechirongwa chekufanirwa.

4. Ndeipi inonyanya kukosha epoxy test yekugadzira matombo?

Iko hakuna bvunzo imwechete yakakosha kune yega application. Pakugadzirisa kutsemuka kwegranite, kupinda kunogona kuve kwakakosha. Kune chena marble, kugadzikana kwemavara uye kudzorwa kupinda kunogona kutonga. Kune mesh kutsigira, kunyorova uye kubata kurapa nyaya. Kune vacuum infusion, viscosity kugadzikana uye nguva yekushanda yakakosha. Edza maererano nenjodzi chaiyo yekugadzira.

5. Fekitori inofanirwa kuisa odha yekuyedza isati yatenga yakazara yakawanda epoxy?

Kune mavhoriyamu ane revo maindasitiri, odha yekuyedza kazhinji inhanho yakangwara yepakati. Inobvumira fekitori kuti iongorore mabheti ekutengesa, kurongedza, kuenderana kwevashandisi, mashandisiro chaiwo, kubuda kwekugadzira, maitiro emwaka, uye kuvimbika kwemupi asati azvipira kutenga hombe.

Maitiro ekushandura epoxy sampuli kuita yakavimbika Kutenga Sarudzo

Iyo yakanaka epoxy sampuli bvunzo inofanirwa kuburitsa mamiriro anoona kubudirira mufekitori yako. Data yetekinoroji ndiyo yekutanga, asi sarudzo yekupedzisira inofanirwa kunge yakavakirwa padombo chairo, tembiricha chaiyo, nguva dzekushandisa chaidzo, maitiro ekupedzisa, uye mitengo inoyerwa yekugadzira. Chinangwa hachisi chekuwana resin inoshanda kamwe chete - ndeyekukodzera nzira inodzokororwa iyo inogona kuyerwa zvakachengeteka mukugadzirwa kwekutengesa.

Edza zvinoenderana nenjodzi yekushandisa

Granite micro-crack kugadzirisa:
koshesa kudzika kwekupinda, nguva yekushanda, kurapa, uye kupukuta mhedzisiro.

White marble
koshesa kutsvuka, kusvibisa, kupenya, kutonga kwekupinda, uye chitarisiko chekupedzisira chakakwenenzverwa.

Mesh kutsigira:
koshesa kunyorova kwefiber, kunamatira kwematombo, nguva yekushanda, kubata kurapwa, uye nemwaka tembiricha kuita.

Vacuum infusion:
koshesa kudzikama kwakadzika-viscosity, hwindo rekupinza, mabhubhu, kunzwa kunodonha, kupinda, uye kushandiswa kweresin.

Seam uye cavity kuzadza:
koshesa kuyerera kwekutonga, kugadzikana kwedimensional, kuchengetedza kwepamusoro, maitiro ekupukuta, uye mutambo wekuona.

Usabvumira sampuli isina nhamba

"Zvinotaridzika zvakanaka" zvakaoma kubereka. Rekodha nhamba dzeresin uye dzakaoma batch, A: B chiyero, tembiricha, saizi yebatch, nguva yekushanda, nguva yekurapa, kushandiswa kweresin, kucherechedzwa kwekuramba, uye mhedzisiro yekupukuta. Kunyangwe muyedzo wefekitori wakapfava unova unobatsira zvakanyanya kana mumwe mushandisi achigona kudzokorora achishandisa mamiriro akafanana.

Enzanisa kukosha kwehuwandu hwekugadzira, kwete mutengo chete pakirogiramu

Yepamusoro-mutengo epoxy inogona kuve yakachipa mukugadzira kana ichideredza kushandiswa, kurapa kunonoka, kuputsika slabs, kukwenenzverazve, kana kuramba. Zvikasadaro, chigadzirwa chinokatyamadza chehunyanzvi chinogona kunge chichiri chisina kukodzera kutengeserana kana nguva yekutenderera kana zvinodiwa nemushandisi zvisingaenderane nefekitari. Ongorora mutengo pane inogamuchirwa yakapera slab pane yedhiramu mutengo wega.

Chii chinoparadzanisa mutengesi anobatsira kubva kune mutengesi wezvigadzirwa?

Mutengesi anobatsira anofanirwa kubatsira kutsanangura iyo chaiyo resin-hardener system, kutsanangura tekinoroji paramita, tsigiro yekuyedzwa kwemuenzaniso, kuongorora miedzo yakakundikana, kukurudzira kugadziridzwa kwemwaka pazvinenge zvichidikanwa, uye kuchengetedza mabheji ekutengesa anowirirana. Kune vatengi vemaindasitiri, rutsigiro rwehunyanzvi mushure mekukundikana bvunzo inogona kuve yakakosha kupfuura yakakwana yekutengesa sampuli.

Kurumbidza Kunoshanda

Rondedzera njodzi dzekutadza kutanga, wobva wavaka bvunzo yekuyedza yakavatenderedza. Shandisa dombo rako, kuyera maitirwo, poridzisa kana kubata slab chaizvo sezvinodiwa nekugadzirwa, dzokorora muyedzo kune akati wandei zvidimbu zvevamiriri, uye enzanisa yakazara kushandiswa kwezvinhu uye kuramba njodzi. Kana muenzaniso ukapfuura, enda kune inodzorwa yekuyedza odha usati wazvipira kutenga hombe yakawanda. Iyo yakachengeteka epoxy kutenga haina kubva pane yakanakisa bhurocha-inobva pane inodzokororwa fekitori mhedzisiro.

Wagadzirira Kuedza Epoxy paDombo Rako Pachako Usati Waodha Kwakawanda?

Govera dombo rako rudzi, hurema, tembiricha yemusangano, dambudziko razvino epoxy, nzira yekushandisa, uye inodiwa kutenderera kwekugadzira. Muedzo wefekitari uchishandisa slabs anomiririra anogona kubatsira kuongorora kupinda, kurapa, kugadzikana kwemavara, kupenya, kushandiswa, uye kuenderana kwemaitiro kusati kwatenga kukuru.


Kumbira Epoxy Sample

References

  1. International Organisation for Standardization.
    TS ISO 2555: 2018 Plastics - Resins muLiquid State kana seEmulsions kana Dispersions - Sarudzo yeInooneka Viscosity Uchishandisa Imwe Silinda Type Inotenderera Viscometer Method.
    ISO/TC 61.
    International Organisation for Standardization.
  2. ASTM International.
    ASTM D2196-20 (2026) - Standard Test Methods for Rheological Properties of Non-Newtonian Materials by Rotational Viscometer.
    Komiti yeASTM D01.
    ASTM International, 2026.
  3. International Organisation for Standardization.
    TS EN ISO 11357-5: 2025 Plastiki - Yakasiyana yekuongorora Calorimetry Chikamu 5: Kutemwa kwehunhu hwekuita-Curve Tembiricha uye Nguva, Enthalpy yeReaction uye Dhigirii reShanduro.
    ISO/TC 61/SC 5.
    International Organization for Standardization, 2025.
  4. International Organisation for Standardization.
    TS EN ISO 868:2003 Plastiki uye Ebonite - Kutemerwa kweIndentation Kuoma nenzira yeDurometer.
    ISO/TC 61.
    International Organisation for Standardization.
  5. International Organisation for Standardization.
    ISO 4587: 2003 - Adhesives - Sarudzo yeTensile Lap-Shear Simba reRigid-ku-Rigid Bonded Assemblies.
    ISO/TC 61/SC 11.
    International Organisation for Standardization.
  6. ASTM International.
    ASTM C882/C882M-23 - Standard Test Method yeBond Simba reEpoxy-Resin Systems Inoshandiswa NeConcrete neSlant Shear.
    Komiti yeASTM C09.
    ASTM International.
  7. WEST SYSTEM Technical Staff.
    WEST SYSTEM User Manual & Chigadzirwa Guide.
    Nhoroondo ye Gougeon Brothers, Inc.
    WEST SYSTEM Technical Publications.
  8. Charles Selwitz.
    Epoxy Resins muKuchengetedza Matombo.