Chidule Chachangu:

Kupewa chikasu cha epoxy pa nsangalabwi yoyera kumafuna chemistry yokhazikika komanso kulowerera koyendetsedwa bwino. UV, kutentha, kusakanizikana kolakwika, kuyamwa kwa utomoni wochuluka, ndi zosayenera zochiritsira zimatha kukhudza mawonekedwe omaliza. Mwala wonyezimira wonyezimira nthawi zambiri umafunika epoxy yotsika kwambiri yachikasu yolowera, pomwe mwala wofewa umafunika kuwongolera kopanda banga komanso chizindikiro chamadzi. Yesani nthawi zonse makina owumitsa utomoni pa nsangalabwi weniweni mutachiritsa ndi kupukuta musanapange zochuluka.

Mwala woyera ndi chimodzi mwa zipangizo zosakhululukidwa kwambiri pokonza miyala.Kukonza komwe kumawoneka kovomerezeka kwathunthu pa granite yakuda kungakhale koonekeratu pa Carrara, Calacatta, Statuario, kapena marble wina wowala. Kamvekedwe kakang'ono ka amber mu utomoni, kuwala koderapo mozungulira mng'alu, kulowa kwambiri pafupi ndi m'mphepete, kapena chigamba chomwe chimawonekera pambuyo popukutidwa chingasinthe kamvekedwe kake kamvekedwe kakanthu kokana malonda. Ichi ndichifukwa chake "Kodi epoxy yellow?" ndi chiyambi chabe cha kukambirana.

Katswiri wa fakitale yamwala ayeneranso kufunsa ngati epoxy imasintha kuwala kwa nsangalabwi, kupanga mthunzi wowoneka wonyowa pozungulira pokonza, kulowa mozama kwambiri mumwala wofewa, kupanga utoto pakatentha, imakhalabe yowoneka bwino pambuyo pa kuwonekera kwa UV, ndi kutulutsa mawonekedwe omwewo pambuyo popukuta monga momwe idakhalira pakuyesa koyamba.

Veropoxy pakadali pano imalekanitsa zofunikira izi mkati mwake White Marble Solution. Mtunduwu umaphatikizapo njira yachikasu yotsika kwambiri yopangidwira mwala wonyezimira woyera komanso njira yosiyana yosadetsa yomwe imapangidwa mozungulira kulowa mkati moyendetsedwa ndi kuchepetsa chizindikiro chamadzi kuti muchepetse mwala woyera wofewa.

Kusiyanitsa kumeneko n'kofunika chifukwa kupewa chikasu si vuto lofanana ndi kupewa kudetsa.

Wogwira ntchito akuyang'ana mwala woyera pambuyo pa chithandizo cha epoxy kuti mtundu ukhale wokhazikika komanso wapamwamba

Chifukwa Chake Mwala Woyera Umapangitsa Mavuto Amtundu wa Epoxy Kuwonekera Kwambiri

Mwala woyera umagwira ntchito ngati maziko a utomoni womwe umayikidwapo. Kusiyana kwakung'ono kwamitundu komwe kungathe kutha mkati mwa granite yakuda kumatha kuoneka mosavuta poyang'ana pamwamba, kuwala kapena mitsempha yopepuka.

Kulekerera kochepa kosiyana

Nsalu zoyera sizilola kulekerera madera amber, bulauni, imvi, kapena mdima.

Epoxy siyenera kukhala yachikasu kwambiri wogula asanazindikire kusiyana. Kusintha kwakung'ono kungakhale kokwanira kupanga mzere wowoneka mozungulira ming'alu, msoko, pore yodzaza, kapena m'mphepete mwake.

Izi ndizofunikira makamaka pamapangidwe apamwamba kwambiri pomwe malo akulu opukutidwa aziwoneka pansi pa kuyatsa kowala mkati.

Translucency ikhoza kukulitsa kusiyana kolowera

Miyala yoyera yambiri imakhala ndi kusinthasintha kwina. Utoto ukalowa mumwalawu, umasintha momwe kuwala kumayendera m'malo oyeretsedwa.

Izi zitha kupanga mawonekedwe akuda kapena "onyowa" ngakhale utomoni womwewo sunakhale wachikasu.

Pazifukwa izi, ogula sayenera kungozindikira kuti chizindikiro chilichonse chakuda chili ngati epoxy yellowing.

Porosity imasiyanasiyana pakati pa mitundu ya nsangalabwi

Miyala yoyera ina ndi yokhuthala komanso yonyezimira. Zina ndi zofewa, zokhala ndi porous, kapena zimakhala ndi zing'onozing'ono zotseguka.

Epoxy yotsika kwambiri yomwe imagwira ntchito bwino pamwala wolimba imatha kulowa patali kwambiri mu slab yoyamwa kwambiri, kutulutsa mthunzi wowoneka pozungulira kukonza.

Ichi ndi chifukwa chimodzi kuti utomoni womwewo suyenera kugwiritsidwa ntchito pamtundu uliwonse wa nsangalabwi woyera.

Kodi Epoxy Yellowing ndi chiyani?

Epoxy yellowing yeniyeni ndi kusintha kwa mtundu wa mankhwala mkati mwa polima dongosolo lokha.

Mu ukalamba, kuwonekera kwa UV, kutentha kwakukulu, kuwonetsa mpweya, kapena kupsinjika kwina kwachilengedwe, kusintha kwamankhwala kumatha kuchitika mu polima wochiritsidwa. Kafukufuku wokhudzana ndi kuwonongeka kwa epoxy wagwirizanitsa chikasu ndi machitidwe a okosijeni ndi mapangidwe a ma chromophoric omwe amamwa kuwala kowoneka mosiyana ndi utomoni woyambirira.

Zotsatira zake zimakhala zochiritsidwa zomwe zimasintha pang'onopang'ono kuchoka pakuwoneka bwino kapena pafupifupi zopanda mtundu kukhala zachikasu, amber, kapena bulauni.

Izi zitha kukhala zowononga kwambiri pamiyala yoyera chifukwa utomoni ukhoza kuwoneka mkati mwa ming'alu, pores, seams, kapena madera opakidwa pamwamba.

Yellow ikhoza kuchitika panthawi yokonza kapena pambuyo pake muutumiki

Kusintha kwina kwamtundu kumawonekera mukangosakaniza kapena kuchiritsa.

Ena amakula pambuyo pa kutentha, kuwala, mpweya, chinyezi, kapena ntchito yotalikirapo.

Kwa fakitale yamwala, izi zikutanthauza kuti kuyesa kwachitsanzo kwa mphindi 30 sikokwanira kuyesa kukhazikika kwa mtundu.

"Zosawoneka zachikasu" siziyenera kutanthauziridwa kuti ziro zikusintha mpaka kalekale

Mayina amalonda nthawi zambiri amagwiritsa ntchito mawu monga osawoneka achikasu, okhazikika a UV, kapena otsika kwambiri achikasu.

Kuchokera pamalingaliro ogula mwaukadaulo, mawuwa akuyenera kumveka ngati kukana kusintha kwamtundu pansi pamikhalidwe yofotokozedwa m'malo motsimikizira kuti polima sangakalamba.

Funso labwino ndilakuti:

Kodi kusintha kwamitundu kumapezeka bwanji pa kutentha, kuyatsa, makulidwe, ndi nthawi yowonekera mogwirizana ndi polojekiti yomwe mukufuna?

Wogula katundu: Kuti mupeze miyala yamtengo wapatali yoyera, funsani deta yolimbana ndi chikasu kapena zoyezetsa ukalamba m'malo mongodalira mawu oti "zomveka." Utoto ukhoza kuwoneka wowonekera tsiku loyamba ndipo ungakhale wosayenera kugwiritsa ntchito tcheru kwambiri mtundu.

Chikasu, Kudetsa ndi Zizindikiro za Madzi Si Vuto Limodzi

Makina opangira miyala ya miyala yoyera nthawi zambiri amagwiritsa ntchito mawu oti "chikasu" pofotokoza zolakwika zingapo zowoneka bwino. Kuzindikira kolondola ndikofunikira chifukwa yankho limasintha malinga ndi zomwe zimayambitsa.

Vuto Lowoneka Mwina Mechanism Maonekedwe Odziwika Zomwe Muyenera Kuzifufuza Choyamba
Epoxy yellowing weniweni Kusintha kwa polima panthawi ya chithandizo kapena ukalamba Chotsani utomoni pang'onopang'ono umakhala wachikasu kapena amber Chemistry ya resin / hardener, kuwonekera kwa UV, kutentha ndi kukalamba
Kudetsa Kuwonongeka kapena kuyanjana kwa mankhwala pafupi ndi miyala Chizindikiro chamtundu chozungulira malo ochitiridwa Ukhondo pamwamba, kugwilizana ndi utomoni ndi zoipitsa
Kujambula Kulowa kwa utomoni kumasintha mawonekedwe a nsangalabwi Malo amdima kapena onyowa pozungulira ming'alu kapena pores Kuzama kolowera, mamasukidwe akayendedwe ndi porosity mwala
Chizindikiro chamadzi Mayamwidwe osagwirizana kapena kusintha kwa kuwala mozungulira porous zones Mtundu wowoneka ngati halo kapena wosakhazikika wakuda Marble absorbency ndi kuwongolera kulowa
Zotsalira pamwamba Utoto wochuluka umatsalira pankhope ya nsangalabwi Gloss, filimu ya amber kapena chigamba chosagwirizana pambuyo pochiritsidwa Kuchuluka kwa ntchito, kukwapula ndi kumaliza
Kusintha mtundu Kutentha, kuipitsidwa, chinyezi kapena kuchiritsa kolakwika Mitundu yosiyana pambuyo pokonza fakitale Kutentha, chiŵerengero chosakanikirana, zida ndi machiritso

Kusiyanitsa kumeneku n'kofunika kwambiri kwa nsangalabwi yofewa yoyera.

Epoxy yomveka bwino imatha kupangabe halo yamdima yosavomerezeka ngati ilowa mozama kwambiri. Zikatero, kugula utomoni wowoneka bwino sikuthetsa vuto lenileni. Fakitale imafunikira kuwongolera bwino kwa malowedwe.

Nchiyani Chimachititsa Epoxy Kukhala Yellow pa White Marble?

Kuwonekera kwa UV ndi Photo-oxidation

Ma radiation a ultraviolet ndi chimodzi mwazinthu zodziwika bwino za ukalamba zomwe zimakhudzidwa ndi zinthu za epoxy.

Kafukufuku wa epoxy pansi pa kuwonekera kwa UV awonetsa kuzama kwa mtundu, kuwonongeka kwa pamwamba, ndi kusintha kwamankhwala komwe kumakhudzana ndi kutsekemera kwa zithunzi.

Zotsatira zake zimakhala zamphamvu kwambiri pafupi ndi malo owonekera chifukwa mphamvu ya UV simalowa m'gawo lakuya la polima.

Pakukonza miyala, izi ndizofunikira kwambiri ngati epoxy ikhalabe pafupi ndi malo owoneka bwino a nsangalabwi kapena pomwe kuyika komalizidwa kulandila kuwonetseredwa kwachilengedwe kapena kochita kupanga kwa UV.

Kutentha ndi matenthedwe oxidation

Kutentha kokwera kumatha kufulumizitsa machitidwe amankhwala okhudzana ndi ukalamba wa polima.

Utoto womwe umakhalabe wovomerezeka m'nyumba zocheperako ukhoza kuchita mosiyana ukakhala ndi kutentha kwambiri, mizere yopangira kutentha, kuwala kwadzuwa, kapena malo ochitiramo kutentha kwambiri.

Ichi ndichifukwa chake kukana kwachikasu kuyenera kuyesedwa pamodzi ndi kutentha kwa fakitale.

Matenda a Veropoxy Epoxy Resin Yokonza Marble & Kukulitsa Mtundu, mwachitsanzo, imayikidwa pafupifupi 28-38 ° C yokonza marble ndipo imatchula kukana kwachikasu kwambiri monga mbali ya zofunikira zopangira.

Resin ndi harder chemistry

The epoxy resin palokha ndi gawo limodzi la dongosolo.

Chowumitsa chimatha kukhudza kwambiri mtundu woyamba, kuchiritsa, kukana kwa okosijeni, komanso mawonekedwe anthawi yayitali.

Ichi ndichifukwa chake ogula ayenera kuwunika mawonekedwe a A+B athunthu m'malo mofanizira kumveka kwa gawo la utomoni kwinaku akunyalanyaza wochiritsa.

Utoto wowoneka bwino bwino wosakanikirana ndi chowumitsa chamitundu yamphamvu kapena wosafanana bwino sutulutsa mawonekedwe osalowerera ndale.

Kusakaniza kolakwika

Kusintha chiŵerengero chotchulidwa kungakhudze khalidwe la machiritso ndikusiya dongosolo losalinganika.

Izi zitha kubweretsa kuchira kosakwanira, kulimba mtima, kuuma kosagwirizana, kapena mawonekedwe osagwirizana ndi mawonekedwe.

Kuwonjezera owumitsa owonjezera "kupanga epoxy kuchiritsa mofulumira" Choncho ndi njira osauka kulamulira liwiro kupanga, makamaka ntchito ndi umafunika woyera nsangalabwi.

Kutentha kwambiri panthawi ya chithandizo

Magulu akuluakulu osakanikirana amatha kutenthetsa kwambiri kuposa zoonda.

Utoto ukakhala wotentha kwambiri m'chidebe kapena malo okonzera, kuphatikiza kutentha kwambiri ndi kufulumira kwachangu kumatha kusintha machitidwe ndikuwonjezera chiwopsezo cha kusinthika.

Choncho mafakitale ayenera kutsata kukula kwa batch, njira yosakaniza, ndi kutentha kusiyana ndi kuganiza kuti epoxy imachita mofanana pa voliyumu iliyonse.

Kukalamba kwanthawi yayitali

Utomoni ukhoza kuwoneka ngati wopanda madzi ndipo umasintha pakapita nthawi.

Ichi ndichifukwa chake maphunziro ofulumizitsa okalamba amakhala othandiza pamene kuyera kwamaso ndikofunikira. Kafukufuku wofalitsidwa pamwala wopangidwa ndi epoxy wasonyeza kuti kusintha kwa maonekedwe, kuphatikizapo chikasu kapena mdima, kungakhale chinthu cholepheretsa posankha consolidants kapena zipangizo zokonzera.

Chifukwa Chake Kulowa Kwambiri Kutha Kuwoneka Ngati Chikasu

Pa nsangalabwi yoyera, utomoni suyenera kukhala wachikasu kuti upangitse chilema chowoneka.

Madzi owoneka bwino akalowa mu porous, amatha kusintha mawonekedwe amwala. Dera lothandizidwa likhoza kukhala lakuda, lodzaza, kapena lowala kwambiri.

Kusintha kwa kuwalako kumatha kukhalabe pambuyo pochiritsidwa.

Mwala wonyezimira woyera ndi mwala wofewa woyera umachita mosiyana

Mwala wonyezimira wonyezimira wonyezimira ukhoza kulolera njira yolunjika yolowera chifukwa utomoniwo umatsatira ming'alu yabwino komanso kusakhazikika kwadongosolo.

Mwala wofewa kapena wopindika kwambiri umatha kuyamwa utomoni m'dera lalikulu.

Chotsatiracho chikhoza kukhala halo yakuda yomwe imawoneka yofanana ndi chizindikiro cha madzi.

Matenda a Veropoxy Epoxy Wopanda Madontho a White Marble imathana ndi vuto lenilenili kudzera m'malowedwe oyendetsedwa m'malo mongodalira kuwonekera kwa utomoni. Zomwe zasindikizidwa pano zimatchula kukhuthala kwa 400-600 CPS, pafupifupi kuchiritsa kwa mphindi 80, kutsika kwachikasu kwambiri, ndi kutentha koyenera kugwira ntchito mozungulira 24°C.

Kulowa kochulukira sikuliko bwino

Kulowa mozama kumakhala kofunikira ngati cholinga chake ndikulimbitsa mamangidwe.

Koma pamene chofunika cha maso chili kukonzanso kosaoneka pa mwala wonyezimira wonyezimira, kuloŵa kosalamulirika kungakhale chilema.

Ichi ndichifukwa chake njira ya "viscosity yotsika kwambiri" siyimagwira ntchito pamwala woyera.

Momwe Mungasankhire Epoxy ya Marble Yoyera Yolimba

Mwala wonyezimira wa nsangalabwi nthawi zambiri umakhala wokhuthala kuposa mitundu yofewa komanso yoyamwa kwambiri.

Epoxy ikufunikabe kulowa mokwanira kuti ilimbikitse ming'alu yaying'ono, koma cholinga chogulira chiyenera kukhalabe chokhazikika pakukhazikika kwamtundu.

Clear epoxy resin jekeseni mu mng'alu wa nsangalabwi woyera kuti aziwongolera ndi kulowa

Ikani patsogolo chikasu chochepa kwambiri

Kwa ma slabs oyera apamwamba kwambiri, kukhazikika kowonekera kuyenera kuwonedwa ngati gawo lalikulu m'malo motsatsa malonda.

Matenda a Veropoxy Epoxy Yosakhala Yachikasu ya Marble Yoyera Yoyera - 5090 / D30M-BS imayikidwa mozungulira chofunikira ichi.

Mndandanda wazinthu zamakono:

  • nsangalabwi yoyera yolimba ngati gawo lapansi lachindunji;
  • chikasu chochepa kwambiri;
  • kulowa molamulidwa;
  • 100:30 resin-to-hardener chiŵerengero;
  • pafupifupi mphindi 80 kuchira;
  • pafupifupi 24°C analimbikitsa kutentha ntchito; ndi
  • 400-600 CPS kukhuthala.

Ziwerengerozi ziyenera kutengedwa ngati dongosolo, osati ngati malo ogulitsa okha.

Wogula ayenera kutsimikizira ngati kuphatikiza kumapereka malowedwe okwanira pa slab yeniyeni ndikusunga mawonekedwe ofunikira atachiritsidwa ndi kupukuta.

Momwe Mungasankhire Epoxy ya Marble Yofewa kapena Yamabowo

Kwa nsangalabwi yofewa yoyera, mbiri yachiwopsezo imasintha.

Wogula amafunikirabe kukana bwino kwa chikasu, koma kuwongolera kulowa kumakhala kofunikanso.

Ikani patsogolo khalidwe losadetsa

Ngati utomoni ufalikira kupyola ming'aluyo kapena pobole, mthunzi wa kuwala ukhoza kuwoneka bwino kuposa chilema choyambirira.

Pazimenezi, kachitidwe kamene kamapangidwira mozungulira kulowetsedwa koyendetsedwa ndi koyenera kuposa kungosankha utomoni wa thinnest womwe ulipo.

Yesani m'mphepete mwamdima

Ikani utomoni ku ming'alu yoyimilira ndi ma porous zones, kenako yang'anani malire ozungulira malo ochiritsidwa.

Ngati mdima wandiweyani utulukira kunja kwa malo omwe mukufuna kukonza, chepetsani kulowa kapena sinthani mapangidwe musanawonjezere kupanga.

Yang'anani mutatha kupukuta

Silab yonyowa kapena yochiritsidwa mwatsopano imatha kubisala kusiyana kowoneka.

Mayeso enieni ovomerezeka amayenera kubwera pambuyo pa kupukuta kwabwinobwino chifukwa kupukuta kumasintha gloss, mawonekedwe a pamwamba, ndi mawonekedwe a madera okonzedwa.

Marble Yoyera Yoyera vs Marble Yofewa Yoyera: Table Decision Table

Chosankha Mwala Woyera Wolimba Mwala Wofewa / Wowonjezera Kwambiri
Chiwopsezo chachikulu chowonera Mizere yowoneka yachikasu komanso yowoneka Kuthimbirira, mthunzi, zizindikiro za madzi ndi kulowa kwambiri
Choyamba utomoni patsogolo Otsika kwambiri achikasu kuphatikiza kulowa mkati mowongolera Khalidwe losadetsa komanso kuyamwa molamulidwa
Viscosity strategy Kuthamanga kokwanira kulowa m'ming'alu yaying'ono Pewani kulowa mopitirira muyeso kupitirira malo okonzera
Chitsanzo choyang'ana Kusintha kwa mtundu pambuyo pochiritsidwa ndi kukalamba Mapangidwe a halo ndi m'lifupi mwake
Kumaliza cheke Kukonza mawonekedwe pambuyo kupukuta Mphepete mwamdima, malo owoneka ngati mvula komanso kuwala kosafanana
Chitsanzo cha Veropoxy 5090 / D30M-BS Non-Staining / D30M-BS

Momwe Kuwonekera kwa UV Kumasintha Kusankhidwa kwa Epoxy

Mwala wamkati ndi mwala wakunja samakumana ndi malo okalamba omwewo.

Mkati mwa marble woyera

Ntchito zamkati zitha kulandira UV wocheperako, koma izi sizimachotsa kufunikira kokhazikika kwamtundu.

Mawindo akulu, ma skylights, zowunikira zowonetsera, komanso nthawi yayitali yogwirira ntchito zitha kupangitsa kuti utomoni wosawoneka bwino uwonekere.

Malo ochezera apamwamba, mahotela, nyumba zapamwamba zamkati, malo ogulitsa, ndi mipando yanyumba zingakhale zovuta kwambiri chifukwa ogula amayendera pafupi.

Kuwonekera kwakunja kapena kowala kwambiri

Kwa ntchito zakunja kapena zowunikira mwamphamvu, kukana kwa UV kumakhala kofunika kwambiri.

Zipangizo zamtundu wa epoxy sizimangofanana ndi zokutira zowoneka bwino zakunja zomwe zimapangidwa mozungulira nthawi yayitali ya UV.

Ngati epoxy yowonekera ikhalabe yowonekera pamtunda, ogula ayenera kutsimikizira ngati dongosolo losankhidwa lili ndi ukalamba wokhudzana ndi chilengedwe chomwe chikuyembekezeka.

Pazinthu zowonekera bwino zomangirira kunja kwa njira yolimbikitsira marble, Veropoxy imalembanso UV Stable Crystal Clear Epoxy Mastic mkati mwa zinthu zake zambiri. Zogulitsa zimafunikirabe kugwirizana ndi zomwe zimafunikira pakukonza miyala m'malo mosankhidwa potengera liwu loti "UV" lokha.

Momwe Kutentha Kumakhudzira White Marble Mtundu Kukhazikika

Kutentha kumakhudza ma kinetics ochiritsira komanso chiopsezo cha kusagwirizana kowonekera.

Ngati epoxy yomweyi ikugwiritsidwa ntchito mu msonkhano wa 15 ° C mwezi umodzi ndi 35 ° C mu nyengo ina, kuyenda, nthawi yogwira ntchito, kuzama kolowera, ndi kuchiritsa kungasinthe.

Kusintha kumeneku kungakhudze maonekedwe ngakhale pamene chemistry yokha siinakhale yachikasu kwambiri.

Kutentha kwakukulu kumatha kusintha kulowa

Epoxy yotentha nthawi zambiri imayenda mosavuta.

Pa nsangalabwi yoyera yoyera, izi zimatha kukulitsa kuyamwa ndikukulitsa malo owoneka bwino.

Kutentha kwakukulu kumafupikitsa zenera logwira ntchito

Kuchita mwachangu kungachepetse nthawi yomwe ogwiritsira ntchito amayenera kuchotsa utomoni wochulukirapo kapena kuyeza pamwamba mosalekeza.

Zotsalira zosagwirizana zimatha kupanga kusiyana kowoneka pambuyo pa kupukuta.

Zozizira zimatha kupanga zolakwika zawo

Kukatentha, utomoni umakhala wokhuthala ndipo sungathe kulowa m'ming'alu yabwino.

Chotsatiracho chikhoza kukhala kulimbikitsana kosakwanira kapena kudzaza koonekeratu pamwamba m'malo mwa kukonza mkati mwaukhondo.

Pazifukwa izi, kutentha kuyenera kujambulidwa panthawi iliyonse yoyeserera zoyenereza za marble.

Momwe Mungayesere Epoxy Yotsika Yachikasu Musanayambe Kupanga Zambiri

Deta ya ogulitsa ndiyothandiza, koma nsangalabwi yoyera iyenera kukhala yoyenerera pamwala wa wogula.

Kupaka utomoni wonyezimira wachikasu wa epoxy mofanana pamwala wa nsangalabwi woyera pafakitale yamwala

Gawo 1: Sankhani masilabu oyimira

Osayesa pazatsanzo zoyera kwambiri komanso zonenepa kwambiri.

Phatikizanipo kusiyanasiyana kofananira:

  • ma slabs wandiweyani;
  • ma slabs ochulukirapo;
  • ma slabs okhala ndi ming'alu yabwino;
  • ma slabs okhala ndi pores otseguka;
  • madera oyera owala; ndi
  • madera amitsempha kwambiri.

Khwerero 2: Lembani mtundu wa mwala woyambirira

Jambulani slab pansi pa kuyatsa koyendetsedwa musanagwiritse ntchito.

Pakupanga kofunikira kwambiri, gwiritsani ntchito colorimeter ndikujambulitsa L*, a*, ndi b* pamalo omwe afotokozedwa.

Kuyeza kosasinthasintha kumapangitsa kuti zikhale zosavuta kusiyanitsa kusintha kwamtundu weniweni kuchokera ku kusiyana kwa kujambula kapena kuyatsa.

Khwerero 3: Sakanizani ndendende molingana ndi zomwe mukufuna

Gwiritsani ntchito chiŵerengero cha A: B.

Osasintha kuchuluka kwa zowumitsa kuti muwongolere kuthamanga kwa machiritso kapena kukhuthala.

Lembani:

  • nambala ya batch ya utomoni;
  • nambala ya batch ya harder;
  • chiŵerengero cha kusakaniza;
  • kutentha kozungulira;
  • kutentha kwamwala;
  • kukula kwa batch; ndi
  • nthawi yosakaniza.

Gawo 4: Ikani kuchuluka kolamulidwa

Zinthu zochulukirapo zimapanga kufananitsa kosokeretsa.

Gwiritsani ntchito kuchuluka kwa ntchito ndi njira yofananira pa utomoni aliyense.

Gawo 5: Onani malire olowera

Kuchiza kusanathe, onani kutalika kwa utomoniwo kupyola ming'alu kapena malo opangira mankhwala.

Pa nsangalabwi yofewa, kulowa kwambiri ndi chizindikiro chochenjeza.

Gawo 6: Lolani kuchiza kwathunthu

Osaweruza utomoni mwamsanga pambuyo ntchito.

Mtundu wa epoxy wosakanikirana watsopano ukhoza kusiyana ndi kuchiritsidwa komaliza.

Khwerero 7: Pulitsani slab

Yendetsani mayeso a slab kudzera munjira yoyakira yomwe imagwiritsidwa ntchito popanga.

Kenako yerekezerani:

  • Kuwala kwathunthu;
  • mawonekedwe a khungu;
  • mdima wakuda;
  • kamvekedwe kachikasu;
  • zotsalira pamwamba;
  • kusiyana kwa gloss; ndi
  • kukonza malire.

Khwerero 8: Chitani zoyezetsa zakukalamba pamene polojekiti ikuwalungamitsa

Pama projekiti apamwamba kwambiri, mapulogalamu otumiza kunja, kapena mapulogalamu omwe ali ndi kuwala kwakukulu, lingalirani za kukalamba kolamuliridwa kapena kuyezetsa kwa UV.

Cholinga sikuneneratu chiwerengero chenicheni cha zaka zautumiki kuchokera ku mayeso afupiafupi a labotale. Ndiko kufananiza makonzedwe osankhidwa pansi pa zochitika zomwezo ndikuzindikira kuti ndi dongosolo liti lomwe limasintha mtundu mwachangu kwambiri.

Mndandanda Wakuyenerera Kwa Marble Epoxy

Chinthu Choyesera Zoyenera Kuzipenda Chifukwa Chake Kuli Kofunika?
Mtundu woyamba wa utomoni Kumveka bwino ndi kamvekedwe ka amber mutatha kusakaniza Mtundu wowoneka wa utomoni ungakhudze mwala woyera nthawi yomweyo
M'lifupi mwake Kutalikirana kuposa ming'alu kapena pore Kulowa mochulukira kungapangitse ma halos akuda
Kuchiritsa mtundu Kuwonekera pambuyo pochiritsidwa kwathunthu Maonekedwe a utomoni wonyowa sangayimire mtundu womaliza
Mawonekedwe opukutidwa Kuwala, kukonzanso mawonekedwe, ndi mthunzi Kuvomereza komaliza kumachitika mukamaliza
Kukhazikika kwa kutentha Kusintha mtundu pansi kwenikweni processing kutentha Zofunikira pamizere yotentha kapena yotenthetsera yopanga
Kuyerekeza kwa UV / ukalamba Wachibale chikasu pambuyo poyang'anira kukhudzana Zothandiza pama projekiti anthawi yayitali osatengera mtundu
Kusasinthasintha kwamagulu Bwerezani zotsatira m'maere angapo Chitsanzo chimodzi changwiro sichitsimikizira kupanga kokhazikika
Kugwirizana kwa miyala Zotsatira zamitundu yeniyeni ya nsangalabwi Miyala yosiyanasiyana imayamwa utomoni mosiyana

Zolakwa Zomwe Zimayambitsa Mavuto Owoneka pa Marble Yoyera

Kusankha epoxy chifukwa chowoneka bwino mumtsuko

Kuwonekera koyamba sikufanana ndi kukana kwachikasu kwa nthawi yayitali.

Wogula akuyenera kuwunika kachitidwe kosakanikirana ndi kochiritsidwa, osati gawo A.

Kugwiritsa ntchito epoxy yemweyo pamwala wolimba komanso wofewa woyera

Izi zitha kugwira ntchito pamiyala ina ndikulephera moyipa pa ena.

Mwala wofewa ungafunike kuwongolera molimba kwambiri.

Kungoganiza kuti mdima uliwonse ndi wachikasu

Halo yotuwa kapena yonyowa pokonzekera nthawi zambiri imakhala vuto la kuyamwa kapena kupenya m'malo mwa chikasu chamankhwala.

Konzani matenda musanasinthe mankhwala.

Kusankha mamasukidwe otsika kwambiri omwe alipo

Low mamachulukidwe akayendedwe kumathandiza micro-ming'alu malowedwe koma akhoza kuwonjezera mthunzi mu kuyamwa kwambiri mwala woyera.

Kunyalanyaza kutentha kwa msonkhano

Kutentha kumasintha mamasukidwe akayendedwe, liwiro lamachitidwe, nthawi yogwira ntchito, ndi machitidwe olowera.

Utoto woyenerera m'nyengo yozizira suyenera kulandiridwa kuti upangidwe kwambiri m'chilimwe popanda kutsimikiziridwa.

Kusiya owonjezera utomoni pamwamba

Zotsalira zam'mwamba zimawoneka bwino kwambiri ndipo zimalandira kuwala kwachindunji kuposa utomoni womwe uli mkati mwa mng'alu.

Lamulirani kukwapula, kusanja, ndi kupukuta m'malo molola kuti filimu ya utomoni yosafunikira ikhalebe.

Kusintha chiŵerengero chosakanikirana

Osayesa kuchepetsa chikasu, kuwonjezera kumveka, kapena kuwongolera liwiro la machiritso posintha chiŵerengero cha A:B chomwe chatchulidwa.

Gwiritsani ntchito mawonekedwe opangidwa kuti agwirizane ndi zofunikira.

Kudumpha kuwunika kwa ukalamba pama projekiti apamwamba

Chitsanzo chomwe chimawoneka bwino pambuyo pa tsiku limodzi sichikhoza kuyimira ntchito yayitali.

Kwa nsangalabwi yoyera yamtengo wapatali, kuyezetsa kuyerekezera kofulumira kumatha kukhala gawo lanzeru pakuyenerera kwa ogulitsa.

Momwe Mungagwirizanitsire Epoxy System ndi Mikhalidwe Yosiyanasiyana ya Marble Yoyera

Mkhalidwe Wopanga Zofunika Kuziika Patsogolo Chifukwa chiyani?
Mwala wandiweyani wolimba Otsika kwambiri achikasu kuphatikiza kulowa mkati molamulidwa Kukhazikika kwamtundu ndikofunikira pomwe ming'alu yabwino imafunikirabe kulimbikitsidwa
Mwala wofewa wonyezimira woyera Kuchita kosadetsa komanso kulowa pang'ono Amachepetsa mithunzi ndi zotsatira za madzi
Silab yopukutidwa kwambiri Zowoneka bwino kwambiri zochiritsidwa komanso zogwirizana ndi kupukuta Zowonongeka zazing'ono zimawonekera pambuyo pomaliza
Malo opangira ofunda Khola kuchiritsa chemistry pa kutentha kwenikweni msonkhano Kutentha kumasintha nthawi yogwira ntchito komanso machitidwe olowera
Ntchito yowonetsedwa ndi UV Ukalamba wotsimikizika komanso kukhazikika kwamtundu UV imathandizira kuwonongeka kwapamwamba pamakina ambiri a epoxy
Mng'alu wakuya wapangidwe Kulowa mokwanira popanda kupangika kwambiri kwa halo Kulimbitsa kwamapangidwe ndi mawonekedwe kuyenera kukhala koyenera
Kudzaza pore pamwamba Kuthamanga koyendetsedwa ndi filimu yotsalira yochepa Amachepetsa maonekedwe a maonekedwe ndi kusiyana kwa gloss

Zomwe Ogula Ayenera Kufunsa Wopereka Epoxy

Kugula kwa nsangalabwi yoyera kuyenera kupitilira "Kodi sikukhala chikasu?"

Funsani:

  • Kodi dongosololi lapangidwira mwala wolimba kapena wofewa woyera?
  • Kodi kukhuthala kosakanikirana ndi chiyani?
  • Kodi kukhuthala kumayezedwa pa kutentha kotani?
  • Kodi resin-to-hardener ratio ndi chiyani?
  • Kodi kutentha kovomerezeka ndi kotani?
  • Kodi nthawi yogwira ntchito ndi nthawi yochiritsa ndi chiyani?
  • Kodi yellowing resistance imawunikidwa bwanji?
  • Kodi dongosololi limayang'anira kulowa kwa miyala ya porous marble?
  • Kodi wogulitsa angapereke zitsanzo zoyesa pamwala wathu?
  • Kodi magwiridwe antchito amagwirizana pakati pa magulu opanga?

Veropoxy ndi zambiri mwala epoxy mankhwala osiyanasiyana amalekanitsa zofunika zosiyanasiyana za nsangalabwi m'malo moyika epoxy wachilengedwe chonse pamwala uliwonse. Ndilo njira yoyenera yogulira akatswiri: kuyambira pavuto la ntchito ndi kapangidwe ka miyala, kenako sankhani dongosolo la utomoni.

Malangizo: Kuwongolera Kukhazikika kwa Mtundu ndi Kulowa Pamodzi

Kupewa zolakwika zowonekera pa nsangalabwi woyera kumafuna maulamuliro awiri osiyana nthawi imodzi.

Choyamba ndi kukhazikika kwa mtundu wa mankhwala.

Epoxy iyenera kugwiritsa ntchito utomoni ndi chemistry yowumitsa yoyenera mwala wosamva mtundu, womwe umatsimikiziridwa kuti ndi wachikasu pang'ono pansi pamikhalidwe yomwe ikukonzedwa ndi ntchito.

Chachiwiri ndi kulamulira kulowa mkati mwa thupi.

Utoto uyenera kulowa m'ming'alu ndi pores mokwanira kuti ukhale wolimba popanda kufalikira mpaka pamwala wamwala kotero kuti umapanga mdima wakuda kapena madera owoneka ngati anyowa.

Ngati nsangalabwi ndi wolimba komanso wandiweyani, njira yolowera yotsika kwambiri yachikasu ingakhale njira yabwinoko.

Ngati nsangalabwi ndi yofewa komanso yoyamwa, yang'anani ntchito yosadetsa ndikulowa mowongolera.

Ngati kuyikako kudzalandira kuwala kwa UV kapena kutentha, musadalire pakumveka koyambirira. Funsani zambiri zokhudzana ndi ukalamba kapena chitani mayeso ofananiza.

Ndipo ngati kukonza kumawoneka kwakuda koma epoxy yokha imakhalabe yomveka bwino, fufuzani zolowera ndi miyala ya miyala musanayimbe mlandu polima chikasu.

Mafunso Ofunsidwa Kawirikawiri Okhudza Epoxy Yellowing pa White Marble

1. Chifukwa chiyani epoxy imasanduka yachikasu pamwala woyera?

Epoxy imatha kukhala yachikasu chifukwa cha ukalamba wa polima womwe umagwirizanitsidwa ndi kukhudzidwa kwa UV, kutentha, okosijeni, utomoni ndi chemistry yowumitsa, ndi zina zachilengedwe. Mwala woyera umapangitsa kusintha kwamitundu kakang'ono kowoneka bwino. Komabe, si mdima uliwonse kapena discolored dera weniweni epoxy yellowing; kulowa mopitirira muyeso, kudetsa, ndi mthunzi wa kuwala kungapangitse zolakwika zofanana.

2. Kodi pali utomoni wopanda chikasu wa epoxy?

Zogulitsa zamalonda zitha kufotokozedwa ngati zopanda chikasu kapena zachikasu pang'ono, koma ogula akuyenera kutanthauzira mawuwa ngati kukhazikika kwamtundu m'mikhalidwe yodziwika m'malo motsimikizira kuti palibe kusintha komwe kungachitike. Pama projekiti ovuta, yerekezerani momwe ukalamba umagwirira ntchito ndikuyesa makina owumitsa utomoni pamwala weniweni.

3. Ndi epoxy yotani yomwe iyenera kugwiritsidwa ntchito pamiyala yolimba yoyera?

Marble oyera olimba nthawi zambiri amapindula ndi epoxy yotsika kwambiri yachikasu yolowera, yomveka bwino, komanso kutuluka kokwanira kulimbitsa ming'alu yabwino. Dongosolo la Veropoxy's 5090 / D30M-BS ndilokhazikika pamwala wonyezimira woyera ndipo limalemba chikasu chochepa kwambiri, 400-600 CPS viscosity, chiŵerengero cha 100:30, ndi pafupifupi mphindi 80 kuchiritsa pafupifupi 24 ° C.

4. Chifukwa chiyani epoxy yowoneka bwino imapanga chizindikiro chakuda pa nsangalabwi yofewa yoyera?

Vuto likhoza kukhala lolowera kwambiri m'malo mwa chikasu chamankhwala. Utoto ukhoza kusintha momwe kuwala kumayendera kudzera mwa nsangalabwi ya porous, kupanga mawonekedwe onyowa kapena oderapo pozungulira malo omwe adakonzedwa. Kwa nsangalabwi yofewa yoyera, gwiritsani ntchito makina opangidwa kuti azitha kulowa mkati mokhazikika komanso osadetsa.

5. Kodi fakitale iyenera kuyesa bwanji epoxy isanagwiritse ntchito pamwala woyera?

Yesani ma epoxy pama slabs oyimira oyimira pa kutentha kwenikweni kwa fakitale. Lembani chiŵerengero chosakanikirana ndi kuchuluka kwa ntchito, fufuzani malire olowera, kulola kuchiritsidwa kwathunthu, pukuta slab pogwiritsa ntchito njira yachibadwa, ndi kuyerekezera mtundu, kuwala, kamvekedwe kachikasu, mthunzi, mawonekedwe a kukonza, ndi gloss. Pama projekiti apamwamba, onjezani kutentha kofananira kapena kuyezetsa ukalamba wa UV musanavomereze zambiri.

Momwe Mungasungire Kukonza Bwino Loyera Kuwoneka Mokhazikika Pakapita Nthawi

Kukhazikika kwa nthawi yayitali pamiyala yoyera kumadalira zambiri kuposa kuwonekera kwa utomoni. Dongosolo lopambana la epoxy liyenera kuphatikiza chemistry yotsika yachikasu, kulowa mkati mowongolera, kuchiritsa koyenera, kusakanikirana kosasintha, komanso kugwirizana ndi kapangidwe kake ka nsangalabwi. Ogula ayenera kuweruza mwala womalizidwa ndi wokalamba-osati maonekedwe a epoxy amadzimadzi mu chidebe.

Choyamba dziwani vuto lenileni

Malo okonzera chikasu atha kuwonetsa kusinthika kwa polima, koma halo yakuda imatha kubwera chifukwa cha kulowa kwambiri, zotsalira zapamtunda, kusintha kwa kuwala kokhudzana ndi chinyezi, kapena kudetsedwa. Kusamalira vuto lililonse lowoneka ngati "chikasu" kungapangitse fakitale kusintha kusintha kolakwika.

Fananizani utomoni ndi kapangidwe ka nsangalabwi

Mwala wolimba, wandiweyani:
khazikitsani chemistry yotsika kwambiri yachikasu, kuwonekera, komanso kulowetsa kokwanira kuti mulimbikitse ming'alu yaying'ono.

Mwala wofewa kapena wonyezimira woyera:
ikani patsogolo khalidwe losadetsa ndi kuwongolera kulowa kotero kuti kukonzako kusapanga ma halos amdima kapena zotsatira zamadzi.

Kupanga kutentha kwambiri:
tsimikizirani kukhazikika kwamtundu ndi machitidwe ochiritsa pamwala weniweni ndi kutentha kwa msonkhano.

Ntchito zowonetsedwa ndi UV:
funsani za momwe ukalamba ukuyendera kapena kuyesa kufananiza koyendetsedwa bwino m'malo mongoweruza momveka bwino.

Malo opukutidwa a Premium:
yang'anani utomoni mutatha kuchiritsidwa kwathunthu ndi kupukuta komaliza chifukwa maonekedwe onyowa okha sangathe kulosera slab yomalizidwa.

Chifukwa chiyani kuyesa kwachitsanzo kumafunika kwambiri pamwala woyera

Mitundu ya nsangalabwi yoyera imasiyana ndi porosity, translucency, veining, crack structure, ndi khalidwe la kuyamwa. Utoto womwe umavomerezeka pa slab umodzi ungapangitse mthunzi pa wina. Zidziwitso za ogulitsa ziyenera kugwiritsidwa ntchito polemba mndandanda wazinthu, pomwe kuyesa miyala yeniyeni kuyenera kupanga chivomerezo chomaliza.

Kodi kusintha kwa akatswiri a white-marble processing ndi chiyani?

Mapurosesa aukadaulo akuchoka pang'onopang'ono kuchoka ku "clear epoxy" kupita ku machitidwe enaake. Mwala wonyezimira wonyezimira, mwala wonyezimira wonyezimira, kutentha kwanyengo, malo owoneka bwino, komanso kuyika kowonekera kwa UV kulikonse komwe kumafunikira pamapangidwe a utomoni ndi momwe amalowera. Izi zimapangitsa kuti deta yogwiritsira ntchito, kukalamba, ndi ziyeneretso za zitsanzo zikhale zofunikira kwambiri pakuwunika kwa ogulitsa.

Malangizo Othandiza

Ngati epoxy palokha ikhala amber, ikani patsogolo utomoni wokhazikika komanso wowumitsa. Ngati nsangalabwiyo ikupanga kuwala kwakuda pomwe utomoni wochiritsidwa ukhalabe wowoneka bwino, chepetsani kulowa ndikufufuza momwe mwala amayamwa. Ngati kutentha kapena kuwala kwa UV kuli kokwera, konzani makinawo pansi pazimenezi. Ngati chiyero chowoneka ndi chofunikira, yesani mwala weniweni, malizitsani kuchiritsa ndi kupukuta, ndipo yerekezerani silabu yomalizidwa musanavomereze kuperekedwa kochuluka. Epoxy yabwino kwambiri ya marble si madzi owoneka bwino kwambiri - ndi mapangidwe omwe amakhalabe amphamvu komanso osawoneka bwino panthawi yonse yokonza ndi ntchito.

Mukuyenera Kuyesa Epoxy System pa White Marble?

Nsalu zoyera zimasiyana kwambiri ndi kachulukidwe, porosity, translucency, ndi mapangidwe a crack. Musanagule zambiri, yesani epoxy pa Carrara, Calacatta, Statuario, kapena marble ena oyera ndikuwunika malowedwe, chikasu, mithunzi, kuchiritsa, ndi maonekedwe opukutidwa pansi pa zochitika zenizeni za fakitale.
Funsani Chitsanzo cha White Marble Epoxy

Maumboni

  1. Charles Selwitz.
    Epoxy Resins mu Kusunga Mwala.
    Getty Conservation Institute.
    Kafukufuku mu Conservation Series, Getty Publications, 1992.
  2. William S. Ginell ndi Richard Coffman.
    Mwala Wophatikizidwa wa Epoxy Resin-Consolidated: Kusintha kwa Mawonekedwe Pakukalamba.
    Getty Conservation Institute.
    Maphunziro mu Conservation, Vol. 43, No. 4, 1998, tsamba 242-248.
  3. Elena Tesser, Lorenzo Lazzarini ndi Susanna Bracci.
    Kufufuza pa Chemical Structure ndi Kukalamba Kusintha kwa Cycloaliphatic Epoxy Resin EP2101 Yogwiritsidwa Ntchito Monga Stone Consolidant.
    Università Iuav di Venezia ndi National Research Council of Italy.
    Journal of Cultural Heritage, 2018.
  4. Chao Wu, Bing Chen Meng, Lik-ho Tam ndi Li He.
    Njira Zachikaso za Epoxy ndi Vinyl Ester Resins pansi pa Kutentha, UV ndi Kukalamba Kwachilengedwe ndi Njira Zotetezera.
    Mabungwe ofufuza kuphatikiza Beihang University.
    Kuyesa kwa Polima, Vol. 114, 2022, Article 107708.
  5. Seungyeon Lee, Seung Jun Oh ndi Koang-Chul Wi.
    Kukonzekera ndi Katundu Wakuthupi wa Epoxy Ndi Kupititsa patsogolo Kukanika kwa Yellowing kwa Kusungidwa kwa Stone Cultural Heritage.
    Hanseo University.
    Conservation Science in Museum, National Museum of Korea, Vol. 26, 2021, masamba 1-12.
  6. Shengzong Ci, Baoming Wang, Chengrui Di, Mingyu Wang, Bo Zhu and Kun Qiao.
    Effect of Ultraviolet Aging on Properties of Epoxy Resin and Its Pultruded Fiber-Reinforced Composite.
    Shandong University and Weihai Research Institute of Industrial Technology.
    Polymers, Vol. 17, No. 3, 2025, Article 294.
  7. WEST SYSTEM Technical Staff.
    WEST SYSTEM Buku Logwiritsa Ntchito & Kalozera wazogulitsa.
    Gougeon Brothers, Inc.
    WEST SYSTEM Technical Publications.
  8. Bruce Burton.
    Strategies for Reducing Amine-Cured Epoxy Yellowing in Decoupage and Decorative Coatings.
    Huntsman Corporation.
    Thermoset Resin Formulators Association Technical Paper, 2019.