Marble ndiyo yekutanga sarudzo yemidziyo yepasi nekuda kwekunaka kwayo uye kusimba. Nekudaro, dambudziko rekugova remabhura pasi rinowanzonetsa varidzi vemba, izvo zvisingakanganisi chitarisiko chete, asiwo zvine chekuita nekuchengetedza. Nzira dzechinyakare dzekugadzirisa dzinotora nguva uye dzinoshanda, uye mhedzisiro yakaoma kuvimbisa. Ichi chinyorwa chicharatidza mhinduro yekuchinja kwauri - epoxy resin teknolojia. Nekuita kwayo kwakanakisa kwekubatana uye kushanda kuri nyore, inopa inoshanda, ine hushamwari kwezvakatipoteredza uye ine hupfumi kugadzirisa nzira yedambudziko rekukomba remarble pasi. Tevere, ngationgororei kuti epoxy resin inogona sei kuve chishandiso chine simba chekugadzirisa dambudziko rekugova remabhura pasi, kuitira kuti imba yako igone kudzoreredza kubwinya kwayo kwekare uye kuchengetedzeka.
Chii chinonzi ngoma isina mhango?
Chii chinonzi hollow ngoma? Mushure mekuiswa kwemvura-paste yekuchengetwa kwematombo epasi, pane mikaha pakati pebwe uye bonding layer, kana iyo yekubatanidza dhizaini uye base layer. Inzwi rakaita sengoma rinogona kunzwika kana uchirova zvinyoro nyoro, saka inowanzonzi hollow ngoma chiitiko chedombo repasi.

Sei marble aine madhiramu asina mhango?
1. Urombo hwekuisa tekinoroji
Mamiriro ezvinhu 1: Kana uchigadzira, simende, dhaka kana dheti kumashure kwebhodhi rakanyanya kutetepa. Mushure mekugadzira, mvura inoputika, uye mukaha unoumbwa pakati pekunamatira nedombo, zvichikonzera madhiramu asina maburi.
Mamiriro ezvinhu 2: Panzvimbo pokuisa simende kuseri kwedombo, mushandi wacho anodururira simende pasi zvakananga, oitsetsenura nechigero, uye ipapo kubatanidza dombo racho. Kana simende ichidirwa pasi, chigadziko chinogezwa chichibviswa, zvichikonzera kugovaniswa kusina kuenzana, izvo zvinozoita kuti simba rekubatanidza rive risina kuenzana uye kuita madhiramu asina maburi.
Mamiriro echitatu: Pakugadzira, kana basa rapera, ibwe riri pamucheto wenzvimbo yakavezwa harina chisimbiso. Kuteuka kwesemende uye kuoma nekukurumidza mumhepo kunokonzeresa makomba.
2. Kusakwana kupora nguva yekugadzira
Mushure mekugadzira, zvinhu zvakasiyana-siyana zvekunamatira zvichiri munguva yekurapa yekusimbisa. Kana ukamhanyira kuyambuka-kuvaka kana kuaisa mukushandiswa pachine nguva, dombo rinosunungura nyore uye kuumba makomba.
Mhinduro kune marble hollowing
1. Bvisa marble slab isina mhango woidzorera zvakare. Iyi nzira inonyanya kunetsa kuvaka uye mutengo wekugadzirisa wakakwira. Zvinotonyanya kukosha, zvakaoma kuita kuti kupenya, ruvara uye pateni yeatsva uye ekare marble slabs aenderane mushure mekugadzirisa. Kana iri nzvimbo yakakura yekuchera, nzira iyi inopedza nguva uye inowedzera mitengo. Inokurudzirwa kushandisa nzira yechipiri.
2. Gamuchira epoxy resin simbi bhoti anchoring nzira. Iyo yepamusoro yakasimba mushure mekugadzirisa uye haizokuvadzi. Nzira yekuvaka iri nyore, kuchengetedza basa uye zvinhu.
Matanho ekutanga ekushanda: cherechedza maburi uye mucherechedzo-kudhirowa chinzvimbo-permeability bvunzo-kuvharwa kwechinguvana kwebhodhi seams-pressurized grouting-cleaning-repair-maintenance.

Hollow stone floor care method
Shandisa epoxy resin simbi bhaudhi anchoring nzira. Mushure mekugadzirisa, chigadziko chakasimba uye chakasimba, uye nzira yekuvaka iri nyore, kuchengetedza basa uye zvinhu. Matanho ekugadzira ndeaya:
(1) Padombo risina mhango rinoda kugadziriswa, tarisa nzvimbo yekuchera uye nhamba, uye tanga washandisa chibooreso chemagetsi chine carbide insert drill bit kuboora gomba rakanaka 5mm. Zvinofanira kucherechedzwa kuti chibooreso chinofanirwa kurerekera pasi pakona ye15-degree angle pakuchera kudzivirira kudonha. epoxy resin slurry kubva pakuyerera kubva mugomba mushure mekuita grouting. Mushure mokunge gomba racho radhirwa, guruva riri mugomba rinobviswa nemhepo compressor. Muchina wekubvisa guruva wemhepo unofanirwa kuiswa pasi pegomba kuitira kuti guruva rose ribude kubva mugomba nemhepo yakamanikidzwa.
(2) Chechipiri, gadzira epoxy resin slurry. Shandisa epoxy resin, dibutyl phthalate, mushonga wekurapa, uye simende zvinoenderana nechikamu chakakodzera chakapihwa mukuchengetwa kwematombo. Paunenge uchisanganisa, tanga wasanganisa epoxy resin uye dibutyl phthalate, wobva wawedzera mushonga wekurapa kusanganisa, wobva wawedzera simende uye sanganisa zvakanaka. Idururire mumushini we grouting uye inogona kushandiswa.
(3) Nhanho inotevera ndeye grouting uye anchoring. Shandisa resin grouting pfuti kuzadza gomba neresin slurry. Musoro wepfuti unofanirwa kuiswa zvakadzika muzasi megomba uye musoro wepfuti unofanirwa kuburitswa panze zvishoma nezvishoma panguva yekuchera. Mushure mekunge slurry yazadzwa, isa musimbi anchor bolt. Kuti uvandudze kusungirirana, bhaudhi rinofanira kuitwa rudzi rwakarukwa uye nati ine hexagonal inofanira kukwizwa kune rumwe rutivi kuti inamire zvakasimba slab yemarble.
(4) Usati waisa bhaudhi, kuitira kudzivirira iyo jekiseni epoxy resin slurry kubva pakuyerera uye kusvibisa marble pamusoro, unogona kutanga washandisa lime paste kuvhara gomba. Mushure mekunge epoxy resin slurry yaoma, chenesa ipulagi. Wobva washandisa acetone kana xylene kuchenesa resin slurry yasara padombo pamusoro panguva kudzivirira kusvibisa pasi.
(5) Mushure mekuita grout kwemaawa maviri kusvika matatu, namira nedhaka jena simende. Mucherechedzo wemuvara wedhaka unofanirwa kunge uri pedyo sezvinobvira kune ruvara rwematombo ari kugadziriswa. Mushure mekupedza kuvaka dombo rekuchengeta dombo, mirira kwerinenge zuva kuti epoxy resin slurry pamusoro kuti iome, uye ipapo unogona kutamba nayo uchifara zvakare.