ʻO Marble ka koho mua no nā mea papahele ma muli o kona nani a me ka lōʻihi. Eia naʻe, pilikia pinepine ka pilikia hollowing o nā papahele marble i nā mea nona ka hale, ʻaʻole ia e pili wale i ka helehelena, akā pili pū kekahi i ka palekana. ʻO nā ʻano hana hoʻoponopono kuʻuna he mau manawa a paʻakikī hoʻi, a paʻakikī ke hōʻoia ʻana i nā hopena. E hōʻike ana kēia ʻatikala i kahi hopena kipi no ʻoe - epoxy resin ʻenehana. Me kāna hana hoʻopaʻa paʻa maikaʻi a me ka hana maʻalahi, hāʻawi ia i kahi ala hoʻoponopono maikaʻi, kūlohelohe a me ka hoʻokele waiwai no ka pilikia hollowing o nā papahele marble. A laila, e ʻimi kākou pehea e hiki ai i ka epoxy resin ke lilo i mea hana ikaika e hoʻoponopono ai i ka pilikia hollowing o nā papahele marble, i hiki ai i kou home ke hoʻihoʻi i kona nani a me ka palekana.
He aha ka pahu pahu?
He aha ka pahu pahu? Ma hope o ka hoʻokomo ʻia ʻana o ka mālama pōhaku papahele, aia nā āpau ma waena o ka pōhaku a me ka papa hoʻopaʻa, a i ʻole ka papa hoʻopaʻa a me ka papa kumu. Hiki ke lohe ʻia ke kani ʻana me he pahu lā ke paʻi mālie, no laila ua kapa ʻia ʻo ia ʻo ka hollow drum phenomenon o ka pōhaku papahele.

No ke aha i loaʻa ai i nā pahu hollow?
1. Ka ʻenehana hoʻonohonoho maikaʻi ʻole
Kūlana 1: I ka wā e paʻi ai, ʻoi aku ka lahilahi o ka sima, ka pāpaʻa a i ʻole ka mea hoʻopili ma ke kua o ka papa. Ma hope o ka paʻi ʻana, hoʻoheheʻe ka wai, a ua hana ʻia kahi āpau ma waena o ka mea hoʻopili a me ka pōhaku, e hoʻoulu ai i nā pahu pahu.
Kūlana 2: Ma mua o ka hoʻopili ʻana i ke kima ma ke kua o ka pōhaku, ninini pololei ka mea hana i ka sima ma ka honua, hoʻomaʻamaʻa me kahi ʻōpala, a laila hoʻopaʻa i ka pōhaku. Ke ninini ʻia ka sima ma ka honua, e holoi ʻia ka papa kumu, e hopena i ka puʻunaue like ʻole, a laila e hoʻoneʻe ʻole ai ka ikaika o ka hoʻopaʻa ʻana a hana i nā pahu pahu.
Kūlana 3: I ka paʻi ʻana, i ka pau ʻana o ka hana, ʻaʻole i hoʻopaʻa ʻia ka pōhaku ma ka lihi o ka wahi i hoʻopaʻa ʻia. ʻO ke kahe ʻana o ka sima a me ka maloʻo wikiwiki ʻana i ka makani e hoʻohua ai.
2. ʻAʻole lawa ka manawa hoʻōla no ka paving
Ma hope o ka paving, aia nā mea hoʻopili like ʻole i ka wā curing o ka solidification. Inā wikiwiki ʻoe e hana i ke keʻa a hoʻohana ʻia paha ia mau mea ma mua, e wehe maʻalahi ka pōhaku a lilo i lua.
Hoʻoholo no ka hollowing marble
1. Wehe i ka papa kinikini hakahaka a kau hou ia. ʻOi aku ka paʻakikī o kēia ʻano hana a ʻoi aku ka nui o ke kumukūʻai hoʻoponopono. ʻO ka mea nui, he paʻakikī ke hoʻohālikelike ʻana i ka ʻōlinolino, ka waihoʻoluʻu a me ke ʻano o nā papa marble hou a kahiko ma hope o ka hoʻoponopono ʻana. Inā he wahi nui o ka hollowing, hoʻopau kēia ʻano i ka manawa a hoʻonui i nā kumukūʻai. Manaʻo ʻia e hoʻohana i ke ala ʻelua.
2. E hoʻohana i ke ʻano epoxy resin steel bolt anchoring method. Paʻa ka ʻili ma hope o ka hoʻoponopono ʻana a ʻaʻole e pōʻino. He maʻalahi ke ʻano hana, mālama i ka hana a me nā mea hana.
Nā ʻanuʻu hana kumu: ʻike i ka hollowing a me ka mark-drilling positioning-permeability test-temporary sealing of board seams-pressurized grouting-cleaning-repair-maintenance.

ʻO ka mālama ʻana i ka papahele pōhaku ʻaʻa
E hoʻohana i ke ʻano epoxy resin steel bolt anchoring method. Ma hope o ka hoʻoponopono ʻana, ikaika a paʻa ke kumu, a maʻalahi ke ʻano hana, mālama i ka hana a me nā lako. ʻO nā hana kūkulu:
(1) No ka pōhaku lua e pono e hoʻoponopono ʻia, e hoʻoholo i ke kūlana wili a me ka helu, a e hoʻohana mua i ka wili uila me kahi pahu hoʻokomo carbide e wili ai i ka lua maikaʻi 5mm. Pono e hoʻomaopopo ʻia e hoʻohuli ʻia ka bit drill i lalo ma kahi kihi 15-degree i ka wā e wili ai e pale i ka epoxy resin slurry mai ka kahe ʻana mai loko mai o ka lua ma hope o ka grouting. Ma hope o ka wili ʻia ʻana o ka lua, hoʻoneʻe ʻia ka lepo i loko o ka lua me kahi mea hoʻoheheʻe ea. Pono e hoʻokomo ʻia ka mīkini ea hoʻoneʻe lepo i lalo o ka lua i hiki i nā lepo āpau ke pakele mai ka lua me ka ea paʻa.
(2) ʻO ka lua, e hana i ka epoxy resin slurry. E hoʻohana i ka resin epoxy, ka dibutyl phthalate, ka lāʻau lapaʻau, a me ka sima e like me ka ʻāpana kūpono i hāʻawi ʻia i ka mālama pōhaku. I ka hui ʻana, hui mua i ka resin epoxy a me ka dibutyl phthalate, a laila hoʻohui i ka mea hoʻōla e hui, a laila hoʻohui i ka sima a hui maikaʻi. E ninini i loko o ka mīkini grouting a hiki ke hoʻohana ʻia.
(3) ʻO ka hana aʻe ʻo ka grouting a me ka heleuma. E hoʻohana i ka pu resin grouting e hoʻopiha i ka lua me ka resin slurry. Pono e hoʻokomo hohonu ʻia ke poʻo o ka pū i lalo o ka lua a e hoʻoneʻe mālie ʻia ke poʻo pū i waho i ka wā o ka grouting. Ma hope o ka hoʻopihaʻiaʻana o ka slurry, e hoʻokomo i ka pahu heleuma kila. I mea e hoʻomaikaʻi ai i ka hopena hoʻopaʻa ʻana, pono e hana ʻia ka bolt i ʻano hilo a pono e wili ʻia kahi nut hexagonal ma kekahi ʻaoʻao e hoʻopaʻa paʻa i ka papa maʻa.
(4) Ma mua o ka hoʻokomo ʻana i ka bolt, i mea e pale ai i ka kahe ʻana o ka epoxy resin slurry i hoʻoheheʻe ʻia a hoʻohaumia i ka ʻili marble, hiki iā ʻoe ke hoʻohana mua i ka paʻi lime e pale i ka lua. Ma hope o ka paʻa ʻana o ka epoxy resin slurry, hoʻomaʻemaʻe i ka plug. A laila e hoʻohana i ka acetone a i ʻole xylene e hoʻomaʻemaʻe i ka slurry resin e waiho ana ma ka ʻili pōhaku i ka manawa e pale aku ai i ka lepo.
(5) Ma hope o ka grouting no ʻelua a ʻekolu mau hola, e hoʻopaʻa ʻia me ka mīkini sima keʻokeʻo. ʻO ka waihoʻoluʻu o ka mortar waihoʻoluʻu e pili kokoke i ke kala o ka ʻili pōhaku e hoʻoponopono ʻia. Ma hope o ka hoʻopau ʻana i ke kūkulu ʻana i nā pōhaku hollow, e kali no kahi lā e maloʻo ai ka epoxy resin slurry ma ka ʻili, a laila hiki iā ʻoe ke pāʻani me ka hauʻoli hou.