Mu rwego rwo gushushanya imyubakire, marble itoneshwa cyane kubwimiterere idasanzwe no kugaragara neza. Nyamara, amagorofa ya marble byanze bikunze azagira ibibazo nko gushushanya no kwangirika mugihe cyo kuyakoresha, bigira ingaruka mubwiza muri rusange no mubuzima bwa serivisi. Kubwamahirwe, hamwe niterambere ryikoranabuhanga ryibikoresho, epoxy resin itanga igisubizo cyiza kandi cyizewe cyo gusana amagorofa. Iyi ngingo izatangiza muburyo burambuye ikoreshwa rya epoxy resin mugusana hasi ya marble, harimo ibiyiranga, uburyo bwo gusana nibyiza.

epoxy resins
Vero Bond epoxy resin

Ibiranga epoxy resin

Epoxy resin nikintu cya polymer kama kirimo amatsinda abiri cyangwa menshi ya epoxy muri molekile, ubusanzwe ikoreshwa muburyo bwa resin. Ifite imbaraga zo guhuza cyane, irashobora guhuzwa cyane hejuru ya marimari, ntabwo byoroshye kumeneka, kandi ikemeza ko igice cyasanwe gihujwe neza nibuye ryambere. Muri icyo gihe, igipimo cyo kugabanuka kwa epoxy resin mugihe cyo gukira kiri hasi cyane, bivuze ko mugihe cyo gusana, nyuma ya epoxy resin yujujwe mugice cyacagaguritse cyangwa cyangiritse, ntihazabaho ihungabana rigaragara nyuma yo gukira, bityo bigatuma habaho ubuso bwubuso bwakosowe.

Byongeye kandi, uburemere bwa molekuline ya epoxy resin irakwiye, kandi ububobere bwayo burashobora guhinduka nkuko bikenewe. Ntishobora kwinjira gusa no kwinjira mu bice bito by'iriba rya marimari, kumenya gusana byimazeyo kuva imbere kugeza hejuru, ariko kandi birashobora gukira ubushyuhe bwicyumba, kandi byihutisha gukira ukoresheje ubushyuhe, butanga ihinduka rikomeye mubikorwa byubwubatsi.

Uburyo bwo gusana hasi ya marble hamwe na epoxy resin

Imyiteguro mbere yo gusanwa

Mbere yo gukoresha epoxy resin kugirango usane hasi ya marble, ugomba gukora imyiteguro ihagije. Ubwa mbere, sukura imyanda n'umukungugu bikikije hasi yangiritse, kandi urebe ko aho gusana byumye kandi nta mavuta arimo. Iyi ntambwe ningirakamaro kugirango habeho guhuza neza hagati ya epoxy resin nubuso bwa marble.

Icya kabiri, genzura neza imiterere yubutaka bwangiritse, harimo intera yangiritse, ubujyakuzimu, niba hari uduce, nibindi, bizafasha kumenya gahunda yo gusana nubwoko nubunini bwibikoresho bisabwa. Hanyuma, ukurikije ibyangiritse, tegura ibikoresho byo gusana epoxy resin ihuye, ibikoresho byo gukiza, ibyuzuza, paste yamabara, nibindi, hanyuma urebe ko ibikoresho byatoranijwe bihuye nibikoresho byumwimerere kugirango urebe neza ko bisanwa.

Gusana ibishushanyo

Kubishushanyo hasi ya marble, intambwe zikurikira zirashobora gukoreshwa mugusana. Ubwa mbere, koresha acetone hamwe na brush ya nylon kugirango ukureho uduce twinshi twa marble tuvuye ahantu hacuramye, bifasha kunoza imiterere ya epoxy resin hejuru ya marble. Noneho, vanga epoxy resin hamwe na agent ikiza mubipimo bikwiye, mubisanzwe 1/10. Niba bikenewe, pigment hamwe nuwuzuza nabyo birashobora kongerwaho kuri epoxy resin kugirango ihuze ibara rya marble yasanwe na marble yumwimerere.

Ibikurikira, shyira epoxy yateguwe neza iringaniye, urebe ko epoxy resin yuzuza byuzuye. Urashobora gukoresha scraper cyangwa brush kugirango uyikoreshe, kandi witondere kudasiga ibituba. Hanyuma, reka epoxy resin ikire muburyo busanzwe. Ukurikije ubushyuhe bwibidukikije nubwoko bwa epoxy resin, igihe cyo gukira kirashobora gutandukana kuva amasaha make kumunsi. Nyuma yo gukira, koresha urusyo cyangwa umusenyi kugirango usukure ahantu hasanwe kugirango uburinganire hamwe nubutaka bukikije.

Gusana ibyangiritse

Kubintu byangiritse bya marble, intambwe zo gusana nuburyo bukurikira. Ubwa mbere, niba agace kangiritse ari nini, ugomba kubanza guca igice cyangiritse kugirango ubanze ugire imbibi zisanzwe zo gusana, zifasha kwemeza ko resin epoxy ishobora kuzuzwa neza mubice byangiritse kandi igahuzwa cyane nubutaka bukikije nyuma yo gukira.

Noneho, ukurikije ibyangiritse, vanga urugero rukwiye rwa epoxy resin mortar. Epoxy resin mortar isanzwe igizwe na epoxy resin, imiti ikiza, yuzuza n'umusenyi wa quartz. Iyi minisiteri ifite imbaraga nyinshi nuburyo bwiza bwo kuzuza, kandi irashobora gusana neza ibice byangiritse hasi ya marimari. Noneho, uzuza epoxy resin mortar yateguwe ahantu yangiritse, koresha scraper kugirango uyisibe neza, hanyuma urebe ko ibikoresho bisukuye hasi. Mugihe cyo kuzuza, witondere kwirinda umwuka winjira kugirango wirinde kwibibyimba.

Hanyuma, nyuma yo gutegereza epoxy resin mortar kugirango ikomere, koresha urusyo kugirango usya ahantu hose hasanwa kugirango igice cyasanwe kiringaniye hasi. Mugihe cyo gusya, witondere kugenzura imbaraga n'umuvuduko kugirango wirinde kwangirika hasi.

Gusana umwobo

Gufata hasi ya marble nikimwe mubibazo bisanzwe. Epoxy resin ibyuma bya bolt anchoring uburyo bushobora gukemura neza iki kibazo. Intambwe zihariye nizi zikurikira. Ubwa mbere, kubuye ryubusa rigomba gusanwa, menya aho gucukura numubare, hanyuma ukoreshe imyitozo yamashanyarazi ifite ibikoresho bya karbide winjizamo bito kugirango ucukure umwobo mwiza wa 5mm. Mugihe cyo gucukura, bito bitobora bigomba guhindukirira hepfo kumurongo wa dogere 15 kugirango wirinde epoxy resin gutembera gusohoka mu mwobo nyuma yo gutontoma.

Noneho, umwobo umaze gucukurwa, koresha compressor yo mu kirere kugirango ukureho umukungugu uri mu mwobo. Imashini yo gukuramo ivumbi igomba kwinjizwa munsi yumwobo kugirango umukungugu wose uve mu mwobo hamwe numwuka uhumanye.

Noneho, koresha epoxy resin, dibutyl phthalate, imiti ikiza, na sima kugirango uvange muburyo bukwiye. Iyo uvanze, banza uvange epoxy resin na dibutyl phthalate, hanyuma ushyiremo imiti ikiza kugirango uvange, hanyuma ushyiremo sima kugirango uvange neza, uyisuke mumashini isya kugirango ikoreshwe.

Hanyuma, suka epoxy resin slurry mumwobo wacukuwe unyuze mumashini ya grouting kugirango epoxy resin slurry yuzure byuzuye mubice byuzuye. Nyuma yo gutontoma, reka epoxy resin slurry ikire bisanzwe. Igihe cyo gukira giterwa n'ubwoko bwa epoxy resin n'ubushyuhe bwibidukikije.

Ibyiza bya epoxy resin yo gusana hasi ya marble

Inzira ya epoxy resin yo gusana hasi ya marble iroroshye kandi byihuse. Kuva kwitegura ibikoresho kugeza gusana birangiye, mubisanzwe birashobora kurangira mumunsi umwe, bigabanya cyane igihe cyubwubatsi kandi bikagabanya kwivanga no gukoresha bisanzwe. Igorofa ya marimari yasanwe irashobora kugarura ububengerane bwayo nuburyo bwayo, kandi ntibishobora gutandukana nigice cyangiritse. Ibara rya epoxy resin ituma ihuza marble yamabara atandukanye, ikemeza ubwiza muri rusange nyuma yo gusanwa.

Byongeye kandi, epoxy resin ifite ibihe byiza byo kurwanya ikirere no kurwanya gusaza, kandi irashobora gukomeza imikorere ihamye mubihe bitandukanye by’ibidukikije. Igorofa ya marimari yasanwe ntishobora kwihanganira kwambara no kurira mu mikoreshereze ya buri munsi, ariko kandi irashobora kurwanya isuri y’ibidukikije hanze, ikongerera igihe cyo gukora hasi ya marimari.

Ibikoresho byinshi bigezweho bya epoxy resin ikoresha formulaire yangiza ibidukikije, idafite uburozi, impumuro nziza, kandi itagira ingaruka kumubiri wumuntu no kubidukikije, ibyo bigatuma inzira ya epoxy resin yo gusana hasi ya marble itekanye kandi ikangiza ibidukikije.

Epoxy resin ya marble
Epoxy resin ya marble

Umwanzuro

Muncamake, epoxy resin ifite ibyiza byingenzi nibisabwa mugukoresha mugusana hasi ya marble. Ntishobora gusa gusana neza ibishushanyo, kumeneka nibibazo byubusa hasi ya marimari, ariko kandi birashobora kwemeza ubwiza nigihe kirekire byubutaka bwa marimari yasanwe, mugihe bitangiza ibidukikije.

Hamwe no gukomeza gutera imbere no guhanga udushya mu ikoranabuhanga, imikorere ya epoxy resin ibikoresho bizaba byiza kurushaho kandi urwego rwo gusaba ruzagurwa. Nka epoxy yumwuga itanga ibikoresho, Veropoxy izakomeza kwiyemeza gukora ubushakashatsi no guteza imbere no gutanga ibicuruzwa byujuje ubuziranenge, ikagira uruhare runini mugutezimbere gusana hasi ya marimari nizindi nzego zijyanye nayo.