I-Epoxy Ephakeme Yokungena Kwemabula Emabula Emazingeni Okushisa Aphezulu (38-45°C) - 5089 / BCO25Q Yemabula Enemibala

I-Epoxy Yokungena Okuphezulu Yezinsimbi Zemabula Ezingeni Lokushisa Eziphakeme (38-45°C) – 5089/BCO25Q uhlelo. Yakhelwe ngokukhethekile ukusetshenziswa kwemabula enombala ezindaweni ezishisayo. Ukungena okujulile kokulungisa imifantu nokuthuthukisa umbala. Ukwelashwa kwemizuzu engama-80, i-400-600 CPS viscosity, ukumelana nokuphuzi okuphezulu. Ilungele ukubuyiselwa kwendawo ye-marble slab kanye nokuqiniswa ezindaweni ezinokushisa okuphezulu. Umkhiqizi waseChina. Amasampuli ayatholakala.

Imininingwane

IsiciI-Epoxy Resin yeGranite
  
  
  
  
  
  
Isifinyezo Esisheshayo: I-High Penetration Epoxy ye-Marble Slabs in High Temperature (38-45°C) - 5089 / BCO25Q i-epoxy resin esebenza kahle eklanyelwe ukusetshenziswa nama-slabs emabula anemibala ezindaweni ezishisayo. Inikeza ukungena okuphezulu, ukuhlangana okuhle kakhulu, kanye nokulungiswa kokuqhekeka okuhlala isikhathi eside, nokusebenza okuzinzile kokwelapha emazingeni okushisa aphakathi kuka-38-45°C.

I-Epoxy Yokungena Okuphezulu Kwezinsimbi Zemabula Ezingeni Lokushisa Eziphakeme (38-45°C) | China Suppliers & Manufacturer

I-High Penetration Epoxy yethu ye-Marble Slabs in High Temperature (38-45°C) iwuhlelo lwe-epoxy resin olusebenza kahle oludizayinelwe ama-slabs emabula, ikakhulukazi ezindaweni ezinezinga lokushisa eliphezulu. Le Epoxy Yokungena Okuphezulu Kwezingqimba Zemabula Ezingeni Lokushisa Eziphakeme (38-45°C) inikeza ukungena okujulile kwemabula enombala, ihlinzeka ngokuthuthukiswa kombala okuphakeme, ukugcwaliswa kokuqhekeka, nokubuyiselwa kwendawo. Uhlelo kulula ukuyisebenzisa, ngaphandle kwamathuluzi akhethekile adingekayo, futhi ilungele kokubili imigqa yokucubungula okwenziwa ngesandla kanye ne-othomathikhi ezimweni zezulu ezishisayo. Njengabahlinzeki nabakhi abaholayo baseShayina, sinikeza amanani entengo aqondile efekthri nezixazululo ezenziwe ngezifiso zama-oda amaningi emhlabeni wonke.

Ingabe ufuna i-High Penetration Epoxy engcono kakhulu ye-Marble Slabs Emazingeni Okushisa aphezulu (38-45°C) kubahlinzeki abathembekile base-China? Uhlelo lwethu lwe-5089/BCO25Q luhlanganisa ukugeleza okuphezulu, ifomula ye-viscosity ephansi eqinisekisa ukungena okujulile kanye nokugcwalisa okusebenzayo okuqhekekile kumabula anombala. Yakhelwe ngokukhethekile indawo enezinga lokushisa eliphezulu (38-45°C), iletha ukusebenza kokwelapha okuzinzile, ukuthuthukiswa kombala okuhle kakhulu, nokumelana nokuphuzi okuphezulu. Ilungele ukubuyiselwa kwendawo ye-marble slab kanye nokuqiniswa ezindaweni ezishisayo.

Incazelo Yomkhiqizo

I-High Penetration Epoxy ye-Marble Slabs in High Temperature (38-45°C) iwuhlelo lwe-epoxy resin olusebenza kahle oludizayinelwe ama-slabs emabula, ikakhulukazi ezindaweni ezinezinga lokushisa eliphezulu. Inikeza ukungena okujulile kwe-marble enemibala, ihlinzeka ngokuthuthukiswa kombala okuphezulu, ukugcwaliswa kwe-crack, nokubuyiselwa kwendawo. Uhlelo kulula ukulusebenzisa, alukho amathuluzi akhethekile adingekayo, futhi lulungele kokubili imigqa yokucubungula okwenziwa ngesandla kanye ne-othomathikhi. Le High Penetration Epoxy yamaSlabs Emabula Emazingeni Okushisa Aphezulu (38-45°C) yakhelwe ngokukhethekile ukusetshenziswa kwemabula enombala, iyihlukanise nama-epoxies aklanyelwe izinhlobo zemabula emnyama, emhlophe, noma emnyama.

 

I-Professional-2-step-epoxy-for-hard-granite

Izici Zomkhiqizo & Ukucaciswa

Isici Incazelo
Isici Ukugeleza okuphezulu, ukungena okuphezulu kwe-epoxy resin yama-slabs emabula anombala
Impahla Esebenzayo Ama-slabs emabula anombala
Ikhodi Yesistimu ye-Epoxy 5089 / BCO25Q
I-Epoxy System Ratio 100 :25
Ukuqina Ukuzinza okuphezulu nokuhlala isikhathi eside ngemuva kokwelashwa
Ukusebenziseka kalula Kulula ukuxuba nokusebenzisa, awekho amathuluzi akhethekile adingekayo
Isikhathi sokuphumula Cishe imizuzu engu-80
Ukumelana Okuphuzi Phezulu
Izinga Lokushisa 38–45°C
I-Viscosity I-CPS 400–600

Izinkinga Iyazixazulula

  • Imifantu nokungapheleli endaweni yemabula enombala - I-Epoxy Yethu Yokungena Okuphezulu YamaSlabs Emabula Emazingeni Okushisa Aphezulu (38-45°C) igcwalisa futhi ilungise ngempumelelo.
  • Umbala ongalingani kanye nobuthuntu kuma-slabs emabula anemibala - Ukungena okujulile kuthuthukisa umbala wemvelo nokukhanya
  • Ukungena okuphansi nokunamathela okunganele kwezinhlelo ze-epoxy zendabuko ekushiseni okuphezulu
  • Ukungaqini kwezinga lokushisa kwamanye amasistimu e-epoxy - Ukusebenza okuzinzile kokuphulukisa ku-38-45°C
  • Izinketho ezinomkhawulo zemabula enombala uma kuqhathaniswa nama-epoxies emabula emnyama, emhlophe, noma emnyama

Izicelo Ezinconyiwe

  • Ukuthuthukiswa kwendawo ye-marble slab enombala kanye ne-toning kusetshenziswa i-High Penetration Epoxy ye-Marble Slabs Emazingeni Okushisa aphezulu (38-45°C)
  • Ukugcwaliswa kwemifantu kanye nokulungiswa kwendawo yamatshe amatshe anemibala ezindaweni ezishisayo
  • Ukubuyisela izindawo zemabula ezinombala endaweni enezinga lokushisa eliphezulu (38-45°C)
  • Ukulungiswa kokupholisha izindawo zemabula ezinemibala ngemva kokukhanda imifantu
  • Izikhungo zokucubungula imabula yesimo sezulu esishisayo ezidinga amasistimu e-epoxy azinzile

Izinzuzo Zokusebenza Ezibalulekile

  • Ukugeleza okuphezulu, ifomula ye-viscosity ephansi iqinisekisa ukungena okujulile kanye nokugcwalisa okusebenzayo okuqhekekile kumabula anombala
  • Ithuthukisa umbala wemvelo nokubukeka kwemabula enombala – 区别于 ama-epoxies emabula amnyama, amhlophe, namnyama
  • Ukusebenza kokwelapha okuzinzile endaweni enezinga lokushisa eliphezulu (38–45°C)
  • Ukumelana okuhle kakhulu nokuphuzi ngemuva kokwelapha ukuzinza kombala kwesikhathi eside
  • Kulula ukukusebenzisa ngaphandle kwamathuluzi akhethekile adingekayo kuyo yomibili imigqa yezandla kanye ne-automated
  • Imizuzu engu-80 yokuphulukisa isikhathi sokuhamba komsebenzi wokukhiqiza okusebenzayo
  • I-Factory Direct Supply: Njengabahlinzeki bempahla baseChina abahamba phambili, sinikeza amanani ancintisanayo nokutholakala okuthembekile.

Incazelo Yesistimu Yomkhiqizo

Lo mkhiqizo uyisistimu ye-epoxy resin enezingxenye ezimbili:

Ingxenye A: I-5089 Resin
Ingxenye B: I-BCO25Q Hardener

Yakhelwe ukunikeza ukungena okuhle kakhulu, ukubopha, kanye nokuthuthukiswa kombala ezindaweni zemabula ezinombala, ikakhulukazi ezindaweni ezinezinga lokushisa eliphezulu. Ngemva kokuxuba izingxenye ngesilinganiso esinconyiwe esingu-100:25, le-High Penetration Epoxy ye-Marble Slabs in High Temperature (38-45°C) ihlinzeka ngokucwebezela, okubuyisiwe kokuqeda kanye nokulungisa imifantu ephumelelayo ngokukhethekile ngezinhlobo zemabula ezinemibala.

Icubungula Iziphakamiso

  1. Qinisekisa ukuthi indawo yemabula enombala ihlanzekile, yomile, futhi ayinalo uthuli noma uwoyela ngaphambi kokufaka le Epoxy Yokungena Okuphezulu YamaSlabs Emabula Emazingeni Okushisa aphezulu (38-45°C)
  2. Hlanganisa izingxenye ngesilinganiso esinconyiwe esingu-100:25 ukuze usebenze kahle
  3. Faka isicelo ngokulinganayo ukuze uqinisekise ukumbozwa okuphelele kwemifantu nezindawo ezingaphezulu
  4. Vumela isikhathi esanele sokungena okujulile ngaphambi kokwelapha (cishe imizuzu engama-80 ku-38-45°C)
  5. Gcina izinga lokushisa le-ambient phakathi kwebanga lama-38-45°C ukuze uphulukiswe kahle
  6. Qhubeka nokupholisha noma ukuqeda indawo ngemuva kokuqeda ukuphulukiswa
  7. Hlanza amathuluzi ngokushesha ngemva kokusetshenziswa ngaphambi kokwelashwa kwe-epoxy

Okubalulekile: Ukulandela lezi ziphakamiso zokucubungula kuqinisekisa ukusebenza kahle kwe-High Penetration Epoxy for Marble Slabs in High Temperature (38-45°C) kubahlinzeki abachwepheshile base-China, ikakhulukazi uma usebenza ngemabula enemibala ezindaweni ezishisayo.

Izinhlobo Zamatshe Ezifanelekayo

  • Imabula enombala - Zonke izinhlobo ezihlanganisa i-beige, epinki, eluhlaza, ephuzi, nezinye zemabula ezinemibala
  • Imabula enombala ominyene enemifantu noma ukungapheleli okudinga ukungena okujulile
  • Ama-slabs emabula acutshungulwa endaweni enezinga lokushisa eliphezulu (38-45°C)

Qaphela: Le High Penetration Epoxy yamaSlabs Emabula Emazingeni Okushisa Okuphezulu (38-45°C) yakhelwe ngokukhethekile ukusetshenziswa kwemabula enombala, iyihlukanise nama-epoxies aklanyelwe izinhlobo zemabula emnyama, emhlophe, noma emnyama. Hlola endaweni encane kuqala ukuze uqinisekise ukuhambisana nemabula yakho enemibala ethile.

Ukupakisha & Supply

  • Ukupakisha Okujwayelekile: Iphakheji ye-epoxy evamile ye-A/B etholakalayo ezindaweni zokucubungula imabula
  • Ukupakisha Ngokwezifiso: Izinketho zokupakisha ngokwezifiso lapho ucela ama-oda amaningi
  • Izinsizakalo ze-OEM / ODM: Ukunikezwa okuqondile kwasefekthri ngosekelo lwe-OEM/ODM lokwakheka ngokwezifiso
  • Ukutholakala Kwesampula: Amasampula okuhlola atholakalayo ukuze kuhlolwe ikhwalithi ngaphambi kokuthenga ngobuningi. Xhumana nethimba lethu labadayisi ukuze ucele amasampula e-High Penetration Epoxy yamaSlabs Emabula Emazingeni Okushisa Aphezulu (38-45°C)
  • I-Factory Direct Supply: Njengabahlinzeki nabakhi be-China abaqeqeshiwe, sinikeza amanani ancintisanayo, ukunikezwa okuthembekile, nokulawulwa kwekhwalithi okuzinzile kwama-oda amaningi.
  • Izimo Zokugcina: Gcina endaweni epholile, eyomile ekude nelanga eliqondile ku-10°C kuya ku-25°C
  • Isipiliyoni Sokuthekelisa: Sithumela emhlabeni wonke sinolwazi lokupakishwa kwamazwe ngamazwe kanye nempahla

Imibuzo Evame Ukubuzwa (FAQ)

Isetshenziselwa ini le epoxy?

A: Le High Penetration Epoxy ye-Marble Slabs in High Temperature (38-45°C) yakhelwe ama-slabs emabula anombala, ehlinzeka kokubili ukugcwaliswa kokuqhekeka nokuthuthukisa umbala endaweni yemabula ezindaweni ezishisayo.

Iliphi ibanga lokushisa elifanele le epoxy?

A: Le resin ye-epoxy yakhelwe ngokukhethekile ukuthi isebenze kahle emazingeni okushisa aphakathi kuka-38–45°C, okuyenza ifaneleke ezindaweni ezinezinga lokushisa eliphezulu.

Le epoxy ithuthukisa kanjani indawo yemabula enombala?

IMP: Le epoxy ingena ngokujulile ezindaweni ezinemibala yemabula, ithuthukisa umbala wemvelo, igcwalise imifantu, futhi inikeze isiphetho esihlala isikhathi eside, esibushelelezi, nesicwebezelayo ikakhulukazi ngezinhlobo zemabula ezinemibala.

Ingabe le epoxy kulula ukuyisebenzisa?

IMPENDULO: Yebo, le Epoxy Yokungena Okuphezulu Yezinsimbi Zemabula Ezingeni Lokushisa Eziphakeme (38-45°C) kulula ukuyixuba futhi isetshenziswe. Ayidingi amathuluzi akhethekile, iyenza ifaneleke kukho kokubili izinhlelo zokusebenza ezenziwa ngesandla nezizenzekelayo.

Kuthatha isikhathi esingakanani ukwelapha le epoxy?

A: Isikhathi sokuphulukisa cishe imizuzu engama-80 ku-38-45°C, kuye ngezimo zemvelo ezifana nezinga lokushisa kanye nomswakama.

Yiziphi izinhlobo zemabula le epoxy efanelekela zona?

A: Le epoxy yakhelwe ngokukhethekile imabula enombala, okuhlanganisa i-beige, epinki, eluhlaza, ephuzi, nezinye izinhlobo ezinemibala. Ihlukile kuma-epoxies akhelwe imabula emnyama, emhlophe, noma emnyama.

Iyini isilinganiso esinconyiwe sokuxuba?

A: Isilinganiso sokuxuba esinconyiwe ngu-100:25 (i-resin : i-hardener) ngesisindo.

Iyini i-viscosity yalesi simiso?

A: I-viscosity ingu-400-600 CPS, ihlinzeka ngokugeleza okuphelele kokungena okujulile emifantwini yemabula enemibala nezimbotshana.

Ingabe uyimboni noma inkampani yokuhweba?

A: Singumkhiqizi ochwepheshe kanye nefekthri ezinze e-China, ochwepheshe bezinhlelo ze-epoxy zokusetshenziswa kwamatshe. Njengabahlinzeki be-China abaqondile, sinikezela ngokuhlinzekwa okuqondile kwasefekthri, izinsizakalo ze-OEM, nezixazululo ezenziwe ngokwezifiso zama-oda amaningi emhlabeni jikelele.

Ingabe uyawahlinzeka ngamasampula okuhlolwa?

IMPENDULO: Yebo, sinikeza amasampula e-High Penetration Epoxy yethu yamaSlabs Emabula Ezinga Lokushisa Eliphezulu (38-45°C) ukuze kuhlolwe ikhwalithi. Sicela uxhumane nethimba lethu labadayisi ngezidingo zakho, futhi singakuhlelela ukuthunyelwa kwesampula ukuze uhlole ukusebenza kwezinto zakho zemabula ezinombala ezimweni ezishisa kakhulu.

Inothi lokugcina / Ukuthathwa Okusebenzayo: Le Epoxy Yokungena Okuphezulu Kwezingqimba Zemabula Ezingeni Lokushisa Eziphakeme (38-45°C) iletha imiphumela yezinga lochwepheshe yezicelo zemabula ezinemibala ezindaweni ezishisayo. Ngefomula yokugeleza okuphezulu, ukungena okujulile, ukuphulukiswa okuzinzile ku-38-45°C, kanye nokuthuthukiswa kombala okuhle kakhulu, iqinisekisa ukulungiswa okusebenzayo kokuqhekeka nokubuyiselwa kwendawo okuhlala isikhathi eside ikakhulukazi ezinhlobonhlobo zemabula ezinemibala. Njengabahlinzeki nabakhi be-China abangochwepheshe, sinikeza amanani aqondile embonini, ukutholakala kwesampula, nokwenza ngokwezifiso ama-oda ayinqwaba. Xhumana nathi namuhla ukuze uthole amasampula noma amanani entengo ye-premium High Penetration Epoxy ye-Marble Slabs in High Temperature (38-45°C).