I-Epoxy Resin yokugcwalisa imingxuma encinci kwiTravertine

I-Epoxy Resin Sealant sisisombululo esikhethekileyo, esine-viscosity ephezulu yokutywina eyenzelwe ukujongana neemfuno ezizodwa zemiphezulu yeTravertine ene-porous. Ingena nzulu kwiintanda kunye neepores, idala itywina elomeleleyo elihlala ixesha elide nelithembekileyo. Le mveliso ye-eco-friendly kulula ukuyisebenzisa, ayifuni zixhobo zikhethekileyo, kunye nokunyanga ukwenza umqobo oqinileyo ngokuchasene nokuphuma kwamanzi. Ngokujolisa kukhuseleko lomsebenzisi kunye noxanduva lokusingqongileyo, isitywini sethu lolona khetho lufanelekileyo lokugcina imfezeko kunye nomtsalane wobuhle bezakhiwo zeTravertine.

Iinkcukacha

UphawuI-Epoxy Resin yeGranite
  
  
  
  
  
  

I-Epoxy Resin Sealant yeTravertine

I-Epoxy Resin  yeTravertine sisixhobo sokutywina esisebenza ngokuphezulu eyilelwe ngokukodwa amatye arhabaxa njengeTravertine. Ingena ngokufanelekileyo kwiintanda kunye neepores edwaleni, yenza i-sealant layer eqinile emva kokunyanga, efezekisa umphumo ohlala ixesha elide kunye nothembekileyo wokuthintela amanzi. Le mveliso ibonakalisa i-viscosity ephezulu, ukunyanzeliswa komphezulu ophantsi, kunye nesakhono sokungena esigqwesileyo, siqinisekisa usetyenziso olusebenzayo kwiindawo ezahlukeneyo zeTravertine.

Iimpawu zeMveliso:

Uphawu I-Epoxy Resin yeTravertine
Esebenzayo mi-aterial Travertine
Ikhowudi yenkqubo ye-epoxy TL4090BF+TLB25Q-KG
Umlinganiselo wenkqubo ye-epoxy 100:25
Ukunyanga eisiphumo Yenza umaleko wokutywina osemi-oluqilima
Ukuqina Ukuzinza okuphezulu kunye nexesha elide emva kokunyanga
Ukusebenziseka lula Kulula ukuxuba kunye nokusebenzisa, akukho zixhobo zikhethekileyo ezifunekayo
Ukusebenziseka lula Kulula ukuxuba kunye nokusebenzisa, akukho zixhobo zikhethekileyo ezifunekayo
Ubuhlobo bendalo IiCompounds ze-Volatile Organic (VOC), eco-friendly

Imiyalelo yokusebenzisa:

  1. Coca umphezulu weTravertine ukuze uqinisekise ukuba aluthuli kwaye alunaoli.
  2. Hlanganisa i-epoxy resin kunye ne-hardener kumlinganiselo ochazwe kwimiyalelo.
  3. Sebenzisa isixhobo esikhethekileyo ukutofa i-epoxy resin edibeneyo kwiintanda kunye neepores zeTravertine.
  4. Vumela i-epoxy resin ukuba iphile ngokupheleleyo, edla ngokuthatha iiyure ezingama-24.
  5. Emva kokunyanga, ukuba kuyimfuneko, isanti kwaye ucoce umphezulu.

Izilumkiso:

  • Sebenzisa le mveliso kwindawo engena umoya.
  • Gcina kwindawo ekude nabantwana kunye nezilwanyana zasekhaya.
  • Funda incwadi yemveliso ngononophelo phambi kokuba uyisebenzise.

Imiba yokuPakisha:

  • I-25 kg yesikhongozeli
  • I-200 kg yesikhongozeli
  • I-1000 kg yesikhongozeli

Ubomi beShelf:

  • Iinyanga ezili-12 xa zingavulwa.

Imiqathango yoGcino:

  • Gcina kwindawo epholileyo, eyomileyo, nengena umoya kakuhle, kude nomlilo namaqondo obushushu aphezulu.

Ngale ntshayelelo, unokuqonda ngokupheleleyo iimpawu zemveliso kunye neendlela zokusetyenziswa kwe-Epoxy Resin Sealant yeTravertine. Sizimisele ukubonelela ngeemveliso ezikumgangatho ophezulu ukuhlangabezana neemfuno zakho zokugcinwa nokulungiswa kweTravertine.