UV-stabilized epoxy resin for marble coatings
- Feature: Epoxy Resin for hard white Marble
- Applicable material: Calacatte , Stuario, Carrara White
- Epoxy system code: 5099-YC +D30M-BS
- Epoxy system ratio by weight: 100:30
- Curing effect: Forms a liquid sealing layer
Overview
Veropoxy, a top company for twelve years, specializes in manufacturing and selling epoxy resins and hardeners, primarily liquid blue epoxy resins, providing quality solutions for municipalities, gardens, squares, and hotels.
Product Description
Veropoxy: A unique epoxy resin
For twelve years, Veropoxy is a top company specializing in the manufacture and sale of epoxy resins and hardeners. Committed to providing quality solutions to customers. Our product range is based on epoxy resins, mainly liquid blue epoxy resins. During the curing process, this special blue liquid can provide excellent visual effects and performance. Veropoxy’s products can be used precisely in municipalities, gardens, squares or hotel areas, with excellent performance and attractive appearance.

Product Features
| Feature | Epoxy Resin for hard white Marble |
|---|---|
| Applicable material | Calacatte , Stuario, Carrara White |
| Epoxy system code | 5099-YC +D30M-BS |
| Epoxy system ratio by weight | 100:30 |
| Curing effect | Forms a liquid sealing layer |
| Durability | High stability and long-lasting after curing, good yellowing resistance, low viscosity, strong bonding |
| Ease of Use | Easy to mix and apply, no special tools required |
Application of epoxy resin to marble slabs
It greatly enhances the decorative effect of marble in addition to its physical qualities, including increase of its impact and durability against cracks. By means of epoxy’s penetration and curing, the minute cracks and pores on the surface of marble may be sufficiently filled, thereby mitigating the entrance of moisture and stains and enhancing the slab’s anti-pollution capacity. Furthermore improving the application value of epoxy resin in the field of high-end decorating are its great gloss and color stability, which help marble slabs to exhibit more vivid and enduring hues after epoxy treatment. Marble’s service life is extended by this mix of elements, which also increase its popularity in contemporary architecture and interior design.
Epoxy instructions
See the Material Safety Data Sheet (MSDS) to learn its chemical composition and potential hazards before applying epoxy; also, store carefully following recommendations. First, the surface to be used has to be meticulously cleaned and sanded to guarantee firm adhesion of epoxy.
To prepare the epoxy, precisely weigh the resin and hardener in line with the manufacturer’s mixing ratio; gently stir in a dry, clean container until the color is homogeneous. Good ventilation should be ensured and skin and eye contact should be avoided during the mixing procedure.
Equally cover the treatment area with the mixed epoxy; then, let it cure for the designated period. The curing time can be influenced by the kind of epoxy and ambient elements including temperature and humidity.
Wear suitable personal protective equipment (gloves, masks, goggles) all through the process to guard the respiratory tract and skin. Furthermore make sure the workspace has enough ventilation to help lower the harmful gas collection.
Clean tools right away after use; store any extra epoxy in a sealed container as advised by the manufacturer. Local environmental rules should direct garbage and used containers on appropriate disposal.
Epoxy Resin Storage
Epoxy resin should be kept dry, cool, well-ventilated inside away from direct sunlight and high temperature surroundings. Usually ranging from 15℃ to 25℃, the appropriate storage temperature controls relative humidity between 40% and 60%.
Epoxy should be kept in a corrosion-resistant, well-sealed container to avoid it coming into touch with moisture, air, other materials.Clearly visible safety signs containing flammable, poisonous, and corrosive warnings should be found in storage spaces.
Epoxy is a flammable substance hence storage of it should be done with consideration for fire prevention. Store epoxy glue away from flammable objects or near a fire source to stop fire starting.
Steer clear of sunlight since long-term exposure of epoxy resin will compromise its performance and quality. Epoxy should thus be kept dark and stay away from direct sunshine.
Usually with a set shelf life, epoxy resin may change in performance once the shelf life expires. Thus, you should investigate the shelf life of epoxy resin and aim to use it within that range before applying it.
Usually supplied in sealed containers, epoxy resin is packaged and sealed; so, unused resin should be kept in a sealed container. Make sure the container is well closed after opening the packaging so the resin won’t absorb moisture or cure from air’s contact.