Epoxy idafite umuhondo kuri marble yera yera - 5090 / D30M-BS

Epoxy itari Umuhondo kuri Hard Marble Yera - 5090 / D30M-BS sisitemu. Umuhondo muke cyane, kugenzura kwinjira, hamwe nigihe kirekire cyamabara. Umuti wiminota 80, 400-600 CPS viscosity. Icyiza cyo hejuru-marble yera yo gusana, gushimangira, hamwe nimishinga yubwubatsi. Ubushinwa. Ingero zirahari.

Ibisobanuro

IkirangaEpoxy Resin ya Granite
  
  
  
  
  
  
Incamake yihuse: Epoxy idafite umuhondo kuri Hard White Marble yagenewe cyane cyane porogaramu ya marble yera, itanga umuhondo muke cyane, igenzurwa, hamwe nigihe kirekire cyamabara. Nibyiza cyane murwego rwohejuru rwo gutunganya amabuye no gushimangira aho ubuziranenge bwibonekeje nigihe kirekire ari ngombwa.

Epoxy itari Umuhondo kuri Hard Marble Yera | Abashinwa batanga ibicuruzwa

Epoxy yacu idafite umuhondo kuri Hard White Marble nigihe kirekire-kitari umuhondo epoxy resin sisitemu yatunganijwe byumwihariko kubikorwa bya marble yera. Iyi Non-Umuhondo Epoxy ya Hard White Marble itanga amabara meza atuje, imikorere yumuhondo muke cyane, hamwe no gukomera kuramba mugihe. Sisitemu ituma igenzurwa ryinjira nta kurenza urugero, kugumana isuku karemano nubucyo bwa marble yera. Nka bayobozi bambere batanga Ubushinwa nababukora, dutanga ibiciro-byinganda-hamwe nibisubizo byabigenewe kubicuruzwa byinshi kwisi yose.

Urashaka Epoxy nziza idafite Umuhondo kuri Hard White Marble kubatanga Ubushinwa bwizewe? Sisitemu yacu 5090 / D30M-BS igaragaramo umuhondo muke cyane kandi muremure wigihe kirekire kumurongo wimishinga yohejuru ya marble yera. Nibyiza kubisate byera byera bya marble gusana, gushimangira, hamwe nuburyo bwububiko, iyi formulaire itanga igenzurwa ryinjira hamwe nubukanishi buhebuje. Utunganye hejuru ya marble yera isaba igihe kirekire.

Ibisobanuro ku bicuruzwa

Epoxy idafite umuhondo kuri Hard White Marble ni sisitemu ndende-idafite umuhondo epoxy resin sisitemu yakozwe cyane cyane kubikorwa bya marble yera. Itanga amabara meza cyane, imikorere yumuhondo muke cyane, hamwe no gushimangira igihe kirekire. Sisitemu ituma igenzurwa ryinjira nta kurenza urugero, kugumana isuku karemano nubucyo bwa marble yera. Iyi Non-Umuhondo Epoxy ya Hard White Marble yateguwe kugirango itunganyirizwe hejuru-amabuye aho gutunganya neza no kumara igihe kirekire ari ngombwa.

 

Umwuga-2-intambwe-epoxy-kuri-ikomeye-granite

Ibiranga ibicuruzwa & Ibisobanuro

Ikiranga Ibisobanuro
Ikiranga Epoxy idafite umuhondo resin ya marble yera ikomeye
Ibikoresho Marble Yera
Epoxy Sisitemu Kode 5090 / D30M-BS
Ikigereranyo cya Epoxy 100: 30
Kuramba Ihungabana ryinshi nibikorwa birebire nyuma yo gukira
Kuborohereza gukoreshwa Biroroshye kuvanga no gushyira mubikorwa, nta bikoresho byihariye bisabwa
Gukiza Igihe Iminota 80
Kurwanya Umuhondo Umuhondo muke cyane
Basabwe gukora Ubushyuhe 24 ° C.
Viscosity 400-600 CPS

Ibibazo bikemura

  • Ibibazo byumuhondo bikunze kuboneka muri epoxy yera ya marble yera - Epoxy yacu idafite umuhondo kuri Hard White Marble irinda ibara.
  • Gutakaza urumuri hejuru nyuma yo gukira igihe kirekire - Igumana isura yera ya marble yera
  • Kuramba bidahagije murwego rwohejuru rwera rwa marble ishimangira - Itanga imashini iramba
  • Guhindura amabara munsi yubushyuhe bwo murugo - Imikorere ihoraho mubihe bitandukanye

Gusabwa

  • Icyuma cyera cya marble gisana gusana no gushimangira ukoresheje Epoxy idafite Umuhondo kuri Hard White Marble
  • Hejuru-yububiko bwububiko bwera marble imishinga isaba amabara maremare
  • Ibara ryera rya marble yera aho bigaragara neza nubucyo birakomeye
  • Uruganda n'amahugurwa resin yo kuvura imirongo yo gutunganya premium marble
  • Inzu ndangamurage-nziza ya marble yubatswe no kugarura

Ibyiza byingenzi byimikorere

  • Umuhondo muke cyane kubwigihe kirekire cyiza gihamye - Igisobanuro kiranga Epoxy yacu itari Umuhondo kuri Hard White Marble
  • Gukorera mu mucyo no gusobanuka nyuma yo gukira
  • Kwihangana gukomeye hamwe nubukanishi bwigihe
  • Kugenzura kwinjirira bikwiranye na marble ikomeye idakabije
  • Iminota 80 yo gukiza igihe cyo gukora neza
  • 400-600 CPS viscosity yo kugenzura neza porogaramu
  • Uruganda rutanga isoko: Nkuyobora ibicuruzwa bitanga Ubushinwa, dutanga ibiciro byapiganwa kandi byizewe kuboneka

Sisitemu Ibicuruzwa Ibisobanuro

Epoxy idafite umuhondo kuri Hard White Marble ikomatanya uburyo bwa resin yateye imbere hamwe na injeniyeri yabugenewe kugirango habeho umuhondo muke cyane kandi uhamye neza. Sisitemu idafite imbaraga kandi yashizweho kugirango igumane imikorere ihamye mugihe cyo gukiza nubuzima bwa serivisi. 5090 resin hamwe na D30M-BS ikomera ikora sisitemu yuzuye ya epoxy sisitemu igenzurwa na reaction hamwe nigikorwa cyo gukiza kimwe, cyanonewe cyane cyane kubikorwa bya marble yera yera aho isura nuburinganire byubatswe ari ngombwa.

Gutunganya ibyifuzo

  1. Menya neza ko hejuru ya marble isukuye, yumye, kandi nta mukungugu cyangwa umwanda mbere yo gukoresha iyi Epoxy itari Umuhondo kuri Hard White Marble
  2. Kuvanga ibice neza ukurikije igipimo cya 100: 30
  3. Koresha neza ukoresheje brush, roller, cyangwa ibikoresho bisanzwe bya resin
  4. Emera gukira kwuzuye (hafi iminota 80) mugihe cy'ubushyuhe butajegajega hafi 24 ° C.
  5. Komeza ubushyuhe bwibidukikije burigihe mugihe cyo gukiza ibisubizo byiza
  6. Sukura ibikoresho ako kanya nyuma yo gukoreshwa mbere yuko epoxy ikira

Icyangombwa: Gukurikiza ibi bitekerezo byo gutunganya byerekana neza imikorere ya Epoxy yawe itari Umuhondo kuri Hard White Marble itangwa nabashinwa babigize umwuga.

Ubwoko bubuye bwamabuye

  • Marble yera ikomeye - Ubwoko bwose burimo Calacatta, Statuario, na Carrara marble yera
  • Imiterere ya marble yuzuye ya kirisiti - Irakwiranye na comptabilite, yuzuye-marike yera ya marble
  • Hejuru-yera yera ya marble isaba amabara ahamye - Ideal ya premium stone amanota

Icyitonderwa: Iyi Epoxy itari Umuhondo kuri Hard White Marble itezimbere kubikorwa byera bya marble. Kuri marble yoroshye, sisitemu yihariye yo kwinjira-irasabwa. Gerageza kumwanya muto ubanze ugenzure guhuza nibikoresho byawe byihariye.

Gupakira & Gutanga

  • Gupakira bisanzwe: Biraboneka muburyo bwo gupakira inganda kubikoresho byo gutunganya amabuye
  • Gupakira ibicuruzwa: Amahitamo menshi yo gupakira aboneka kubikorwa binini
  • Serivisi za OEM / ODM: Guhitamo ibicuruzwa hamwe na label yihariye ishyigikiwe
  • Icyitegererezo Kuboneka: Icyitegererezo cyibizamini biboneka kugirango bisuzumwe ubuziranenge mbere yo kugura byinshi. Menyesha itsinda ryacu ryo kugurisha kugirango usabe ingero za Epoxy itari Umuhondo kuri Hard White Marble
  • Uruganda rutanga amasoko: Nkabashinwa babigize umwuga nabatanga ibicuruzwa, dutanga ibiciro byapiganwa, amasoko yizewe, hamwe nubuziranenge buhamye kubicuruzwa byinshi
  • Uburyo bwo kubika: Bika ahantu hakonje, humye kure yizuba ryinshi kuri 10 ° C kugeza 25 ° C.
  • Uburambe bwo kohereza hanze: twohereza ku isi yose dufite uburambe mubipfunyika mpuzamahanga n'ibikoresho

Ibibazo Bikunze Kubazwa (Ibibazo)

Iyi epoxy irakwiriye yoroshye ya marble yera?

Igisubizo: Iyi Epoxy itari Umuhondo kuri Hard White Marble itezimbere kuri marble yera ikomeye. Kuri marble yoroshye, sisitemu yihariye yo kwinjira-irasabwa kwirinda gukabya.

Ese resin yumuhondo mugihe runaka?

Igisubizo: Oya. Sisitemu yateguwe hamwe nibiranga umuhondo muke cyane kugirango ibungabunge amabara maremare kandi ibungabunge ubwiza nyaburanga bwa marble yera.

Irashobora gukoreshwa mumurongo wibyakozwe?

Igisubizo: Yego. 400-600 ya CPS yuzuye kandi igenzura imyitwarire ikiza ituma iyi Epoxy itari Umuhondo kuri Hard White Marble ikwiranye na sisitemu yo gutunganya intoki kandi zikoresha.

Ni ikihe kigereranyo cyo kuvanga?

Igisubizo: Ikigereranyo cyo kuvanga ni 100: 30 (resin: gukomera) kuburemere.

Gukiza bifata igihe kingana iki?

Igisubizo: Igihe cyo gukira ni iminota 80 mugihe wasabwe kuri 24 ° C.

Ni ubuhe bwenge bw'iyi sisitemu?

Igisubizo: Ubukonje ni 400-600 CPS, butanga kwinjira byinjira muburyo bukomeye bwa marble yera idakabije.

Ni ubuhe bushyuhe busabwa gukoreshwa?

Igisubizo: Ubushyuhe bwo gukora busabwa ni 24 ° C kugirango ukire neza kandi ukore neza.

Waba uruganda cyangwa uruganda rwubucuruzi?

Igisubizo: Turi uruganda rukora uruganda rukora mubushinwa, kabuhariwe muri sisitemu ya epoxy yo gukoresha amabuye. Nkabatanga Ubushinwa butaziguye, dutanga ibicuruzwa bitaziguye, serivisi za OEM, hamwe nibisubizo byabigenewe kubicuruzwa byinshi kwisi yose.

Utanga ingero zo kwipimisha?

Igisubizo: Yego, turatanga ingero za Epoxy yacu itari Umuhondo kuri Hard White Marble yo gupima ubuziranenge. Nyamuneka hamagara itsinda ryacu ryo kugurisha hamwe nibisabwa, kandi turashobora gutegekanya ibicuruzwa byoherejwe kugirango dusuzume imikorere kubikoresho byawe bya marble yera.

Ni ubuhe buryo ntarengwa bwo gutumiza (MOQ) bwo gutanga ibicuruzwa bitaziguye?

Igisubizo: MOQ yacu iroroshye bitewe nibicuruzwa byihariye. Kuri iyi Epoxy itari Umuhondo kuri Hard White Marble, turashobora kwakira ibyateganijwe bito hamwe nibicuruzwa byinshi byoherejwe. Nkabatanga Ubushinwa butaziguye, dukorana nawe kugirango wuzuze ibisabwa.

Icyitonderwa cya nyuma / Gufata ibyemezo: Iyi Non-Umuhondo Epoxy ya Hard White Marble itanga ibisubizo-byumwuga ibisubizo byanyuma-byera byera bya marble. Hamwe n'umuhondo muke cyane, ugenzurwa no kwinjira, kuramba kwigihe kirekire, hamwe nubukorikori buhebuje, butuma ubuziranenge busanzwe nubwiza bwimiterere ya marble yera bibikwa kumyaka. Nkabashinwa babigize umwuga batanga ibicuruzwa nuwabikoze, dutanga ibiciro-bitaziguye byinganda, icyitegererezo kiboneka, hamwe no kugenera ibicuruzwa byinshi. Twandikire uyumunsi kuburugero cyangwa kugiciro cyibiciro bya premium yacu Yumuhondo Epoxy ya Hard White Marble.