Marble Slabs Epoxy Resin Decorative Furniture Countertops Polished Floor Tiles Finishes
- Feature: Epoxy Resin for Gray Marble
- Applicable material: Diano Real Gray Marble,Venetian Brown
- Epoxy system code: 4099+B25Q-KG
- Epoxy system ratio by weight: 100:25
- Curing effect: Forms a liquid sealing layer
Overview
Epoxy resin is a high-strength, hard, and fast curing material suitable for various paving projects, stone repair, bonding positioning, and filling. It offers good adhesion, resistance to external impact, and a natural stone luster after polishing.
Product Description
Epoxy resin has the characteristics of high strength, high hardness, fast curing speed and stable storage. It is suitable for all kinds of paving projects and all kinds of stone repair, bonding positioning and filling. It has good adhesion and resistance to external impact, is easy to operate, and has the luster of natural stone after polishing. It can be selected for stones of different colors.
Product Features:
Feature | Epoxy Resin for Gray Marble |
Applicable material | Diano Real Gray Marble,Venetian Brown |
Epoxy system code | 4099+B25Q-KG |
Epoxy system ratio by weight | 100:25 |
Curing effect | Forms a liquid sealing layer |
Durability | High stability and long-lasting after curing,good yellowing resistance , low viscosity , strong Bonding |
Ease of Use | Easy to mix and apply, no special tools required |
Epoxy resin for marble
Epoxy resin performs well in marble repair and reinforcement, and is suitable for occasions where broken and damaged boards need to be re-bonded. Epoxy resin has the characteristics of high strength, slow curing, and full penetration. It can cure within 25 hours at room temperature or 1 hour in a 40°C drying oven. It can reach 100% of its maximum strength after full hardening. In addition, epoxy resin adhesives have extremely high adhesion to most building materials and are suitable for bonding marble to metal, concrete and other bases. It has super strength and ability
The application steps of epoxy resin in stone processing are as follows:
First, place the large board on the glue repair trolley or glue repair line, and ensure that the surface to be sanded is facing up. For large boards with severe cracks, repairs are required and reinforcement may be used with steel bars, aluminum bars or plastic bars. Next, clean the surface to be sanded and ensure that it is dry and dust-free to remove any substances that may affect the adhesion of epoxy resin.
Then, choose a suitable fiber mesh according to the area of the large board. The size of the fiber mesh should be 60mm smaller than the length and width of the large board. When mixing epoxy resin glue, mix according to the proportion of A and B components on the instructions, and use a mixer to ensure uniform mixing. Scrape the prepared epoxy resin glue evenly on the surface of the stone and the fiber mesh, ensuring that the colloid completely covers the mesh.
Then, evenly sprinkle the marble sand that meets the requirements on the surface of the epoxy resin glue. The large board after sanding needs to be cured by natural drying or drying. After the epoxy resin glue on the sanding surface is completely dry, the board is collected to prevent sand particles from falling off and offset printing.
Add a plastic film between the sanding surface and the front of the slab to prevent the sand from rubbing against the front of the stone. Pack or stack the sanded slabs in turns. Finally, cut the sanded slabs that need to be processed, and use spacers to protect the front of the product from being scratched by sand.
These steps describe the use of epoxy resin in stone processing in detail, from preparation to final processing, ensuring that epoxy resin can be effectively used for stone repair and enhancement.
Benefits of using epoxy resin for marble slabs
Epoxy resin brings significant benefits in the application of marble slabs. First, it acts as a strong adhesive that ensures a strong connection between marble slabs, thereby improving the stability and durability of the structure. The permeability of epoxy resin helps fill the tiny cracks in the marble and prevents the cracks from expanding, enhancing the overall crack resistance of the slab. In addition, its excellent waterproof performance can prevent moisture penetration and reduce damage caused by moisture.
Epoxy resin is also chemically resistant and can protect marble from the erosion of chemicals such as acid rain and detergents. Its wear resistance also helps to reduce the wear and tear of marble in daily use. The flexibility of epoxy resin allows it to adapt to the slight deformation of marble caused by temperature changes, thereby reducing damage caused by stress concentration.
In terms of construction, epoxy resin is easy to mix and apply, and its consistency can be adjusted as needed, making it simple to apply on marble slabs. Epoxy resin also provides a variety of color options, which can match the natural tone of marble or be used to create unique decorative effects.
The easy cleaning and maintenance of epoxy resin coatings help to maintain the beauty of marble and extend its service life. In addition, epoxy resin can also improve the mechanical strength of marble, making it more durable. Finally, the environmental adaptability of epoxy resin makes it an ideal choice for indoor and outdoor marble applications, able to maintain performance in a variety of environmental conditions.
Precautions:
Use this product in a well-ventilated area.
Keep out of reach of children and pets.
Read the product manual carefully before use.
Packaging Specifications:
1 kg container
5 kg container
Shelf Life:
12 months when unopened.
Storage Conditions:
Store in a cool, dry, and well-ventilated area, away from fire and high temperatures.
With this introduction, you can fully understand the product features and usage methods of the Epoxy Resin Sealant for Marble. We are committed to providing high-quality products to meet your needs for the maintenance and repair of Marble.