Manufacturers wholesale epoxy resin adhesive quick fix stone countertop adhesive marble glue

  • Feature: Epoxy Resin for Purple Marble
  • Applicable Material: Purple Marble, Amethyst, Royal Purple
  • Epoxy System Code: 4099+B25Q-KG
  • Epoxy System Ratio by Weight: 100:25
  • Curing Effect: Forms a liquid sealing layer
INQUIRY

Overview

Epoxy provides excellent protection and enhancement. It enhances marble’s abrasion and chemical resistance while highlighting its grain and color. Easy to apply and fix, Veropoxy enhances the beauty and durability of marble, making it ideal for interior design and furniture construction. Choose Veropoxy for professional-grade epoxy protection and the beauty of your marble slab project.

Product Description

Product Definition

 

Veropoxy is a premium two-component epoxy adhesive brand manufacturer, formulated specifically for marble slabs, providing unparalleled protection and enhancement for the natural stone. This epoxy adhesive provides a strong protective layer, significantly improving the abrasion and chemical resistance of marble, while highlighting the original veins and colors of the marble through its superior clarity and gloss. Easy to apply and fix to smooth surfaces, the epoxy not only enhances the beauty of the marble, but also significantly improves its durability. Ideal for interior design and furniture manufacturing, Veropoxy will bring a modern and lasting appeal to marble slabs. Choose Veropoxy for professional-grade epoxy protection and beauty for your marble slab project.

 

Product Features:

 

Feature Epoxy Resin for Purple Marble
Applicable Material Purple Marble, Amethyst, Royal Purple
Epoxy System Code 4099+B25Q-KG
Epoxy System Ratio by Weight 100:25
Curing Effect Forms a liquid sealing layer
Durability High stability and long-lasting after curing, good yellowing resistance, low viscosity, strong bonding
Ease of Use Easy to mix and apply, no special tools required

 

Advantages:

 

—-100% curable at room temperature or under heating.

—-High gloss, transparent, impact resistant, waterproof, self-leveling.

—-Will not turn yellow when exposed to sunlight for a long time.

—-Simple operation; excellent air release.

Early development of performance and physical properties

—-No ripples, bright surface, odorless, eco-friendly, non-toxic, waterproof, etc.

—-Easy to repair and clean.

 

Application areas

 

This epoxy resin is mainly used in the stone industry, such as the installation and repair of high-end materials such as marble, granite, and quartz. Due to its high strength, Vero Bond Epoxy resin is not only suitable for stone splicing in home decoration, but also widely used in stone installation in outdoor buildings. Whether it is kitchen countertops, bathroom walls, or outdoor stone decoration, this epoxy resin can provide excellent bonding effect.

Operation

 

1.Weigh A and B glue according to the given weight ratio into the prepared cleaned container, fully mixed the mixture again the container wall by clockwise, place it along for 3 to 5 minutes, and then it can be used.

 

2.Take the glue according to the usable time and dosage of mixture to avoid wasting. When the temperature is below 15 ℃, please heat A glue to 30 ℃ first and then mix it to the B glue (A glue will be thicken in low temperature ); The glue must be sealed lid after use to avoid rejection caused by moisture absorption.

 

3.When the relative humidity is higher than 85%, the surface of the cured mixture will absorb moisture in the air, and form a layer of white mist in the surface, so when the relative humidity is higher than 85%, is not suitable for room temperature curing, suggest to use the heat curing.

 

Precautions

 

When using Vero Bond Epoxy resin, be careful to avoid direct contact with skin and eyes, and keep the workplace well ventilated. After use, the remaining adhesive should be sealed in time to prevent air from entering and causing curing failure. At the same time, mix strictly according to the proportion to ensure the best bonding effect.

 

If you are looking for a high-performance bonding solution, then Vero Bond Epoxy resin is definitely a reliable choice. Its exceptional adhesion, weather resistance, chemical corrosion resistance, environmental protection and safety make it an ideal adhesive for all kinds of stone and composite materials.

marble

 

Store epoxy resin

 

Stored in a dry, cold, well-ventilated room, epoxy resin should avoid direct sunlight and high temperature environment. Usually ranging from 15 to 25 degrees Celsius, the suitable storage temperature controls the relative humidity between 40 and 60%.

 

Stored in corrosion-resistant, well-sealed containers, epoxy resin should prevent coming into touch with moisture, air, or other materials. Safety signs with flammable, poisonous, and corrosive warnings should be obviously visible in the storage area.

 

Since epoxy glue is combustible, storage of it should take fire prevention into account. To stop fire, store epoxy glue far from flammable objects or fire sources.

 

Steer clear of sunlight since long-term epoxy resin performance and quality will suffer. Epoxy glue ought so to be kept dark and away from direct sunshine.

 

Usually with a fixed shelf life, epoxy resin may operate differently if the shelf life runs out. Consequently, you should look into the shelf life of epoxy resin and aim to apply it within this range before usage.

 

Usually packed in sealed containers, epoxy resins should be sealed; so, unused resin should be kept in sealed containers. Make sure the container is tightly sealed following package opening so the resin does not absorb moisture or cure from contact with air.

Why Marble

Get A Free Quote
Contact us for free quotes and more professional knowledge about product. We will prepare a professional solution for you.


    Leave Your Message

      * Name

      * Email

      Phone/WhatsAPP/WeChat

      * What I have to say