Color Enhancing Epoxy for Light Granite | China Suppliers & Manufacturer
Our Color Enhancing Epoxy for Light Granite is a high-performance epoxy system specifically designed for light granite applications. This Color Enhancing Epoxy for Light Granite features a low-viscosity formulation that penetrates deep into the granite, filling micro-cracks while improving the color and surface appearance of the stone. This epoxy provides a smooth, seamless finish without altering the natural texture of the granite. The epoxy’s enhanced color depth and uniformity make it ideal for use in both commercial stone processing and DIY projects, ensuring long-lasting results with high stability after curing. As leading China suppliers and manufacturer, we provide factory-direct pricing and customized solutions for bulk orders worldwide.
Looking for the best Color Enhancing Epoxy for Light Granite from reliable China suppliers? Our 4099-BBS/D30M-BS system features low viscosity for deep penetration into micro-cracks and pores, enhancing the natural color of light granite without altering its appearance. Ideal for light granite slab crack repair, color enhancement, and surface restoration before polishing. Perfect for both commercial stone processing and professional finishing applications.
Product Description
Color Enhancing Epoxy for Light Granite is a high-performance epoxy system specifically designed for light granite applications. It features a low-viscosity formulation that penetrates deep into the granite, filling micro-cracks while improving the color and surface appearance of the stone. This epoxy provides a smooth, seamless finish without altering the natural texture of the granite. The epoxy’s enhanced color depth and uniformity make it ideal for use in both commercial stone processing and DIY projects, ensuring long-lasting results with high stability after curing.

Product Features & Specifications
| Feature | Description |
|---|---|
| Feature | High-flow, color-enhancing, low-viscosity epoxy for light granite |
| Applicable Material | Light granite, dense granite with micro-cracks |
| Epoxy System Code | 4099-BBS / D30M-BS |
| Epoxy System Ratio | 100 : 30 |
| Durability | High stability and long-lasting after curing |
| Ease of Use | Easy to mix and apply, no special tools required |
| Curing Time | 80 minutes |
| Yellowing Resistance | High |
| Temperature | 24°C |
| Viscosity | CPS 400-600 |
Problems It Solves
- Micro-cracks in light granite slabs – Our Color Enhancing Epoxy for Light Granite penetrates deep to fill and repair
- Uneven color or tone in light-colored granite surfaces – Enhances and evens out natural color
- Weak adhesion and poor internal bonding after crack repair – Creates strong, durable bonds
- Visible repair marks caused by insufficient penetration of traditional epoxies – Seamless integration with no visible痕迹
Recommended Applications
- Light granite slab crack repair using Color Enhancing Epoxy for Light Granite
- Granite color enhancement before polishing for uniform appearance
- Deep penetration treatment for dense granite materials with micro-cracks
- Stone finishing and surface restoration projects
- Granite slab pre-treatment before surface finishing operations
Key Performance Advantages
- Low viscosity for deep penetration into micro-cracks and stone pores – Ensures thorough repair and enhancement
- Enhances the natural color of light granite without altering its appearance or texture
- High stability and long-lasting results after curing for durable performance
- Seamless crack filling with no tactile difference after polishing
- Easy to apply with no need for special tools, suitable for both manual and automated lines
- 80-minute curing time for efficient production workflow
- High yellowing resistance for long-term color stability
- Factory Direct Supply: As leading China suppliers, we offer competitive pricing and reliable availability
Product System Description
The product is a two-component epoxy resin system, composed of:
Component A: 4099-BBS
Component B: D30M-BS
This Color Enhancing Epoxy for Light Granite is designed for light granite applications, providing high-flow penetration and excellent color enhancement. Once mixed at the recommended 100:30 ratio, it forms a stable, durable bond that ensures effective repair and surface toning without compromising the stone’s natural aesthetics. The system delivers a smooth, seamless finish that integrates perfectly with light granite surfaces.
Processing Suggestions
- Clean cracks thoroughly and remove dust before applying this Color Enhancing Epoxy for Light Granite
- Mix components at the recommended ratio (100:30) for optimal performance
- Apply the epoxy evenly, ensuring full penetration into cracks and pores
- Allow sufficient time for deep penetration before curing (approximately 80 minutes at 24°C)
- Maintain ambient temperature around 24°C for optimal curing results
- Proceed with polishing or further surface treatment after curing is complete
- Clean tools immediately after use before epoxy cures
Important: Following these processing suggestions ensures optimal performance of your Color Enhancing Epoxy for Light Granite from professional China suppliers.
Suitable Stone Types
- Light granite – All varieties of light-colored granite including beige, cream, white, and gray tones
- Dense granite with micro-cracks requiring deep penetration repair
- Granite with high porosity needing color enhancement and stabilization
Note: This Color Enhancing Epoxy for Light Granite is specially formulated for light granite applications. Test on a small area first to verify compatibility with your specific granite type and application conditions.
Packaging & Supply
- Standard Packaging: Standard A/B epoxy packaging available for granite processing facilities
- Custom Packaging: Custom packaging options upon request for bulk orders
- OEM / ODM Services: Factory direct supply with OEM/ODM support for custom formulations
- Sample Availability: Test samples available for quality evaluation before bulk purchase. Contact our sales team to request samples of Color Enhancing Epoxy for Light Granite
- Factory Direct Supply: As professional China suppliers and manufacturer, we offer competitive pricing, reliable supply, and stable quality control for bulk orders
- Storage Conditions: Store in cool, dry place away from direct sunlight at 10°C to 25°C
- Export Experience: We ship worldwide with experience in international packaging and logistics
Frequently Asked Questions (FAQ)
Is this epoxy suitable for light granite?
A: Yes. This Color Enhancing Epoxy for Light Granite is specially designed for light granite, enhancing its color while providing seamless crack repair and deep penetration.
What is the curing time for this product?
A: The curing time is approximately 80 minutes at 24°C. Ensure the ambient temperature is consistent for optimal performance of this Color Enhancing Epoxy for Light Granite.
Does this epoxy yellow over time?
A: No, this epoxy has high resistance to yellowing, ensuring it maintains its clear finish even after prolonged exposure to light and air.
How do I apply this epoxy to granite?
A: This Color Enhancing Epoxy for Light Granite is easy to apply with basic tools like brushes or a roller. Simply mix the components at the 100:30 ratio and apply to the cracked or surface-treated granite.
Can this epoxy be used on all types of granite?
A: This epoxy is best suited for light granite but can also work on other dense granite materials with micro-cracks requiring deep penetration.
What is the recommended mixing ratio?
A: The recommended mixing ratio is 100:30 (resin : hardener) by weight.
What is the viscosity of this system?
A: The viscosity is 400-600 CPS, providing optimal flow for deep penetration into light granite micro-cracks and pores.
Does this epoxy enhance the natural color of light granite?
A: Yes, it enhances the natural color of light granite without altering its appearance or texture, providing even tone and depth.
Are you a factory or trading company?
A: We are a professional manufacturer and factory based in China, specializing in epoxy systems for stone applications. As direct China suppliers, we offer factory direct supply, OEM services, and customized solutions for bulk orders worldwide.
Do you provide samples for testing?
A: Yes, we provide samples of our Color Enhancing Epoxy for Light Granite for quality testing. Please contact our sales team with your requirements, and we can arrange sample shipment for you to evaluate the color enhancement performance on your light granite materials.