Low-Viscosity Epoxy Resin for Stone Vacuum Infusion – 5080/B25Q-KG High Penetration & Stable Curing

Low Viscosity Epoxy for Stone Vacuum Infusion with 5080/B25Q-KG system. 400-600 CPS viscosity ensures deep penetration and uniform impregnation. High yellowing resistance, stable curing in 3-5 hours. Ideal for marble, granite, and engineered stone reinforcement. China manufacturer. Samples available.

Specifications

FeatureEpoxy Resin for Granite
  
  
  
  
  
  
Quick Summary: Low-Viscosity Epoxy for Stone Vacuum Infusion is engineered for efficient resin flow and deep penetration in vacuum infusion processes. It delivers stable curing, high yellowing resistance, and long-term durability, making it ideal for professional stone reinforcement and composite stone production.

Low Viscosity Epoxy for Stone Vacuum Infusion | China Suppliers & Manufacturer

Our Low Viscosity Epoxy for Stone Vacuum Infusion is a specially formulated epoxy resin system designed to ensure excellent flowability and uniform impregnation under vacuum conditions. This Low Viscosity Epoxy for Stone Vacuum Infusion features controlled viscosity that allows deep penetration into stone structures, improving internal strength while maintaining visual clarity and long-term stability after curing. As leading China suppliers and manufacturer, we provide factory-direct pricing and customized solutions for bulk orders worldwide.

Product Description

Low-Viscosity Epoxy for Stone Vacuum Infusion is a specially formulated epoxy resin system designed to ensure excellent flowability and uniform impregnation under vacuum conditions. Its controlled viscosity allows deep penetration into stone structures, improving internal strength while maintaining visual clarity and long-term stability after curing.

 

Professional-2-step-epoxy-for-hard-granite

 

Product Features & Specifications

 

Feature Description
Applicable Material Natural stone and engineered stone
Epoxy System Code 5080 / B25Q-KG
Epoxy System Ratio 100 : 25
Durability High stability and long-lasting performance after curing
Ease of Use Easy to mix and apply, no special tools required
Curing Time 3–5 hours
Yellowing Resistance High
Recommended Temperature 24°C
Viscosity CPS 400–600

Problems It Solves

  • Insufficient resin penetration in vacuum infusion processes
  • Uneven reinforcement caused by high-viscosity systems
  • Structural weakness inside stone slabs
  • Yellowing and instability after curing

Recommended Applications

  • Stone vacuum infusion and impregnation processes
  • Slab reinforcement for natural and engineered stone
  • Composite stone manufacturing
  • Industrial stone processing lines

Key Performance Advantages

  • Low viscosity for excellent flow and deep penetration
  • Stable curing with long-term mechanical performance
  • High resistance to yellowing for improved appearance
  • Consistent performance under controlled vacuum conditions

Product System Description

This is a two-component epoxy resin system consisting of resin (Part A) and hardener (Part B). When mixed at a ratio of 100:25 by weight, it forms a low-viscosity system optimized for vacuum infusion, ensuring uniform impregnation and reliable curing.

Processing Suggestions

  1. Mix both components thoroughly according to the specified ratio
  2. Degas the mixed resin if necessary before vacuum infusion
  3. Operate at an ambient temperature of approximately 24°C
  4. Ensure stone materials are dry and free from dust or contaminants

Suitable Stone Types

  • Marble
  • Granite
  • Limestone
  • Onyx
  • Engineered stone

Packaging & Supply

  • Available in standard industrial packaging
  • Suitable for bulk supply and continuous production
  • Factory-direct supply with stable quality control

Frequently Asked Questions (FAQ)

What makes this epoxy suitable for vacuum infusion?

A: Its low viscosity allows excellent resin flow and deep penetration under vacuum conditions.

What is the recommended mixing ratio?

A: The recommended mixing ratio is 100:25 by weight.

How long does curing take?

A: The typical curing time is 3–5 hours, depending on processing conditions.

Does this epoxy resist yellowing?

A: Yes, it offers high yellowing resistance after curing.

At what temperature should it be processed?

A: The ideal processing temperature is around 24°C.

Are you a factory or trading company?

A: We are a professional manufacturer and factory based in China, specializing in AB glue systems for stone applications. We offer direct factory supply, OEM services, and customized solutions for bulk orders.

Do you provide samples for testing?

A: Yes, we provide samples for quality testing. Please contact our sales team with your requirements, and we can arrange sample shipment for you to evaluate the performance on your stone materials.

What is the minimum order quantity (MOQ) for factory direct supply?

A: Our MOQ is flexible depending on the product specifications. For this Low Viscosity Epoxy for Stone Vacuum Infusion, we can accommodate both small trial orders and large bulk shipments. Please contact us for detailed pricing and MOQ information.

How should I store these epoxy products?

A: Store both products in a cool, dry place away from direct sunlight. Keep containers tightly sealed when not in use. Recommended storage temperature is 10°C to 25°C. Avoid freezing or excessive heat.

Final Note / Practical Takeaway: This low-viscosity epoxy system is specifically optimized for stone vacuum infusion, combining excellent flow characteristics with durable curing performance, making it a dependable choice for high-quality stone reinforcement applications. As a China-based manufacturer, we offer factory-direct pricing and customization options for bulk orders. Contact us for samples or volume pricing.