Epoxy Resin to fill small pits in Travertine
- Feature: Epoxy Resin for Travertine
- Applicable material: Travertine
- Epoxy system code: TL4090BF+TLB25Q-KG
- Epoxy system ratio: 100:25
- Curing effect: Forms a semi-solid sealing layer
- Durability: High stability and long-lasting after curing
- Ease of Use: Easy to mix and apply, no special tools required
Overview
Epoxy Resin Sealant is a specialized, high-viscosity sealing solution designed to address the unique needs of porous Travertine surfaces. It penetrates deep into cracks and pores, creating a robust seal that is both durable and reliable. This eco-friendly product is easy to apply, requiring no special tools, and cures to form a solid barrier against water seepage. With a focus on user safety and environmental responsibility, our sealant is the ideal choice for maintaining the integrity and aesthetic appeal of Travertine structures.
Product Description
Epoxy Resin Sealant for Travertine

The Epoxy Resin for Travertine is a high-performance sealing material specifically designed for porous rocks like Travertine. It effectively penetrates the cracks and pores in the rock, forming a solid sealant layer after curing, which achieves a long-lasting and reliable water-blocking effect. This product features high viscosity, low surface tension, and excellent penetration capabilities, ensuring efficient application on various surfaces of Travertine.

Product Features:
| Feature | Epoxy Resin for Travertine |
| Applicable material | Travertine |
| Epoxy system code | TL4090BF+TLB25Q-KG |
| Epoxy system ratio | 100:25 |
| Curing effect | Forms a semi-solid sealing layer |
| Durability | High stability and long-lasting after curing |
| Ease of Use | Easy to mix and apply, no special tools required |
| Ease of Use | Easy to mix and apply, no special tools required |
| Environmental Friendliness | Low Volatile Organic Compounds (VOC), eco-friendly |
Usage Instructions:
- Clean the surface of the Travertine to ensure it is dust and oil-free.
- Mix the epoxy resin and hardener in the ratio specified in the instructions.
- Use a specialized tool to inject the mixed epoxy resin into the cracks and pores of the Travertine.
- Allow the epoxy resin to cure completely, which usually takes 24 hours.
- After curing, if necessary, sand and clean the surface.
Precautions:
- Use this product in a well-ventilated area.
- Keep out of reach of children and pets.
- Read the product manual carefully before use.
Packaging Specifications:
- 25 kg container
- 200 kg container
- 1000 kg container
Shelf Life:
- 12 months when unopened.
Storage Conditions:
- Store in a cool, dry, and well-ventilated area, away from fire and high temperatures.
With this introduction, you can fully understand the product features and usage methods of the Epoxy Resin Sealant for Travertine. We are committed to providing high-quality products to meet your needs for the maintenance and repair of Travertine.