Epoxy resin adhesives for stone bonding, repairing, sealing and packaging marble
                                    - Feature: Epoxy Resin for hard white Marble
 - Applicable material: Calacatte , Stuario, Carrara White
 - Epoxy system code: 5099-YC +D30M-BS
 - Epoxy system ratio by weight: 100:30
 - Curing effect: Forms a liquid sealing layer
 
Overview
Epoxy is a premium adhesive designed specifically for marble slabs, providing superior protection and enhancement. It increases the abrasion and chemical resistance of marble, highlights the veins and colors, and increases its durability. Ideal for interior design and furniture manufacturing, Epoxy provides professional-grade epoxy protection.
Product Description
Epoxy Resin Sealant for Marble
The Epoxy Resin for Marble is a high-performance sealing material specifically designed for porous stones like Marble. It effectively penetrates the cracks and pores in the stone, forming a solid sealant layer after curing, which achieves a long-lasting and reliable water-blocking effect. This product features high viscosity, low surface tension, and excellent penetration capabilities, ensuring efficient application on various surfaces of Marble.

Product Features
| Feature | Epoxy Resin for hard white Marble | 
|---|---|
| Applicable material | Calacatte , Stuario, Carrara White | 
| Epoxy system code | 5099-YC +D30M-BS | 
| Epoxy system ratio by weight | 100:30 | 
| Curing effect | Forms a liquid sealing layer | 
| Durability | High stability and long-lasting after curing, good yellowing resistance, low viscosity, strong Bonding | 
| Ease of Use | Easy to mix and apply, no special tools required | 
Application of Epoxy Resin on Marble Slabs
- Adhesive
 
Epoxy resin’s strong adhesion makes it ideal for securing marble slabs, ensuring stability in both large projects and small repairs. It bonds marble to various materials, like wood, glass, or metal, and withstands external stress, providing long-term safety.
- Filling
 
As a filler, epoxy resin smooths out cracks or holes in marble, enhancing durability and appearance. This repair not only boosts visual appeal but also reinforces structural stability, preventing future damage.
- Surface Coating
 
An epoxy coating enhances marble’s look and offers waterproof, stain-resistant protection, preserving marble’s shine and simplifying maintenance. Ideal for kitchens, bathrooms, and public spaces, it helps marble retain its natural charm across various settings.
- Decorative Value
 
Epoxy resin’s versatility in design allows for unique visual effects. Whether for custom furniture or art, it adds charm, adapting to both minimalist and traditional aesthetics.
- Chemical and Heat Resistance
 
With high resistance to chemicals and heat, epoxy resin protects marble in areas like bathrooms and kitchens. It prevents damage from cleaners and oils, maintaining marble’s appearance and reducing future maintenance needs.
- Protection and Restoration
 
Epoxy resin extends marble’s life by minimizing wear and scratches, helping it maintain its natural luster. Regular treatment prevents minor damage from worsening, keeping marble looking pristine.
- Environmentally Friendly Properties
 
Modern, low-VOC epoxy resins reduce indoor air impact, making them environmentally friendly and suitable for interiors. This option supports sustainable development while preserving marble’s beauty and durability.
Usage Instructions:
Clean the surface of the Marble to ensure it is dust and oil-free.
Mix the epoxy resin and hardener in the ratio specified in the instructions.
Use a specialized tool to inject the mixed epoxy resin into the cracks and pores of the Marble.
Allow the epoxy resin to cure completely, which usually takes 24 hours.
After curing, if necessary, sand and clean the surface.
Precautions:
Use this product in a well-ventilated area.
Keep out of reach of children and pets.
Read the product manual carefully before use.
Packaging Specifications:
25 kg container
200 kg container
1000 kg container
Shelf Life:
12 months when unopened.
Storage Conditions:
Store in a cool, dry, and well-ventilated area, away from fire and high temperatures.
With this introduction, you can fully understand the product features and usage methods of the Epoxy Resin Sealant for Marble. We are committed to providing high-quality products to meet your needs for the maintenance and repair of Marble.